Study on Separation of Pb and Zn from Mixed Rougher Concentrates
1
作者 张桂芳 张宗华 《Journal of Rare Earths》 SCIE EI CAS CSCD 2004年第S1期33-39,共7页
The compositions of Pb and Zn mixed rougher concentrates were studied. The process utilizes flotation and gravity flow sheet to separate Pb or Zn. Pb and Zn in the tailings were reclaimed by gravity more efficiently. ... The compositions of Pb and Zn mixed rougher concentrates were studied. The process utilizes flotation and gravity flow sheet to separate Pb or Zn. Pb and Zn in the tailings were reclaimed by gravity more efficiently. This test used an ion-wave shaking table developed by Kunming University of Science and Technology. Based on the test results, the optimum test condition was chosen and testing of synthetic condition was performed. The results show that the process produces a final Zn concentrate with a 42.16% grade and 79.64% recovery and a final Pb concentrate with a 46.52% grade and 78.41% recovery. 展开更多
关键词 ore dressing pb-zn separation floatation-gravity separation rare earths
下载PDF
兰坪盆地白秧坪Cu-Pb-Zn-Ag多金属矿集区元素共生分异机制及物质来源 被引量:12
2
作者 冯彩霞 毕献武 +4 位作者 胡瑞忠 刘燊 武丽艳 唐永永 邹志超 《岩石学报》 SCIE CAS CSCD 北大核心 2011年第9期2609-2624,共16页
兰坪白秧坪Cu-Ag多金属矿集区夹持于金沙江和澜沧江断裂之间,属兰坪-思茅中新生代坳陷带之兰坪盆地北部,可分东矿带和西矿带二部分。本文通过对白秧坪金属矿集区东西2个矿带的矿石矿物电子探针分析、成矿元素含量和组合分析及S同位素的... 兰坪白秧坪Cu-Ag多金属矿集区夹持于金沙江和澜沧江断裂之间,属兰坪-思茅中新生代坳陷带之兰坪盆地北部,可分东矿带和西矿带二部分。本文通过对白秧坪金属矿集区东西2个矿带的矿石矿物电子探针分析、成矿元素含量和组合分析及S同位素的讨论得出:(1)东西2个矿带矿石矿物组合类型及微量元素组合特征具明显不同,前者矿石矿物组分较为简单,西带较为复杂,不仅有Pb、Zn和Cu的独立矿物,还存在Co和Bi的矿物;(2)东矿带Ag、As、Cd、Pb、Sb和Zn的富集从南到北依次减弱,Bi的富集依次增强,Cu的富集趋势越往北越富集,亏损元素为Co、Cr、Ni和V;西矿带Ag、Pb、Zn的富集属吴底厂和李子坪矿段最富集,而Cu则在小丫口和白秧坪矿段最富集。亏损元素为Ba、Co、Cr、Ni和V,但各个矿段这些元素的亏损程度有所不同,有的矿段部分元素有稍富集趋势;(3)Co、Ni和Cr等微量元素西带高于东带,而Sr、Pb、Zn和Ba元素则东带高于西带,与各自的矿物组合类型一致,且元素的共生分异机制与构造分带存在一定的耦合关系;(4)兰坪盆地火山岩为白秧坪多金属矿集区提供了主要物源,Mo、Co和Ni等元素显示其成矿可能与隐伏基性-超基性岩浆有关的深部来源有关;S同位素特征表明东西矿带金属硫化物硫源均以幔源为主。 展开更多
