INVESTIGATION ON HOT DUCTILITY AND STRENGTH OF CONTINUOUS CASTING SLAB FOR AH32 STEEL 被引量:2
1
作者 G. Y. Li X.F. Li L.G. Ao 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2006年第1期75-78,共4页
By means of Gleeble-1500 testing machine, the simulation of continuous casting process forAH32 steel was carried out and hot ductility and strength were determined. The cracking sensitivity was studied under the diffe... By means of Gleeble-1500 testing machine, the simulation of continuous casting process forAH32 steel was carried out and hot ductility and strength were determined. The cracking sensitivity was studied under the different temperatures and strain rates. The Precipitations of AIN at different temperatures and the fractures of high-temperature tensile samples were observed by using TEM (transmission electron microscope) and SEM (scanning electron microscope). The factors affecting the brittle temperature zone were discussed. 展开更多
关键词 continuous casting slab brittle temperature zone tensile strength ductility SIMULATION
下载PDF
Web Shear Strengthening Technique of Deep Precast Prestressed Hollow Core Slabs under Truck Loads
2
作者 Islam M. Ezz El-Arab 《Journal of Building Construction and Planning Research》 2017年第4期129-145,共17页
Precast prestressed Hollow Core Slabs (HCS), are one of the famous and widely used slabs for concrete structures all over the world and widely implemented in the Middle East. HCS are used in industrial, commercial, re... Precast prestressed Hollow Core Slabs (HCS), are one of the famous and widely used slabs for concrete structures all over the world and widely implemented in the Middle East. HCS are used in industrial, commercial, residential buildings, as well as, in the parking structures. This paper succeeded to present new special details for deep HCS to enhance and strengthen the web shear strength capacity of HCS 400 and 500 mm depths respectively at the open parking area. This is subjected to heavy truck wheel