Developing effective strategies to improve the initial Coulombic efficiency(ICE)and cycling stability of hard carbon(HC)anodes for sodium-ion batteries is the key to promoting the commercial application of HC.In this ...Developing effective strategies to improve the initial Coulombic efficiency(ICE)and cycling stability of hard carbon(HC)anodes for sodium-ion batteries is the key to promoting the commercial application of HC.In this paper,homotype heterojunctions are designed on HC to induce the generation of stable solid electrolyte interfaces,which can effectively increase the ICE of HC from 64.7%to 81.1%.The results show that using a simple surface engineering strategy to construct a homotypic amorphous Al_(2)O_(3) layer on the HC could shield the active sites,and further inhibit electrolyte decomposition and side effects occurrence.Particularly,due to the suppression of continuous decomposition of NaPF 6 in ester-based electrolytes,the accumulation of NaF could be reduced,leading to the formation of thinner and denser solid electrolyte interface films and a decrease in the interface resistance.The HC anode can not only improve the ICE but elevate its sodium storage performance based on this homotype heterojunction composed of HC and Al_(2)O_(3).The optimized HC anode exhibits an outstanding reversible capacity of 321.5mAhg^(−1) at 50mAg^(−1).The cycling stability is also improved effectively,and the capacity retention rate is 86.9%after 2000 cycles at 1Ag^(−1) while that of the untreated HC is only 52.6%.More importantly,the improved sodium storage behaviors are explained by electrochemical kinetic analysis.展开更多
The rapid development of new energy vehicles and 5G communication technologies has led to higher demands for the safety,energy density,and cycle performance of lithium-ion batteries as power sources.However,the curren...The rapid development of new energy vehicles and 5G communication technologies has led to higher demands for the safety,energy density,and cycle performance of lithium-ion batteries as power sources.However,the currently used liquid carbonate compounds in commercial lithium-ion battery electrolytes pose potential safety hazards such as leakage,swelling,corrosion,and flammability.Solid electrolytes can be used to mitigate these risks and create a safer lithium battery.Furthermore,high-energy density can be achieved by using solid electrolytes along with high-voltage cathode and metal lithium anode.Two types of solid electrolytes are generally used:inorganic solid electrolytes and polymer solid electrolytes.Inorganic solid electrolytes have high ionic conductivity,electrochemical stability window,and mechanical strength,but suffer from large solid/solid contact resistance between the electrode and electrolyte.Polymer solid electrolytes have good flexibility,processability,and contact interface properties,but low room temperature ionic conductivity,necessitating operation at elevated temperatures.Composite solid electrolytes(CSEs) are a promising alternative because they offer light weight and flexibility,like polymers,as well as the strength and stability of inorganic electrolytes.This paper presents a comprehensive review of recent advances in CSEs to help researchers optimize CSE composition and interactions for practical applications.It covers the development history of solid-state electrolytes,CSE properties with respect to nanofillers,morphology,and polymer types,and also discusses the lithium-ion transport mechanism of the composite electrolyte,and the methods of engineering interfaces with the positive and negative electrodes.Overall,the paper aims to provide an outlook on the potential applications of CSEs in solid-state lithium batteries,and to inspire further research aimed at the development of more systematic optimization strategies for CSEs.展开更多