关键词 共生分异机制 来源 成矿元素 Cu-pb-zn-Ag多金属矿集区 白秧坪 兰坪盆地
下载PDF
0.91Pb(Zn_(1/3)Nb_(2/3)O_3-0.09PbTi0_3的析晶行为及助溶剂法生长 被引量:6
3
作者 徐家跃 范世(?) 孙仁英 《硅酸盐学报》 EI CAS CSCD 北大核心 2002年第6期721-724,共4页
研究了0.91Pb(znl/3Nb2/3)O3-0.09PbTiO3(PZNT91/9,摩尔分数)在不同组分和配比熔盐中的析晶行为及其对晶体生长的影响。发现B2O3,PbF2等助溶剂不利于钙钛矿相的析出;而BaTiO3-PbO复合体系虽然能够促进钙钛矿相析出,但晶体析出量很少;只... 研究了0.91Pb(znl/3Nb2/3)O3-0.09PbTiO3(PZNT91/9,摩尔分数)在不同组分和配比熔盐中的析晶行为及其对晶体生长的影响。发现B2O3,PbF2等助溶剂不利于钙钛矿相的析出;而BaTiO3-PbO复合体系虽然能够促进钙钛矿相析出,但晶体析出量很少;只有适当比例的。PbO助溶剂比较适合于生长具有铁电性的钙钛矿相PZNT91/9单晶。助溶剂法生长的工艺参数为:溶质与PbO助溶剂的摩尔比为l:l,泡料温度1 150-1 200℃,泡料时间10 h,晶体生长时降温速度0.8-2℃/h,当温度降到900℃时停止生长,以50℃/h快速冷却至室温。所得晶体为琥珀色,最大尺寸达φ30 mm×15 mm,其压电系数和机电偶合系数分别为2000 pc/N和0.92。 展开更多
关键词 0.91pb(zn1/3Nb2/3)O3-0.09pbTiO3 析晶行为 助溶剂法 铌锌钛酸铅 钙钛矿相 晶体生长
下载PDF
[001]c极化0.93Pb(Zn_(1/3)Nb_(2/3))O_3-0.07PbTiO_3单晶中声表面波传播特性
4
作者 李秀明 吴广涛 +2 位作者 徐权 张锐 李玉春 《人工晶体学报》 EI CAS CSCD 北大核心 2015年第5期1222-1226,1253,共6页
利用室温下弛豫铁电单晶0.93Pb(Zn1/3Nb2/3)O3-0.07PbTiO3的材料参数,计算了[001]c极化PZN-7%PT晶体中的声表面波传播特性。结果表明,[001]c极化0.93Pb(Zn1/3Nb2/3)O3-0.07Pb TiO3单晶具有明显优于传统压电材料的声表面波特性。0.93Pb(Z... 利用室温下弛豫铁电单晶0.93Pb(Zn1/3Nb2/3)O3-0.07PbTiO3的材料参数,计算了[001]c极化PZN-7%PT晶体中的声表面波传播特性。结果表明,[001]c极化0.93Pb(Zn1/3Nb2/3)O3-0.07Pb TiO3单晶具有明显优于传统压电材料的声表面波特性。0.93Pb(Zn1/3Nb2/3)O3-0.07Pb Ti O3单晶的声表面波特性随着传播方向发生明显的变化。综合考虑晶体的三种声表面波特性,发现Y切型晶体的综合声表面波性能最好,声表面波机电耦合系数k2值较大,能流角和声表面波自由表面相速度值较小,有望应用于下一代低频声表面波设备中。 展开更多
关键词 0.93pb(zn1/3Nb2/3)O3-0.07pbTiO3 声表面波 机电耦合系数
下载PDF
丙烯酸-马来酸酐共聚物络合超滤分离水溶液中Pb^(2+)和Zn^(2+)的实验研究 被引量:1
5
作者 曹光亮 李振山 包立超 《北京大学学报(自然科学版)》 EI CAS CSCD 北大核心 2014年第3期542-548,共7页