loads so as to achieve the LRFD Code’s requirements. However, it is noticed many web shear cracks of HCS are used at parking area at many projects in Gulf Region. On the other hand, ACI318-14 permits no shear reinforcement in prestressed HCS thickness of less than 12.5 in (320 mm). The paper presents experimental tests program, to verify the numerical finite element of deep HCS under maximum design uniform loads, in addition to the new strengthening techniques. New strengthening techniques succeed to enhance the web shear capacity by significant percentage, due to the new details for HCS 400 by 68% up to 256% increasing of the web shear capacity compared to the ordinary HCS section. Also, HCS 500 shear capacity is enhanced with different percentages of strengthening techniques by 55%, up to 197% based on the different cases of strengthening. Furthermore enhancing deep HCS shear performance;the new techniques have an advantage of an easy execution at the site;casting with structural topping, otherwise the preparation can be done in precast factory before site handover, which saves time and cost compared to the others traditional strengthening techniques. 展开更多
关键词 HOLLOW Core slabS SHEAR Stress PRESTRESSED slabS SHEAR strength
下载PDF
FRP筋混凝土双向板冲切强度公式评估
3
作者 张亚坤 张雪婧 +1 位作者 侯黎黎 王建伟 《水电能源科学》 北大核心 2024年第2期52-56,共5页
为评价现有FRP筋混凝土双向板冲切强度计算公式的精度,采用数理统计的方法对收集到的38组FRP筋混凝土双向板冲切强度试验数据进行评估。结果表明,影响FRP筋混凝土双向板冲切强度的主要因素有混凝土强度、临界冲切截面周长、有效板厚、FR... 为评价现有FRP筋混凝土双向板冲切强度计算公式的精度,采用数理统计的方法对收集到的38组FRP筋混凝土双向板冲切强度试验数据进行评估。结果表明,影响FRP筋混凝土双向板冲切强度的主要因素有混凝土强度、临界冲切截面周长、有效板厚、FRP筋配筋率及其弹性模量、尺寸效应;在所评价的10个计算公式中,规范公式的预测结果大多比较保守,且其精度均低于文献公式;Ospina公式预测结果与试验结果最为接近,且精度最高,预测结果与试验结果比值的均值为1.03,标准差为16.04%,变异系数为15.53%。研究结果为FRP筋混凝土双向板冲切强度计算公式的进一步优化提供了参考。 展开更多
关键词 FRP筋 双向板 冲切强度 计算公式 评估
下载PDF
叠合板底板弯折钢筋与附加钢筋连接试验研究
4
作者 刘庆文 付光麒 李劲杰 《力学季刊》 CAS CSCD 北大核心 2024年第1期230-238,共9页