Sulfide solid electrolytes are promising for high energy density and safety in all-solid-state batteries due to their high ionic conductivity and good mechanical properties.However,the application of sulfide solid ele...Sulfide solid electrolytes are promising for high energy density and safety in all-solid-state batteries due to their high ionic conductivity and good mechanical properties.However,the application of sulfide solid electrolytes in all-solid-state batteries with lithium anode is restricted by the side reactions at lithium/electrolytes interfaces and the growth of lithium dendrite caused by nonuniform lithium deposition.Herein,a homogeneous LiF-Li_(3)N composite protective layer is in situ formed via a manipulated reaction of pentafluorobenzamide with Li metal.The LiF-Li_(3)N layer with both high interfacial energy and interfacial adhesion energy can synergistically suppress side reactions and inhibit the growth of lithium dendrite,achieving uniform deposition of lithium.The critical current densities of Li_(10)GeP_(2)S_(12)and Li_(6)PS_(5)Cl are increased to 3.25 and 1.25 mA cm^(-2)with Li@LiF-Li_(3)N layer,which are almost triple and twice as those of Li-symmetric cells in the absence of protection layer,respectively.Moreover,the Li@LiF-Li_(3)N/Li10GeP2S12/Li@LiF-Li_(3)N cell can stably cycle for 9000 h at 0.1 mA cm^(-2)under 0.1 mA h cm^(-2),and Li@LiF-Li_(3)N/Li_(6)PS_(5)Cl/Li@LiF-Li_(3)N cell achieves stable Li plating/stripping for 8000 h at 0.1 mA cm^(-2)under10 m A h cm^(-2).The improved dynamic stability of lithium plating/stripping in Li@LiF-Li_(3)N/Li_(10)GeP_(2)S_(12)or Li_(6)PS_(5)Cl interfaces is proved by three-electrode cells.As a result,LiCoO_(2)/electrolytes/Li@LiF-Li_(3)N batteries with Li_(10)GeP_(2)S_(12)and Li_(6)PS_(5)Cl exhibit remarkable cycling stability of 500 cycles with capacity retentions of 93.5%and 89.2%at 1 C,respectively.展开更多
All-solid-state lithium metal batteries(ASSLMBs)are considered as one of the ultimate goals for the development of energy storage systems due to their high energy density and high safety.However,the mismatching of int...All-solid-state lithium metal batteries(ASSLMBs)are considered as one of the ultimate goals for the development of energy storage systems due to their high energy density and high safety.However,the mismatching of interface transport kinetics as well as interfacial instability induces the growth of lithium dendrite and thus,leads to severe degradation of battery electrochemical performances.Herein,an integrated interface configuration(IIC)consisting of in-situ generated Li I interphase and Li-Ag alloy anode is proposed through in-situ interface chemistry.The IIC is capable of not only regulating charge transport kinetics but also synchronously stabilizing the lithium/electrolyte interface,thereby achieving uniform lithium platting.Therefore,Li||Li symmetric cells with IIC achieve a critical current density of up to 1.6 mA cm^(-2)and achieve stable cycling over 1600 hours at a high current density of 0.5 mA cm^(-2).Moreover,a high discharge capacity of 140.1 mA h g-1at 0.1 C is also obtained for the Li(Ni_(0.6)Co_(0.2)Mn_(0.2))O_(2)(NCM622)full battery with a capacity retention of 65.6%after 300 cycles.This work provides an effective method to synergistically regulate the interface transport kinetics and inhibit lithium dendrite growth for high-performance ASSLMBs.展开更多
Succinonitrile-based plastic crystal electrolytes have emerged for high-energy-density Li metal batteries in terms of their superior ambient ionic conductivity,low flammability,and benign compatibility with high volta...Succinonitrile-based plastic crystal electrolytes have emerged for high-energy-density Li metal batteries in terms of their superior ambient ionic conductivity,low flammability,and benign compatibility with high voltage cathode,but are hampered by inherent instabilities toward Li anodes.Constructing hierarchical solid electrolytes structure is a fundamental approach to protect Li anode from succinonitrile attacks,with succinonitrile-based oxidation-resistance layer facing high voltage cathode and reduction-tolerant layer contacting Li anode.However,free succinonitrile molecules in succinonitrile-based electrolyte layer can diffuse across the electrolyte/electrolyte interface and further reach Li anode surface during the battery cycle.This chemical“crosstalk”cause reduction-tolerant electrolyte layer to fail to protect the Li anode from the attacks of free succinonitrile molecules.Nano Li_(6.4)La_(3)Zr_(1.4)Ta_(0.6)O_(12)is introduced creatively into succinonitrile-based electrolyte layer.By taking advantage of the complexation between La atoms in Li_(6.4)La_(3)Zr_(1.4)Ta_(0.6)O_(12)and N atoms in succinonitrile,the free succinonitrile molecules are successfully immobilized in succinonitrile-based electrolyte layer.The resulting low resistance and highly durable solid electrolyte interphase and cathode electrolyte interphase endow NCM622||Li batteries with remarkable cycle stability.Our research provides a new idea for the real application of plastic crystal electrolytes in high voltage solid-state lithium metal batteries.展开更多