采用丙烯酸-马来酸酐共聚物(PMA)为络合剂,研究络合超滤技术对水溶液中Pb2+和Zn2+的分离效果、竞争络合效应以及外加盐对分离效果的影响。以两种金属离子截留率之差表示分离率,以单一金属离子溶液中离子截留率与混合溶液中该离子的截留... 采用丙烯酸-马来酸酐共聚物(PMA)为络合剂,研究络合超滤技术对水溶液中Pb2+和Zn2+的分离效果、竞争络合效应以及外加盐对分离效果的影响。以两种金属离子截留率之差表示分离率,以单一金属离子溶液中离子截留率与混合溶液中该离子的截留率之差表示金属离子间的竞争强度。结果表明:随着PMA浓度增加,两种金属离子的分离率先增大后减小,当PMA浓度为200 mg/L时,分离率达到最大值,为54.47%。pH从2增加到6时,分离率先增大后减小,且在pH=4时达到最大,为71.34%。两种金属离子的竞争效应随pH及PMA浓度的增加先增强后减弱,在pH=5,PMA浓度为200 mg/L时,混合溶液中两种离子竞争效应最强。外加Na2SO4对分离率有较大影响,随着n(Na2SO4)增大分离率增加,随后基本保持不变,在n(Na2SO4)=0.06mol/L时,分离率达到最大值,为97.677%。加入Na2SO4减弱了Zn2+的竞争络合能力,有利于两种金属离子的分离。 展开更多
关键词 pb2+ zn2+ 丙烯酸-马来酸酐共聚物 超滤 选择性分离 竞争络合
下载PDF
甘肃厂坝-李家沟超大型铅锌矿床成矿金属来源——来自闪锌矿原位S-Pb和Zn同位素证据
6
作者 魏然 王义天 +3 位作者 胡乔青 黄诗康 窦平 胡文荣 《矿床地质》 CAS CSCD 北大核心 2022年第4期722-740,共19页
甘肃厂坝-李家沟铅锌矿床位于西秦岭多金属成矿带内的西成矿集区,为矿集区内重要的超大型铅锌矿床。矿体赋存在中泥盆统安家岔组的白云石化大理岩及石英片岩中,其成因认识一直存在争议,主要分歧集中在是同生还是后生。文章对不同成矿阶... 甘肃厂坝-李家沟铅锌矿床位于西秦岭多金属成矿带内的西成矿集区,为矿集区内重要的超大型铅锌矿床。矿体赋存在中泥盆统安家岔组的白云石化大理岩及石英片岩中,其成因认识一直存在争议,主要分歧集中在是同生还是后生。文章对不同成矿阶段的闪锌矿,采用多接收电感耦合等离子体质谱(MC-ICP-MS)测定Zn同位素组成、采用激光剥蚀-多接收电感耦合等离子体质谱(LA-MC-ICP-MS)原位微区分析技术测定S、Pb同位素组成,示踪成矿物质来源,并分析矿物沉淀机制,为深入理解矿床成因提供新的精细证据。研究结果显示,Ⅰ、Ⅱ、Ⅲ三个成矿阶段闪锌矿的δ^(66)Zn分别为0.08‰~0.29‰,平均0.20‰;0.19‰~0.37‰,平均0.30‰;0.36‰~0.37‰,平均0.37‰。其中,Ⅰ阶段的闪锌矿δ^(34)SⅠ值为20.9‰~26.1‰,平均24.4‰;Ⅱ阶段的闪锌矿δ^(34)SⅡ值为12.2‰~21.9‰,平均19.1‰;Ⅲ阶段的闪锌矿δ^(34)SⅢ值为18.2‰~24.7‰,平均21.5‰。3个阶段的矿石矿物Pb同位素组成变化不大,^(206)Pb/^(204)Pb为17.922~18.013,^(207)Pb/^(204)Pb为15.567~15.647,^(208)Pb/^(204)Pb为37.990~38.266。δ^(66)Zn同位素值显示,成矿金属早期来源于围岩海相碳酸盐岩,由于混合了岩浆热液或者是瑞利分馏作用,在成矿作用中后期δ^(66)Zn同位素逐渐上升。δ^(34)S同位素值显示,早期硫源主要为地层中的硫酸盐,中后期的δ^(34)S同位素值降低,可能是成矿流体中岩浆热液中的S^(2-)成分逐渐增多导致,闪锌矿为硫酸盐通过TSR反应沉淀成矿。Pb同位素指示成矿物质来源于上地壳,并混入了部分古老的变质基底的成分。笔者研究发现,厂坝-李家沟铅锌矿的成矿机制为不同来源的流体混合,随着pH值、成矿流体的温度发生变化而沉淀成矿。 展开更多
关键词 地球化学 闪锌矿 zn同位素 原位S同位素 原位pb同位素 沉淀机制 厂坝-李家沟铅锌矿床
下载PDF
The Forming Conditions of and Ore-searching Direction for B, Mg,Pb, Zn and Au Deposits in the Liaoji Proterozoic Rift
7
作者 Zhu Yongzheng and Yao Fengliang (College of Earth Sciences,Jilin University, Changchun 130026 P. R. China) 《Global Geology》 2001年第1期20-25,共6页