为研究边缘叠合板U型钢筋和叠合区域预制底板钢筋弯折高度的影响,进行了1个现浇板和4个叠合板受弯性能试验,对比分析了试验板的裂缝发展、破坏模式、挠度、承载力以及钢筋应变情况.结果表明:配置U型钢筋的叠合板承载能力和变形能力与现... 为研究边缘叠合板U型钢筋和叠合区域预制底板钢筋弯折高度的影响,进行了1个现浇板和4个叠合板受弯性能试验,对比分析了试验板的裂缝发展、破坏模式、挠度、承载力以及钢筋应变情况.结果表明:配置U型钢筋的叠合板承载能力和变形能力与现浇板接近,U型钢筋的销栓作用限制了裂缝沿叠合斜面的发展;预制底板钢筋采用90°弯折措施的叠合板在叠合区域根部开裂以后,随着荷载的加大,叠合板的裂缝宽度沿叠合斜面发展很快,不利位置出现在板的叠合斜面处,导致叠合板承载能力和刚度降低;预制底板90°弯折钢筋叠合板在破坏时,叠合斜面根部位置钢筋达到了屈服强度,表明底板钢筋弯折构造措施可以让钢筋充分发挥性能.最后,提出了采用预制底板90°弯折钢筋边缘叠合板的设计建议. 展开更多
关键词 边缘叠合板 弯折钢筋 锚固强度 受弯性能
下载PDF
基于声发射技术的高强全珊瑚钢筋混凝土板破坏特性研究
5
作者 石丹丹 陈徐东 +1 位作者 尚楷 马林建 《东南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2024年第2期398-406,共9页
为了探究全珊瑚钢筋混凝土板破坏特性,设计了3种不同配筋率(0.85%、1.13%和1.41%)的高强全珊瑚钢筋混凝土板构件.结合声发射技术,开展了全珊瑚混凝土板构件四点弯曲加载试验,揭示了配筋率对高强全珊瑚钢筋混凝土板力学性能的影响.基于... 为了探究全珊瑚钢筋混凝土板破坏特性,设计了3种不同配筋率(0.85%、1.13%和1.41%)的高强全珊瑚钢筋混凝土板构件.结合声发射技术,开展了全珊瑚混凝土板构件四点弯曲加载试验,揭示了配筋率对高强全珊瑚钢筋混凝土板力学性能的影响.基于声发射参数速率过程理论,建立了损伤定量评估模型,并进一步提出了可用于工程实践的损伤评估准则.结果表明:随配筋率增大,高强全珊瑚混凝土板构件起裂荷载、起裂时间与峰值荷载均增大,但中心挠度降低了11.29%;单位时间声发射参数变化均存在2个峰值区,可作为板构件的起裂评判和破坏预兆;根据声发射参数累计值变化可将高强全珊瑚混凝土板构件破坏过程划分为轻度(<0.35)、中度(0.35~0.66)、高度(0.66~0.84)和重度(>0.84)损伤4个程度.所建立模型适用于不同配筋率的全珊瑚混凝土板构件损伤评估. 展开更多
关键词 高强全珊瑚钢筋混凝土板 配筋率 声发射 破坏特性 损伤评估
下载PDF
陡倾片麻岩滑坡演化过程研究——以兰陵溪滑坡为例
6
作者 王建平 马思哲 党超 《人民长江》 北大核心 2024年第6期152-158,共7页
弯曲-倾倒破坏是陡倾顺层岩质斜坡的一种变形模式,当其折断面贯通形成滑移面时,斜坡演化为滑坡。以三峡库区兰陵溪滑坡为例,引入反转应力法、梁板强度理论对滑坡变形模式与演化过程进行了研究。结果表明:①该岩质斜坡具有典型的陡倾顺... 弯曲-倾倒破坏是陡倾顺层岩质斜坡的一种变形模式,当其折断面贯通形成滑移面时,斜坡演化为滑坡。以三峡库区兰陵溪滑坡为例,引入反转应力法、梁板强度理论对滑坡变形模式与演化过程进行了研究。结果表明:①该岩质斜坡具有典型的陡倾顺层、岩体结构软硬相间的特点,为其发生弯曲-倾倒破坏提供了先天性条件。②差异性风化是兰陵溪滑坡发生弯曲-倾倒变形的主要原因,片状片麻岩抗弯强度变弱,促使片麻岩逐渐发生弯曲,最后产生弯曲折断-倾倒变形破坏。③兰陵溪滑坡演化过程历经差异性风化、岩层弯曲变形、岩层倾倒破坏、折断面贯通等4个阶段,所有折断面贯通形成潜在滑移面时,斜坡演化为滑坡。研究成果可为该滑坡工程治理提供理论依据,也可为同类型岩质斜坡治理提供思路。 展开更多
关键词 陡倾顺层岩质斜坡 弯曲-倾倒破坏 软硬相间 差异性风化 反转应力法 梁板强度理论 兰陵溪滑坡 三峡库区
下载PDF
钢筋桁架叠合板楼盖模板支架合理拆除时间研究
7
作者 张卫军 钱逢君 +4 位作者 陈兴生 李辉 蔡青松 李猛 葛承坤 《建筑施工》 2024年第2期271-273,277,共4页
针对现有装配整体式楼盖的模板支架计算通常是等同于现浇结构,未计入预制底板的刚度和承载能力等有利因素,而造成模板支架拆除时间较晚,经济效益和工期效益不良的问题,结合工程实际进行了模板支架最佳拆除时间的研究。现场测试结果及理... 针对现有装配整体式楼盖的模板支架计算通常是等同于现浇结构,未计入预制底板的刚度和承载能力等有利因素,而造成模板支架拆除时间较晚,经济效益和工期效益不良的问题,结合工程实际进行了模板支架最佳拆除时间的研究。现场测试结果及理论计算表明,在一定跨度条件下,考虑预制底板的刚度和承载能力贡献,现场可以实现板底支架的提前拆除,相关研究结论可为类似工程提供参考。 展开更多