The rapid development and widespread application of lithium-ion batteries(LIBs) have increased demand for high-safety and high-performance LIBs. Accordingly, various additives have been used in commercial liquid elect...The rapid development and widespread application of lithium-ion batteries(LIBs) have increased demand for high-safety and high-performance LIBs. Accordingly, various additives have been used in commercial liquid electrolytes to severally adjust the solvation structure of lithium ions, control the components of solid electrolyte interphase, or reduce flammability. While it is highly desirable to develop low-cost multifunctional electrolyte additives integrally that address both safety and performance on LIBs, significant challenges remain. Herein, a novel phosphorus-containing organic small molecule, bis(2-methoxyethyl) methylphosphonate(BMOP), was rationally designed to serve as a fluorine-free and multifunctional additive in commercial electrolytes. This novel electrolyte additive is low-toxicity,high-efficiency, low-cost, and electrode-compatible, which shows the significant improvement to both electrochemical performance and fire safety for LIBs through regulating the electrolyte solvation structure, constructing the stable electrode-electrolyte interphase, and suppressing the electrolyte combustion. This work provides a new avenue for developing safer and high-performance LIBs.展开更多
Lithium sulfur batteries are regarded as a promising candidate for high-energy-density energy storage devices.However,the lithium metal anode in lithium-sulfur batteries encounters the problem of lithium dendrites and...Lithium sulfur batteries are regarded as a promising candidate for high-energy-density energy storage devices.However,the lithium metal anode in lithium-sulfur batteries encounters the problem of lithium dendrites and lithium metal consumption caused by polysulfide corrosion.Herein we design a dualfunction PMMA/PPC/LiNO3composite as an artificial solid electrolyte interphase(PMCN-SEI)to protect Li metal anode.This SEI offers multiple sites of C=O for polysulfide anchoring to constrain corrosion of Li metal anode.The lithiated polymer group and Li3N in PMCN-SEI can homogenize lithium-ion deposition behavior to achieve a dendrite-free anode.As a result,the PMCN-SEI protected Li metal anode enables the Li||Li symmetric batteries to maintain over 300 cycles(1300 h)at a capacity of 5 m Ah cm^(-2),corresponding to a cumulative capacity of 3.25 Ah cm^(-2).Moreover,Li-S batteries assembled with 20μm of Li metal anode(N/P=1.67)still deliver an initial capacity of 1166 m A h g-1at 0.5C.Hence,introducing polycarbonate polymer/inorganic composite SEI on Li provides a new solution for achieving the high energy density of Li-S batteries.展开更多
The solvent-free in situ polymerization technique has the potential to tailor-make conformal interfaces that are essential for developing durable and safe lithium metal polymer batteries(LMPBs).Hence,much attention ha...The solvent-free in situ polymerization technique has the potential to tailor-make conformal interfaces that are essential for developing durable and safe lithium metal polymer batteries(LMPBs).Hence,much attention has been given to the eco-friendly and rapid ultraviolet(UV)-induced in situ photopolymerization process to prepare solid-state polymer electrolytes.In this respect,an innovative method is proposed here to overcome the challenges of UV-induced photopolymerization(UV-curing)in the zones where UV-light cannot penetrate,especially in LMPBs where thick electrodes are used.The proposed frontal-inspired photopolymerization(FIPP)process is a diverged frontal-based technique that uses two classes(dual)of initiators to improve the slow reaction kinetics of allyl-based monomers/oligomers by at least 50%compared with the conventional UV-curing process.The possible reaction mechanism occurring in FIPP is demonstrated using density functional theory calculations and spectroscopic investigations.Indeed,the initiation mechanism identified for the FIPP relies on a photochemical pathway rather than an exothermic propagating front forms during the UV-irradiation step as the case with the classical frontal photopolymerization technique.Besides,the FIPP-based in situ cell fabrication using dual initiators is advantageous over both the sandwich cell assembly and conventional in situ photopolymerization in overcoming the limitations of mass transport and active material utilization in high energy and high power LMPBs that use thick electrodes.Furthermore,the LMPB cells fabricated using the in situ-FIPP process with high mass loading LiFePO_(4)electrodes(5.2 mg cm^(-2))demonstrate higher rate capability,and a 50%increase in specific capacity against a sandwich cell encouraging the use of this innovative process in large-scale solid-state battery production.展开更多