The Liaoji Proterozoic rift is an inter-intracontinenatl rift developed from Archean granite-greenstone tectonic regime and contains many important mineral deposits of U, B, magnesite, Pb-Zn, Au, Ag, Co and P. These d... The Liaoji Proterozoic rift is an inter-intracontinenatl rift developed from Archean granite-greenstone tectonic regime and contains many important mineral deposits of U, B, magnesite, Pb-Zn, Au, Ag, Co and P. These deposits were formed as the result of late mobilization, transportation and concentfation of the previously enriched ore-forming mate- rials in several ore-bearing formations formed during the rift stage. So the metallogeny of these deposits in the rift shows both inheritance and new generation of the ore-forming materials. In future ore-searching practice, attentions should be paid on the studies of the ore-bearing formations in the rift, on the multiple stages of metallogeny and and on multiple derivations of the ore-forming materials. 展开更多
关键词 Liaoji PROTEROZOIC rift B Mg pb - zn AU deposits ORE - forming conditions ORE - SEARCHING direction
下载PDF
pH和Cu^(2+)Zn^(2+)对两种可变电荷土壤中吸附态Pb解吸行为的影响 被引量:10
8
作者 杨金燕 杨肖娥 +3 位作者 何振立 李廷强 章明奎 申屠佳丽 《农业环境科学学报》 CAS CSCD 北大核心 2005年第3期469-475,共7页
采用连续解吸法对两种可变电荷土壤中吸附态Pb的解吸行为进行研究。结果表明,红砂土和黄筋泥的Pb2+吸附量和解吸量都随Pb2+加入量的增加而增加。红砂土和黄筋泥对Pb的吸附等温线可用Langmuir模型来描述,最大吸附量(Xm)分别为10899和6195... 采用连续解吸法对两种可变电荷土壤中吸附态Pb的解吸行为进行研究。结果表明,红砂土和黄筋泥的Pb2+吸附量和解吸量都随Pb2+加入量的增加而增加。红砂土和黄筋泥对Pb的吸附等温线可用Langmuir模型来描述,最大吸附量(Xm)分别为10899和6195mg·kg-1。pH对吸附态Pb的解吸影响较大,解吸量随pH升高而降低。当pH≤2.00时2种土壤吸附态Pb2+的解吸率很高,接近100%;当pH由2.00上升至4.00时,解吸率呈直线下降;至pH>4.00时2种土壤吸附态Pb2+的解吸率均降至很低的水平。Cu2+和Zn2+的加入可增加土壤吸附态Pb2+的解吸,其中Cu2+对Pb2+解吸作用较Zn2+大。铜加入量从0到20mmol·L-1,红砂土和黄筋泥吸附Pb2+的解吸率分别从9.6%和15.9%增加到83.8%和98.2%,锌加入量从0到20mmol·L-1,2种土壤吸附Pb2+的解吸率则分别增加到81.2%和89.9%。 展开更多
关键词 pb CU zn PH 可变电荷土壤 吸附-解吸
下载PDF
与长途输送和当地污染物排放有关的大气悬浮物中的Cd/Pb和Zn/Pb比例特征(英文)
9