关键词 钢筋桁架叠合板 模板支架 拆除时间 混凝土早龄期强度
下载PDF
不同熔剂体系制备的陶瓷岩板及其性能
8
作者 赵存河 聂光临 +4 位作者 刘一军 左飞 庞伟科 汪庆刚 包亦望 《硅酸盐通报》 CAS 北大核心 2024年第9期3386-3398,共13页
本文利用钾钠质与钙镁质原料配制了SiO_(2)-Al_(2)O_(3)-K_(2)O(Na_(2)O)(K_(2)O-Na_(2)O)与SiO_(2)-Al_(2)O_(3)-CaO-MgO(CaO-MgO)体系陶瓷,系统探究了熔剂体系(CaO-MgO、K_(2)O-Na_(2)O)在不同烧结温度(1 110~1 210℃)下对陶瓷岩板烧... 本文利用钾钠质与钙镁质原料配制了SiO_(2)-Al_(2)O_(3)-K_(2)O(Na_(2)O)(K_(2)O-Na_(2)O)与SiO_(2)-Al_(2)O_(3)-CaO-MgO(CaO-MgO)体系陶瓷,系统探究了熔剂体系(CaO-MgO、K_(2)O-Na_(2)O)在不同烧结温度(1 110~1 210℃)下对陶瓷岩板烧结性能和力学性能的影响,并利用XRD和SEM研究陶瓷岩板的物相组成和显微结构演变规律。结果表明:CaO-MgO与K_(2)O-Na_(2)O体系陶瓷的最佳烧结温度分别为1 170、1 150℃,钙镁质原料的引入导致CaO-MgO体系陶瓷的烧成收缩率与体积密度均低于K_(2)O-Na_(2)O体系陶瓷,且CaO-MgO体系陶瓷中气孔尺寸与含量均大于K_(2)O-Na_(2)O体系陶瓷;钙镁质原料的引入会促进CaO-MgO体系陶瓷中钙长石与α-堇青石的形成,且可以大幅度提升CaO-MgO体系的结晶相含量(质量分数为75.66%,较K_(2)O-Na_(2)O体系高56%)。高结晶相含量导致的弥散强化效果大于气孔对强度的劣化作用,CaO-MgO体系的弯曲强度为(56.9±2.6) MPa、断裂功为(183.2±9.5) J/m^(2)、极限应变为(7.4±0.1)×10^(-4)、比强度为(24.9±1.1) kN·m·kg^(-1),较K_(2)O-Na_(2)O体系分别提高了15%、25%、11%、23%,这说明CaO-MgO熔剂体系陶瓷更加适用于高强韧、高柔性陶瓷岩板的制备。 展开更多
关键词 陶瓷岩板 熔剂体系 烧成温度 力学性能 弯曲强度 断裂功 物相组成 微观结构
下载PDF
某大跨度异形板的结构设计与分析 被引量:1
9
作者 张志华 李祖维 《广东土木与建筑》 2024年第2期80-82,共3页
以广州某住宅楼大跨度异形板为例,针对大跨度异形板及周边剪力墙容易出现裂缝的问题,通过强度设计、挠度裂缝分析、温度应力分析、舒适度分析、剪力墙平面外强度分析等设计方法,提出防止出现裂缝问题的措施在于大跨度异形板不仅要加强构... 以广州某住宅楼大跨度异形板为例,针对大跨度异形板及周边剪力墙容易出现裂缝的问题,通过强度设计、挠度裂缝分析、温度应力分析、舒适度分析、剪力墙平面外强度分析等设计方法,提出防止出现裂缝问题的措施在于大跨度异形板不仅要加强构造,还应在计算中同时满足强度计、裂缝计算、温度应力计算、舒适度计算、剪力墙平面外强度计算,以此满足结构安全和使用舒适度要求。 展开更多
关键词 大跨度异形板 挠度裂缝 温度应力 舒适度 剪力墙平面外强度
下载PDF
钢-UHPC组合板受弯性能的试验研究 被引量:45
10
作者 李文光 邵旭东 +1 位作者 方恒 张哲 《土木工程学报》 EI CSCD 北大核心 2015年第11期93-102,共10页
提出钢-UHPC轻型组合桥面系,以消除正交异性钢桥面铺装层易损和钢桥面板疲劳开裂两类病害。为探究该组合桥面系在局部轮载作用下的横向受弯性能,对10块钢-UHPC组合板进行试验研究与理论分析。试验结果表明:负弯矩作用下,组合板的弹性... 提出钢-UHPC轻型组合桥面系,以消除正交异性钢桥面铺装层易损和钢桥面板疲劳开裂两类病害。为探究该组合桥面系在局部轮载作用下的横向受弯性能,对10块钢-UHPC组合板进行试验研究与理论分析。试验结果表明:负弯矩作用下,组合板的弹性阶段取决于UHPC的弹性性能;保护层厚度与截面配筋率对UHPC开裂影响十分显著;纵向配筋率越高,纯弯段裂缝分布越密集;当裂缝宽度小于0.2mm时,荷载与最大裂缝宽度关系近似线性;破坏形态为UHPC层受拉断裂。正弯矩作用下,组合板的弹性阶段取决于钢板与UHPC层界面的自然黏结强度;纯弯段裂缝间距几乎与横向钢筋的间距相同;在极限荷载前,荷载与最大裂缝宽度关系近似线性;钢板将纯弯段UHPC最大裂缝宽度有效限制在0.2mm左右;破坏形态为剪跨区栓钉被剪断。按截面换算法计算UHPC的开裂强度为18.1~32.7MPa,满足工程要求;按塑性分析方法计算钢-UHPC组合板的抗弯承载力,与试验值吻合较好。 展开更多