Due to its high theoretical capacity(820 mAh g^(−1)),low standard electrode potential(−0.76 V vs.SHE),excellent stability in aqueous solutions,low cost,environmental friendliness and intrinsically high safety,zinc(Zn)...Due to its high theoretical capacity(820 mAh g^(−1)),low standard electrode potential(−0.76 V vs.SHE),excellent stability in aqueous solutions,low cost,environmental friendliness and intrinsically high safety,zinc(Zn)-based batteries have attracted much attention in developing new energy storage devices.In Zn battery system,the battery performance is significantly affected by the solid electrolyte interface(SEI),which is controlled by electrode and electrolyte,and attracts dendrite growth,electrochemical stability window range,metallic Zn anode corrosion and passivation,and electrolyte mutations.Therefore,the design of SEI is decisive for the overall performance of Zn battery systems.This paper summarizes the formation mechanism,the types and characteristics,and the characterization techniques associated with SEI.Meanwhile,we analyze the influence of SEI on battery performance,and put forward the design strategies of SEI.Finally,the future research of SEI in Zn battery system is prospected to seize the nature of SEI,improve the battery performance and promote the large-scale application.展开更多
In the past few years,the all-solid lithium battery has attracted worldwide attentions,the ionic conductivity of some all-solid lithium-ion batteries has reached 10^(-3)-10^(-2) S/cm,indicating that the transport of l...In the past few years,the all-solid lithium battery has attracted worldwide attentions,the ionic conductivity of some all-solid lithium-ion batteries has reached 10^(-3)-10^(-2) S/cm,indicating that the transport of lithium ions in solid electrolytes is no longer a major problem.However,some interface issues become research hotspots.Examples of these interfacial issues include the electrochemical decomposition reaction at the electrode-electrolyte interface;the low effective contact area between the solid electrolyte and the electrode etc.In order to solve the issues,researchers have pursued many different approaches.The addition of a buffer layer between the electrode and the solid electrolyte has been at the center of this endeavor.In this review paper,we provide a systematic summarization of the problems on the electrode-solid electrolyte interface and detailed reflection on the latest works of buffer-based therapies,and the review will end with a personal perspective on the improvement of buffer-based therapies.展开更多
All-solid-state lithium batteries(ASSLBs) employing sulfide electrolyte and lithium(Li) anode have received increasing attention due to the intrinsic safety and high energy density.However,the thick electrolyte layer ...All-solid-state lithium batteries(ASSLBs) employing sulfide electrolyte and lithium(Li) anode have received increasing attention due to the intrinsic safety and high energy density.However,the thick electrolyte layer and lithium dendrites formed at the electrolyte/Li anode interface hinder the realization of high-performance ASSLBs.Herein,a novel membrane consisting of Li_(6)PS_(5) Cl(LPSCl),poly(ethylene oxide)(PEO) and Li-salt(LiTFSI) was prepared as sulfide-based composite solid electrolyte(LPSCl-PEO3-LiTFSI)(LPSCl:PEO=97:3 wt/wt;EO:Li=8:1 mol/mol),which delivers high ionic conductivity(1.1 × 10^(-3) S cm^(-1)) and wide electrochemical window(4.9 V vs.Li^(+)/Li) at 25 ℃.In addition,an ex-situ artificial solid electrolyte interphase(SEI) film enriched with LiF and Li3 N was designed as a protective layer on Li anode(Li(SEI)) to suppress the growth of lithium dendrites.Benefiting from the synergy of sulfide-based composite solid electrolyte and ex-situ artificial SEI,cells of S-CNTs/LPSCI-PEO3-LiTFSI/Li(SEI) and Al_(2)O_(3)@LiNi_(0.5)Co_(0.3)Mn_(0.2)O_(2)/LPSCl-PEO3-LiTFSI/Li(SEI) are assembled and both exhibit high initial discharge capacity of 1221.1 mAh g^(-1)(135.8 mAh g^(-1)) and enhanced cycling stability with 81.6% capacity retention over 200 cycles at 0.05 C(89.2% over 100 cycles at 0.1 C).This work provides a new insight into the synergy of composite solid electrolyte and artificial SEI for achieving high-performance ASSLBs.展开更多