作者 Shih-Chieh Hsu Shaw Chen Liu Ru-Ting Hsu 《干旱区资源与环境》 CSSCI CSCD 2004年第S1期97-103,共7页
Along with windblown dust, large quantities of pollutants are annually brought out of the continental by the westerlies in winter and spring; thereafter they are partly subjected to transport by northeastern monsoon w... Along with windblown dust, large quantities of pollutants are annually brought out of the continental by the westerlies in winter and spring; thereafter they are partly subjected to transport by northeastern monsoon winds to Taiwan. Both PM10 and PM2.5 aerosols collected from northern Taiwan from February 2002 to March 2003 were determined for three heavy metals, namely Pb, Cd and Zn, to characterize the heavy metal compositions between long-range transported and local aerosols and to evaluate their contributions of long-range transport during the northeastern monsoon season. Low Cd/Pb (0.017) and Zn/Pb (1.82) ratios were measured in aerosols during the Asian dust period, in which the sources of ambient aerosols are dominated by long-range transport. By contrast, high Cd/Pb(0.030) and Zn/Pb (3.44) ratios were measured during the summer monsoon season, in which local pollutant emissions dominate the sources of heavy metals. Such characteristic Cd/Pb and Zn/Pb ratios appear to be successfully applied to identify the pollutants originated from the long-range transport or local emissions. 展开更多
关键词 污染物排放 大气悬浮物 pbzn 英文 长途 PM2.5-10 ICP-MS Regression SPATIAL HighC
下载PDF
咪唑-菲咯啉-苯氧乙酸锌、铅配合物的合成,结构及与DNA的相互作用(英文) 被引量:4
10
作者 沈伟 胡未极 +1 位作者 吴小勇 赵国良 《无机化学学报》 SCIE CAS CSCD 北大核心 2016年第6期1101-1110,共10页