关键词 超高性能混凝土 钢-UHPC组合板 开裂强度 最大裂缝宽度 抗弯承载力
下载PDF
Q235G钢连铸坯的高温力学性能分析 被引量:33
11
作者 陈登福 高兴健 +2 位作者 王启明 王水根 宋立伟 《过程工程学报》 CAS CSCD 北大核心 2009年第S1期210-213,共4页
采用Gleeble-1500D热/力模拟试验机,测试了Q235G钢连铸板坯的高温力学性能,获得600~1300℃范围内铸坯的高温强度、热塑性和高温塑性模量随温度的变化规律.测试结果表明,Q235G钢铸坯的高温强度较小,600℃时抗拉强度约164MPa,屈服强度和... 采用Gleeble-1500D热/力模拟试验机,测试了Q235G钢连铸板坯的高温力学性能,获得600~1300℃范围内铸坯的高温强度、热塑性和高温塑性模量随温度的变化规律.测试结果表明,Q235G钢铸坯的高温强度较小,600℃时抗拉强度约164MPa,屈服强度和抗拉强度均随测试温度降低而增大;铸坯具有良好的塑性,脆性区温度范围较窄,第I脆性温度范围为1300℃至熔点,第III脆性温度范围为750~850℃,在850~1250℃内,该钢种连铸坯的断面收缩率均大于85%.Q235G钢连铸坯的高温塑性模量随测试温度降低而增大,且塑性模量值较小,铸坯可以承受较大的均匀塑性变形. 展开更多
关键词 Q235G钢连铸坯 高温强度 断面收缩率 塑性模量
下载PDF
肋形楼盖的一种有限元算法及内力分布 被引量:16
12
作者 丁圣果 刘广宁 李绮文 《建筑结构》 CSCD 北大核心 1999年第6期46-50,共5页
肋形楼盖是梁板协同工作体系,作者提出以十字交叉梁系杆元及矩形四节点板元共同集成总刚计算助形楼盖的直接刚度法,较传统的内力计算方法更为精确。对大量算例结果的分析表明:一般现浇板在次梁位置受正弯矩作用(下缘受拉);考虑梁... 肋形楼盖是梁板协同工作体系,作者提出以十字交叉梁系杆元及矩形四节点板元共同集成总刚计算助形楼盖的直接刚度法,较传统的内力计算方法更为精确。对大量算例结果的分析表明:一般现浇板在次梁位置受正弯矩作用(下缘受拉);考虑梁板协同作用,结构刚度可以提高30%左右。 展开更多
关键词 楼盖 有限元法 内力分布 钢筋混凝土 肋形楼盖
下载PDF
钢纤维高强混凝土方形冲切板的变形与强度 被引量:6
13
作者 林旭健 钱在兹 郑作樵 《土木工程学报》 EI CSCD 北大核心 2004年第12期23-28,共6页
通过试验 ,研究钢纤维高强混凝土方形冲切板的变形和强度性能 ,认为板在冲切破坏之前发生的变形主要是弯曲变形 ,该变形反映了板在各个受力阶段的抗弯性能 ,也在很大程度上直接影响着冲切锥面上的应力分布和板面钢筋的抗冲切能力。对方... 通过试验 ,研究钢纤维高强混凝土方形冲切板的变形和强度性能 ,认为板在冲切破坏之前发生的变形主要是弯曲变形 ,该变形反映了板在各个受力阶段的抗弯性能 ,也在很大程度上直接影响着冲切锥面上的应力分布和板面钢筋的抗冲切能力。对方形冲切板在各个受力阶段的挠度进行了计算 ,并在分析试验结果的基础上 ,建立了考虑受弯变形的冲切破坏机构 ,提出板的极限强度由冲切锥抗冲切力和板的部分抗弯能力组成。对冲切板变形和强度的计算结果与实测值吻合良好。 展开更多
关键词 钢纤维高强混凝土 冲切板 挠度 强度
下载PDF
基于轨道板抗弯疲劳强度的不均匀沉降控制 被引量:10
14
作者 陈仁朋 王作洲 +1 位作者 蒋红光 边学成 《浙江大学学报(工学版)》 EI CAS CSCD 北大核心 2013年第5期796-802,共7页
为了研究高速铁路无砟轨道路基不均匀沉降对轨道板受力的影响及基于轨道板疲劳强度的不均匀沉降控制标准.以京沪高铁工程为背景,建立20、30、40、50、75、100m等不同弦长以及0到100mm不同沉降幅值的余弦式不均匀沉降分析模型,研究轨道... 为了研究高速铁路无砟轨道路基不均匀沉降对轨道板受力的影响及基于轨道板疲劳强度的不均匀沉降控制标准.以京沪高铁工程为背景,建立20、30、40、50、75、100m等不同弦长以及0到100mm不同沉降幅值的余弦式不均匀沉降分析模型,研究轨道板上的弯矩分布规律,比较分析沉降曲线始端截面与中间截面的弯矩规律.基于轨道板混凝土疲劳强度史密斯设计图,确定轨道板的动力疲劳强度允许值,并基于轨道板抗弯疲劳强度提出高铁路基中长波不均匀沉降的控制准则. 展开更多
关键词 高速铁路 不均匀沉降 疲劳强度 轨道板
下载PDF