Transition metal selenides have been widely studied as anode materials of sodium ion batteries(SIBs),however,the investigation of solid-electrolyte-interface(SEI)on these materials,which is critical to the electrochem...Transition metal selenides have been widely studied as anode materials of sodium ion batteries(SIBs),however,the investigation of solid-electrolyte-interface(SEI)on these materials,which is critical to the electrochemical performance of SIBs,remains at its infancy.Here in this paper,ZnSe@C nanoparticles were prepared from ZIF-8 and the SEI layers on these electrodes with and without reduced graphene oxide(rGO)layers were examined in details by X-ray photoelectron spectroscopies at varied charged/discharged states.It is observed that fast and complicated electrolyte decomposition reactions on ZnSe@C leads to quite thick SEI film and intercalation of solvated sodium ions through such thick SEI film results in slow ion diffusion kinetics and unstable electrode structure.However,the presence of rGO could efficiently suppress the decomposition of electrolyte,thus thin and stable SEI film was formed.ZnSe@C electrodes wrapped by rGO demonstrates enhanced interfacial charge transfer kinetics and high electrochemical performance,a capacity retention of 96.4%,after 1000 cycles at 5 A/g.This study might offer a simple avenue for the designing high performance anode materials through manipulation of SEI film.展开更多
The specific energy of Li metal batteries(LMBs)can be improved by using high‐voltage cathode materials;however,achieving long‐term stable cycling performance in the corresponding system is particularly challenging f...The specific energy of Li metal batteries(LMBs)can be improved by using high‐voltage cathode materials;however,achieving long‐term stable cycling performance in the corresponding system is particularly challenging for the liquid electrolyte.Herein,a novel pseudo‐oversaturated electrolyte(POSE)is prepared by introducing 1,1,2,2‐tetrafluoroethyl‐2,2,3,3‐tetrafluoropropyl ether(TTE)to adjust the coordination structure between diglyme(G2)and lithium bis(trifluoromethanesulfonyl)imide(LiTFSI).Surprisingly,although TTE shows little solubility to LiTFSI,the molar ratio between LiTFSI and G2 in the POSE can be increased to 1:1,which is much higher than that of the saturation state,1:2.8.Simulation and experimental results prove that TTE promotes closer contact of the G2 molecular with Li^(+)in the POSE.Moreover,it also participates in the formation of electrolyte/electrode interphases.The electrolyte shows outstanding compatibility with both the Li metal anode and typical high‐voltage cathodes.Li||Li symmetric cells show a long life of more than 2000 h at 1 mA cm^(−2),1 mAh cm^(−2).In the meantime,Li||LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2)(NCM811)cell with the POSE shows a high reversible capacity of 134.8 mAh g^(−1 )after 900 cycles at 4.5 V,1 C rate.The concept of POSE can provide new insight into the Li^(+)solvation structure and in the design of advanced electrolytes for LMBs.展开更多
The widespread adoption of lithium-ion batteries has been driven by the proliferation of portable electronic devices and electric vehicles,which have increasingly stringent energy density requirements.Lithium metal ba...The widespread adoption of lithium-ion batteries has been driven by the proliferation of portable electronic devices and electric vehicles,which have increasingly stringent energy density requirements.Lithium metal batteries(LMBs),with their ultralow reduction potential and high theoretical capacity,are widely regarded as the most promising technical pathway for achieving high energy density batteries.In this review,we provide a comprehensive overview of fundamental issues related to high reactivity and migrated interfaces in LMBs.Furthermore,we propose improved strategies involving interface engineering,3D current collector design,electrolyte optimization,separator modification,application