以2-4-(1H-咪唑-2-[4,5-f][1,10]菲咯啉基)苯氧乙酸(HPIMPHC)和2-2-(1H-咪唑-2-[4,5-f][1,10]菲咯啉基)苯氧乙酸(HOIMPHC)为配体,水热合成了2种新型配合物[Zn(PIMPHC)_2]_n(1)和{[Pb(OIMPHC)_2]·4H_2O}_n(2)。配合物1属正交晶系,... 以2-4-(1H-咪唑-2-[4,5-f][1,10]菲咯啉基)苯氧乙酸(HPIMPHC)和2-2-(1H-咪唑-2-[4,5-f][1,10]菲咯啉基)苯氧乙酸(HOIMPHC)为配体,水热合成了2种新型配合物[Zn(PIMPHC)_2]_n(1)和{[Pb(OIMPHC)_2]·4H_2O}_n(2)。配合物1属正交晶系,空间群为Pbcn;Zn(Ⅱ)的配位数为6,配位构型为变形的八面体,形成2D网状结构。配合物2属单斜晶系,空间群为P21/n;Pb(Ⅱ)的配位数为7,配位构型为变形的五角双锥,形成2D网状结构。荧光光谱的结果表明,配合物与DNA的相互作用强于配体。 展开更多
关键词 2-4-(1H-咪唑-2-[4 5-f][1 10]菲咯啉基)苯氧乙酸 2-2-(1H-咪唑-2-[4 5-f][1 10]菲咯啉基)苯氧乙酸 zn(Ⅱ) pb(Ⅱ) DNA作用
下载PDF
ICP-AES测定多目标水地球化学普查样品中的14种微量元素 被引量:4
11
作者 程泽 阿拉木斯 +1 位作者 苏金华 谭玉娟 《光谱实验室》 CAS CSCD 2006年第1期130-132,共3页
采用IRIS Intrepid II SXP ICP光谱仪,对地球化学普查水样中Ba、Be、Cd、Co、Cr、Cu、Fe、 Mn、Mo、Ni、P、Pb、Sr和Zn等元素的测量条件进行了探讨,优化了实验条件,进行了大批量实际样品的测定。方法简便,快速。检出限、精密度和准确度... 采用IRIS Intrepid II SXP ICP光谱仪,对地球化学普查水样中Ba、Be、Cd、Co、Cr、Cu、Fe、 Mn、Mo、Ni、P、Pb、Sr和Zn等元素的测量条件进行了探讨,优化了实验条件,进行了大批量实际样品的测定。方法简便,快速。检出限、精密度和准确度均符合质量管理的要求。 展开更多
关键词 电感耦合等离子体-原子发射光谱法 地球化学普查水 BA Bo Cd Co Cr Cu Fe Mn MO Ni P pb Sr zn
下载PDF
基体分离-电感耦合等离子体原子发射光谱(ICP-AES)法测定精铋中10种杂质元素 被引量:5
12
作者 孔会民 董更福 +1 位作者 王景凤 岳萍 《中国无机分析化学》 CAS 北大核心 2021年第3期71-74,共4页
采用电感耦合等离子体原子发射光谱(ICP-AES)法测定精铋中Cd、Co、Cu、Fe、Mg、Mn、Ni、Pb、Ti、Zn等十种杂质元素,样品用优级纯硝酸溶解,往60℃左右的溶液中,滴加氨水(1+1),控制pH值在3.0~4.0。考察了温度、酸度、沉降时间对铋的去除... 采用电感耦合等离子体原子发射光谱(ICP-AES)法测定精铋中Cd、Co、Cu、Fe、Mg、Mn、Ni、Pb、Ti、Zn等十种杂质元素,样品用优级纯硝酸溶解,往60℃左右的溶液中,滴加氨水(1+1),控制pH值在3.0~4.0。考察了温度、酸度、沉降时间对铋的去除率和对检测结果的影响。根据分析线的选择原则,结合待测元素的检测范围,选择无干扰、峰形对称、灵敏度适中的谱线作为分析线(Cd 228.802 nm、Co 237.862 nm、Cu 324.754 nm、Fe 259.940 nm、Mg 279.553 nm、Mn 257.610 nm、Ni 231.604 nm、Pb 182.205 nm、Ti 323.452 nm、Zn 213.856 nm)。各元素的质量浓度在一定范围内与其发射强度呈线性,校准工作曲线的线性相关系数均大于0.9997,各元素检出限为0.002~0.253μg/g。按照实验方法测定精铋实际样品,结果的相对标准偏差(RSD,n=9)为2.5%~9.8%,加标回收率为95.1%~102%,满足检测要求。 展开更多
关键词 基体分离 电感耦合等离子体原子发射光谱法(ICP-AES)
下载PDF
BK-302用于某铅锌矿铜铅分离试验研究
13
作者 何伟 肖巧斌 刘龙利 《世界有色金属》 2018年第16期70-71,共2页
BK302是一种新型高选择性铜捕收剂,用于某铅锌矿铜铅分离研究表明,可有效的实现铜铅分离,分离效果优于重铬酸盐法。BK302用量少,可降低选矿成本,是一种具有应用前景的新型铜铅分离捕收剂。
关键词 捕收剂 铜铅分离 铜铅锌矿
下载PDF