水泥混凝土路面断板、破碎板维修方法试验研究 被引量:2
15
作者 战高峰 苗若愚 +2 位作者 杨兆升 李玉良 高群 《公路交通科技》 EI CAS CSCD 北大核心 1998年第1期19-21,共3页
结合工程实际研究用于水泥混凝土路面维修的早强混凝土,并对水泥砼路面断板和破碎板的维修进行了试验研究,工程应用结果表明,文中的方法可行并具有一定的实用性。
关键词 维修 早强混凝土 水泥混凝土路面 断板 破碎板
下载PDF
复合剪力墙板抗剪承载力计算方法的探讨 被引量:6
16
作者 李升才 江见鲸 于庆荣 《建筑结构》 CSCD 北大核心 2001年第9期32-33,27,共3页
对CL(CompositeLight weight)体系中复合墙板的抗剪试验测得的抗剪承载力结果与各国理论公式计算值进行了对比分析 ,从而提出CL体系中复合剪力墙板的抗剪承载力理论计算公式 ,并由试验结果确定了公式中的系数。应用该公式可计算复合剪... 对CL(CompositeLight weight)体系中复合墙板的抗剪试验测得的抗剪承载力结果与各国理论公式计算值进行了对比分析 ,从而提出CL体系中复合剪力墙板的抗剪承载力理论计算公式 ,并由试验结果确定了公式中的系数。应用该公式可计算复合剪力墙板的极限抗剪承载力 ,或确定墙板的厚度和配筋。 展开更多
关键词 复合剪力墙板 抗剪承载力 计算公式 配筋
下载PDF
高温下压型钢板-混凝土粘结强度的试验 被引量:12
17
作者 蒋首超 李国强 李明菲 《同济大学学报(自然科学版)》 EI CAS CSCD 北大核心 2003年第3期273-276,共4页
对我国常用的一种类型的压型钢板与混凝土在常温下的粘结应力 -滑移关系及高温下的粘结强度进行了试验研究 .研究结果表明压型钢板与混凝土间的粘结强度随温度的升高而迅速下降 .通过对试验结果的分析 。
关键词 组合楼板 抗火 粘结强度 粘结应力-滑移关系
下载PDF
板式轨道用高弹模水泥沥青砂浆与混凝土黏结性能的试验研究 被引量:9
18
作者 元强 郭建光 +3 位作者 邓德华 谢友均 王世雄 曾志平 《铁道科学与工程学报》 CAS CSCD 北大核心 2013年第6期40-44,共5页
采用一种直接拉伸法试验研究了水泥乳化沥青砂浆与支承层混凝土(C15)、底座板混凝土(C30)和轨道板蒸养混凝土(C55)的黏结强度及其影响因素。试验结果表明:砂浆配合比(用水量)对砂浆与轨道板蒸养混凝土、底座板混凝土及支承层混凝土的黏... 采用一种直接拉伸法试验研究了水泥乳化沥青砂浆与支承层混凝土(C15)、底座板混凝土(C30)和轨道板蒸养混凝土(C55)的黏结强度及其影响因素。试验结果表明:砂浆配合比(用水量)对砂浆与轨道板蒸养混凝土、底座板混凝土及支承层混凝土的黏结强度影响很小;混凝土表面拉毛显著提高了黏结强度;板腔的润湿状态对砂浆充填层与混凝土的黏结力影响很大;黏结强度随龄期增加而增加,在7 d龄期时已基本达到最大值。 展开更多
关键词 水泥沥青砂浆 CRTS II型板式轨道结构 黏结强度 混凝土
下载PDF
混凝土板的冲切强度 被引量:3
19
作者 杨雪强 李子生 梁仕华 《应用力学学报》 CAS CSCD 北大核心 2009年第4期731-735,共5页
基于混凝土强度的试验资料,首先建立了合理描述混凝土强度破坏特性的Lade-Duncan破坏准则,并将该Lade-Duncan破坏准则转化为等效的Mohr-Coulomb破坏准则。依据塑性上限分析理论和合理的混凝土板冲切强度破坏模式,求出了圆形和矩形分布... 基于混凝土强度的试验资料,首先建立了合理描述混凝土强度破坏特性的Lade-Duncan破坏准则,并将该Lade-Duncan破坏准则转化为等效的Mohr-Coulomb破坏准则。依据塑性上限分析理论和合理的混凝土板冲切强度破坏模式,求出了圆形和矩形分布荷载下混凝土板冲切强度的统一表达式。通过与已发表的研究成果、试验结果和规范公式相比较,论证了本文给出的混凝土板冲切强度公式的合理性。 展开更多
关键词 Lade—Duncan破坏准则 塑性上限理论 混凝土板 冲切强度
下载PDF
钢塑轻质板的正截面抗弯承载能力 被引量:3
20
作者 林子臣 孙纲廷 《建筑结构》 CSCD 北大核心 1996年第9期49-51,共3页
经简化分析建立了钢塑轻质板正截面抗弯承载力计算公式,并提出了板的改制方法.试验表明,改制板的承载能力和变形能力均有较大提高,且理论计算与实测承载力吻合较好;未改制的钢塑板呈少筋脆性破坏特征.无论改制与否这种板仅能单向传力.
关键词 钢塑轻质板 抗弯承载力 正截面 计算
下载PDF