of alloyed anodes,and external field regulation to address these challenges.The utilization of solid-state electrolytes can significantly enhance the safety of LMBs and represents the only viable approach for advancing them.This review also encompasses the variation in fundamental issues and design strategies for the transition from liquid to solid electrolytes.Particularly noteworthy is that the introduction of SSEs will exacerbate differences in electrochemical and mechanical properties at the interface,leading to increased interface inhomogeneity—a critical factor contributing to failure in all-solidstate lithium metal batteries.Based on recent research works,this perspective highlights the current status of research on developing high-performance LMBs.展开更多
Solid polymer electrolytes(SPEs)are highly promising for realizing high-capacity,low-cost,and safe Li metal batteries.However,the Li dendritic growth and side reactions between Li and SPEs also plague these systems.He...Solid polymer electrolytes(SPEs)are highly promising for realizing high-capacity,low-cost,and safe Li metal batteries.However,the Li dendritic growth and side reactions between Li and SPEs also plague these systems.Herein,a fluorinated lithium salt coating(FC)with organic-inorganic gradient and soft–rigid feature is introduced on Li surface as an artificial protective layer by the in-situ reaction between Li metal and fluorinated carboxylic acid.The FC layer can improve the interface stability and wettability between Li and SPEs,assist the transport of Li ions,and guide Li nucleation,contributing to a dendrite-free Li deposition and long-lifespan Li metal batteries.The symmetric cell with FC-Li anodes exhibits a high areal capacity of 1 mAh cm^(-2)at 0.5 mA cm^(-2),and an ultra-long lifespan of 2000 h at a current density of 0.1 mA cm^(-2).Moreover,the full cell paired with the LiFePO4 cathode exhibits improved cycling stability,remaining 83.7%capacity after 500 cycles at 1 C.When matching with the S cathode,the FC layer can prevent the shuttle effect,contributing to stable and high-capacity Li–S battery.This work provided a promising way for the construction of stable all-solid-state lithium metal batteries with prolonged lifespan.展开更多
Owing to its low potential, crustal abundances and environmental friendliness, calcium metal anode(CMA) is emerging as a powerful contender in post-lithium era. However, the passivation of CMA fatally hinders its deve...Owing to its low potential, crustal abundances and environmental friendliness, calcium metal anode(CMA) is emerging as a powerful contender in post-lithium era. However, the passivation of CMA fatally hinders its development. Recently, several feasible electrolytes have been developed. Nevertheless, as a pivotal part, the solid electrolyte interface(SEI) formed on CMA has not been paid enough attention to. In this review, based on the passivation mechanism of CMA, the favorable composition of SEI is emphasized with the corresponding electrolytes. It is considered that boron-containing and organic–inorganic hybrid SEI might be preferred. By comparing electrolytes and SEI on CMA with lithium and magnesium metal anodes, the root causes of CMA passivation are further elaborated, enlightening rational design rules of suitable SEI. Furthermore, some noteworthy details when assembling secondary calcium metal batteries(CMBs) are put forward. It is expected that deeper understanding of SEI on CMA will promote the development of CMBs.展开更多
The scientific basis of all-solid-state lithium batteries with inorganic solid electrolytes is reviewed briefly, touching upon solid electrolytes, electrode materials, electrolyte/electrode interface phenomena, fabric...The scientific basis of all-solid-state lithium batteries with inorganic solid electrolytes is reviewed briefly, touching upon solid electrolytes, electrode materials, electrolyte/electrode interface phenomena, fabrication, and evaluation. The challenges and prospects are outlined as well.展开更多