0.2Pb(Zn_(1/3)Nb_(2/3))O_3-0.8Pb(Zr_(0.5),Ti_(0.5))O_3(1-x)(Ni_(51.5)Mn_(25)Ga_(23.5))x固溶体系磁电性能研究
14
作者 仲麒 张铭 +5 位作者 邓浩亮 郑木鹏 胡州 侯育冬 朱满康 严辉 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2013年第S1期201-203,共3页
采用传统的固相烧结法合成了0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3(1-x)(Ni51.5Mn25Ga23.5)x复合体系陶瓷。XRD结果表明,随着Ni51.5Mn25Ga23.5(NMG)掺入,Ni51.5Mn25Ga23.5先溶于0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3中,后NMG... 采用传统的固相烧结法合成了0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3(1-x)(Ni51.5Mn25Ga23.5)x复合体系陶瓷。XRD结果表明,随着Ni51.5Mn25Ga23.5(NMG)掺入,Ni51.5Mn25Ga23.5先溶于0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3中,后NMG量超过5%不溶于复合体系中,使得0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3的峰位向右偏移;铁电性能测试结果表明,0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3(1-x)(Ni51.5Mn25Ga23.5)x复合体系陶瓷随着Ni51.5Mn25Ga23.5的掺入量的增加矫顽场E先降低后增加,剩余极化强度Pr逐渐降低,这与XRD的测试结果相一致;磁性测试结果表明,0.2Pb(Zn1/3Nb2/3)O3-0.8Pb(Zr0.5,Ti0.5)O3(1-x)(Ni51.5Mn25Ga23.5)x随着Ni51.5Mn25Ga23.5掺入量的增加,以独立相析出在复合体系中,剩余磁化强度Mr逐渐增大。 展开更多
关键词 0.2pb(zn1/3Nb2/3)O3-0.8pb(Zr0.5 Ti0.5)O3 Ni51.5Mn25Ga23.5 固相烧结 复合材料
原文传递
云南某含碳铅锌矿浮选回收铅锌试验研究 被引量:15
15
作者 张晶 简胜 +2 位作者 王少东 乔吉波 吕晋芳 《矿冶工程》 CAS CSCD 北大核心 2014年第4期55-58,共4页
采用优先浮选碳-铅硫混选分离-锌硫混选分离的浮选工艺流程对云南某含碳铅锌矿进行了试验研究,成功获得了铅精矿、锌精矿,并有效回收了硫。铅精矿中铅品位47.72%、锌品位4.25%、铅回收率48.05%、锌回收率0.38%,锌精矿中锌品位50.27%、... 采用优先浮选碳-铅硫混选分离-锌硫混选分离的浮选工艺流程对云南某含碳铅锌矿进行了试验研究,成功获得了铅精矿、锌精矿,并有效回收了硫。铅精矿中铅品位47.72%、锌品位4.25%、铅回收率48.05%、锌回收率0.38%,锌精矿中锌品位50.27%、铅品位0.72%、锌回收率94.21%、铅回收率15.13%。铅、锌在碳产品中损失不大。 展开更多
关键词 浮选 含碳铅锌矿 铅硫分离 锌硫分离
下载PDF
某铜铅锌矿清洁浮选技术研究 被引量:7
16
作者 张晶 王少东 +2 位作者 乔吉波 简胜 阚赛琼 《矿冶工程》 CAS CSCD 北大核心 2016年第6期49-52,56,共5页
对某嵌布粒度不均匀的铜铅锌多金属矿进行了选矿试验研究。采用铜铅混选-铜铅分离-尾矿选锌的浮选工艺流程,采用硫化钠作铜铅分离调整剂,可得到含铜19.87%、铜回收率83.46%的铜精矿,含铅54.19%、铅回收率83.57%的铅精矿和含锌52.57%、... 对某嵌布粒度不均匀的铜铅锌多金属矿进行了选矿试验研究。采用铜铅混选-铜铅分离-尾矿选锌的浮选工艺流程,采用硫化钠作铜铅分离调整剂,可得到含铜19.87%、铜回收率83.46%的铜精矿,含铅54.19%、铅回收率83.57%的铅精矿和含锌52.57%、锌回收率89.39%的锌精矿。矿石中的伴生银大多富集于各浮选精矿中,银在铜、铅和锌精矿中的含量分别为165.2,537.6和15.1 g/t,银总回收率77.19%。各有价金属都得到了很好地回收。 展开更多