Lithium-ion battery has greatly changed our lifestyle and the solid electrolyte interphase(SEI)covered on the graphite anode determines the service life of a battery.The formation method and the formation temperature ...Lithium-ion battery has greatly changed our lifestyle and the solid electrolyte interphase(SEI)covered on the graphite anode determines the service life of a battery.The formation method and the formation temperature at initial cycle of a battery determine the feature of the SEI.Herein,we investigate the gap of formation behavior in both a half cell(graphite matches with lithium anode)and a full cell(graphite matches with NCM,short for LiNixCoyMn1-x-yO2)at different temperatures.We conclude that high temperature causes severe side reactions and low temperature will result in low ionic conductive SEI layer,the interface formed at room temperature owns the best ionic conductivity and stability.展开更多
基金supported by the National Natural Science Foundation of China(grant nos.21975026 and 22005033)the National Postdoctoral Program of China(no.BX20180037)+1 种基金China Postdoctoral Science Foundation(no.2018M640077)the Beijing Institute of Technology Research Fund Program for Young Scholars(no.XSQD-202108005).
文摘Developing effective strategies to improve the initial Coulombic efficiency(ICE)and cycling stability of hard carbon(HC)anodes for sodium-ion batteries is the key to promoting the commercial application of HC.In this paper,homotype heterojunctions are designed on HC to induce the generation of stable solid electrolyte interfaces,which can effectively increase the ICE of HC from 64.7%to 81.1%.The results show that using a simple surface engineering strategy to construct a homotypic amorphous Al_(2)O_(3) layer on the HC could shield the active sites,and further inhibit electrolyte decomposition and side effects occurrence.Particularly,due to the suppression of continuous decomposition of NaPF 6 in ester-based electrolytes,the accumulation of NaF could be reduced,leading to the formation of thinner and denser solid electrolyte interface films and a decrease in the interface resistance.The HC anode can not only improve the ICE but elevate its sodium storage performance based on this homotype heterojunction composed of HC and Al_(2)O_(3).The optimized HC anode exhibits an outstanding reversible capacity of 321.5mAhg^(−1) at 50mAg^(−1).The cycling stability is also improved effectively,and the capacity retention rate is 86.9%after 2000 cycles at 1Ag^(−1) while that of the untreated HC is only 52.6%.More importantly,the improved sodium storage behaviors are explained by electrochemical kinetic analysis.
基金the support of the Zhejiang Provincial Natural Science Foundation of China (LR20E020002, LD22E020006)the National Natural Science Foundation of China (NSFC) (U20A20253, 21972127, 22279116)。
文摘The rapid development of new energy vehicles and 5G communication technologies has led to higher demands for the safety,energy density,and cycle performance of lithium-ion batteries as power sources.However,the currently used liquid carbonate compounds in commercial lithium-ion battery electrolytes pose potential safety hazards such as leakage,swelling,corrosion,and flammability.Solid electrolytes can be used to mitigate these risks and create a safer lithium battery.Furthermore,high-energy density can be achieved by using solid electrolytes along with high-voltage cathode and metal lithium anode.Two types of solid electrolytes are generally used:inorganic solid electrolytes and polymer solid electrolytes.Inorganic solid electrolytes have high ionic conductivity,electrochemical stability window,and mechanical strength,but suffer from large solid/solid contact resistance between the electrode and electrolyte.Polymer solid electrolytes have good flexibility,processability,and contact interface properties,but low room temperature ionic conductivity,necessitating operation at elevated temperatures.Composite solid electrolytes(CSEs) are a promising alternative because they offer light weight and flexibility,like polymers,as well as the strength and stability of inorganic electrolytes.This paper presents a comprehensive review of recent advances in CSEs to help researchers optimize CSE composition and interactions for practical applications.It covers the development history of solid-state electrolytes,CSE properties with respect to nanofillers,morphology,and polymer types,and also discusses the lithium-ion transport mechanism of the composite electrolyte,and the methods of engineering interfaces with the positive and negative electrodes.Overall,the paper aims to provide an outlook on the potential applications of CSEs in solid-state lithium batteries,and to inspire further research aimed at the development of more systematic optimization strategies for CSEs.