关键词 清洁浮选 铜铅锌矿 铜铅分离 硫化钠
下载PDF
钢铁厂含锌铅粉尘中锌铅分离理论及实践 被引量:22
17
作者 张丙怀 郭兴忠 +1 位作者 阳海彬 唐元位 《有色金属(冶炼部分)》 CAS 2002年第1期7-11,共5页
提出钢铁厂含锌铅粉尘中锌铅分离理论 ,并研制出一种新的火法处理工艺———铝浴法熔融还原。通过与其它还原方法的比较 ,并考察了温度、时间等工艺因素的影响 ,得到了铝浴法合理工艺参数 :温度 110 0℃ ,时间45min ,收集所得氧化锌粉含... 提出钢铁厂含锌铅粉尘中锌铅分离理论 ,并研制出一种新的火法处理工艺———铝浴法熔融还原。通过与其它还原方法的比较 ,并考察了温度、时间等工艺因素的影响 ,得到了铝浴法合理工艺参数 :温度 110 0℃ ,时间45min ,收集所得氧化锌粉含ZnO90 %以上 (最高达 92 5 2 % ) ,PbO小于 5 % ,锌挥发率和铅富集率达 90 %以上 。 展开更多
关键词 含锌铅粉尘 锌铅分离 铝浴法熔融还原 钢铁厂
下载PDF
豫西某难选铅锌矿选矿试验研究 被引量:8
18
作者 曹飞 吕良 +1 位作者 李文军 岳铁兵 《矿冶工程》 CAS CSCD 北大核心 2013年第6期36-37,41,共3页
豫西某铅锌矿有用矿物共生关系密切、嵌布粒度较细,采用铅锌等可浮、铅锌分离-硫化锌浮选-氧化铅浮选工艺,成功实现了该矿的铅锌回收与分离,并有效回收了氧化铅矿物,最终获得了铅品位、回收率分别为58.95%、68.67%的铅精矿和锌品位、回... 豫西某铅锌矿有用矿物共生关系密切、嵌布粒度较细,采用铅锌等可浮、铅锌分离-硫化锌浮选-氧化铅浮选工艺,成功实现了该矿的铅锌回收与分离,并有效回收了氧化铅矿物,最终获得了铅品位、回收率分别为58.95%、68.67%的铅精矿和锌品位、回收率分别为48.67%、66.06%的锌精矿。 展开更多
关键词 浮选 铅锌矿 铅锌分离 氧化铅
下载PDF
黑龙江铁力铜铅锌硫化矿铜铅浮选分离试验研究 被引量:5
19
作者 彭志兵 刘三军 +2 位作者 覃文庆 张博 杨聪仁 《矿冶工程》 CAS CSCD 北大核心 2013年第3期53-57,共5页
对黑龙江铁力铜铅锌硫化矿进行了浮选试验研究。采用铜铅混浮-铜铅分离-混浮尾矿选锌的工艺流程,并采用CMC+亚硫酸钠组合抑制剂,实现了铜铅分离,闭路试验获取得了铜精矿品位20.25%、回收率60.52%,铅精矿品位55.25%、回收率70.07%,锌精... 对黑龙江铁力铜铅锌硫化矿进行了浮选试验研究。采用铜铅混浮-铜铅分离-混浮尾矿选锌的工艺流程,并采用CMC+亚硫酸钠组合抑制剂,实现了铜铅分离,闭路试验获取得了铜精矿品位20.25%、回收率60.52%,铅精矿品位55.25%、回收率70.07%,锌精矿锌品位46.35%、回收率86.73%的指标。 展开更多
关键词 浮选 铜铅锌硫化矿 铜铅分离 CMC 部分混浮
下载PDF
四川某难选硫铁铅锌矿合理选矿工艺研究 被引量:6
20
作者 蒋素芳 郭玉武 +2 位作者 魏党生 叶从新 韦华祖 《矿产综合利用》 CAS 北大核心 2016年第3期35-39,共5页
针对四川某磁黄铁矿含量高、铅锌品位低、矿物共生关系密切的铅锌矿石进行了选矿工艺试验研究。采用铅优先浮选-磁选脱硫-锌硫混浮再分离的工艺流程,可获得Pb品位62.37%,回收率86.75%的铅精矿,Zn品位46.46%,回收率83.13%的锌精矿,S品位3... 针对四川某磁黄铁矿含量高、铅锌品位低、矿物共生关系密切的铅锌矿石进行了选矿工艺试验研究。采用铅优先浮选-磁选脱硫-锌硫混浮再分离的工艺流程,可获得Pb品位62.37%,回收率86.75%的铅精矿,Zn品位46.46%,回收率83.13%的锌精矿,S品位39.10%,回收率82.37%的硫铁精矿,试验指标良好,实现了铅锌硫的综合回收,为经济合理开发该类矿石提供了一定参考。 展开更多