基金supported by the National Key R&D Program of China(2022YFB3807700)the National Natural Science Foundation of China(U1964205,51872303,52172253)+3 种基金the Ningbo S&T Innovation 2025 Major Special Programme(2019B10044,2021Z122)the Zhejiang Provincial Key R&D Program of China(2022C01072)the Jiangsu Provincial S&T Innovation Special Programme for carbon peak and carbon neutrality(BE2022007)the Youth Innovation Promotion Association CAS(Y2021080)。
文摘Sulfide solid electrolytes are promising for high energy density and safety in all-solid-state batteries due to their high ionic conductivity and good mechanical properties.However,the application of sulfide solid electrolytes in all-solid-state batteries with lithium anode is restricted by the side reactions at lithium/electrolytes interfaces and the growth of lithium dendrite caused by nonuniform lithium deposition.Herein,a homogeneous LiF-Li_(3)N composite protective layer is in situ formed via a manipulated reaction of pentafluorobenzamide with Li metal.The LiF-Li_(3)N layer with both high interfacial energy and interfacial adhesion energy can synergistically suppress side reactions and inhibit the growth of lithium dendrite,achieving uniform deposition of lithium.The critical current densities of Li_(10)GeP_(2)S_(12)and Li_(6)PS_(5)Cl are increased to 3.25 and 1.25 mA cm^(-2)with Li@LiF-Li_(3)N layer,which are almost triple and twice as those of Li-symmetric cells in the absence of protection layer,respectively.Moreover,the Li@LiF-Li_(3)N/Li10GeP2S12/Li@LiF-Li_(3)N cell can stably cycle for 9000 h at 0.1 mA cm^(-2)under 0.1 mA h cm^(-2),and Li@LiF-Li_(3)N/Li_(6)PS_(5)Cl/Li@LiF-Li_(3)N cell achieves stable Li plating/stripping for 8000 h at 0.1 mA cm^(-2)under10 m A h cm^(-2).The improved dynamic stability of lithium plating/stripping in Li@LiF-Li_(3)N/Li_(10)GeP_(2)S_(12)or Li_(6)PS_(5)Cl interfaces is proved by three-electrode cells.As a result,LiCoO_(2)/electrolytes/Li@LiF-Li_(3)N batteries with Li_(10)GeP_(2)S_(12)and Li_(6)PS_(5)Cl exhibit remarkable cycling stability of 500 cycles with capacity retentions of 93.5%and 89.2%at 1 C,respectively.
基金supported by the Beijing Natural Science Foundation(L223009)the National Natural Science Foundation of China(22075029)+1 种基金the National Key Research and Development Program of China(2021YFB2500300)the Key Research and Development(R&D)Projects of Shanxi Province(2021020660301013)。
文摘All-solid-state lithium metal batteries(ASSLMBs)are considered as one of the ultimate goals for the development of energy storage systems due to their high energy density and high safety.However,the mismatching of interface transport kinetics as well as interfacial instability induces the growth of lithium dendrite and thus,leads to severe degradation of battery electrochemical performances.Herein,an integrated interface configuration(IIC)consisting of in-situ generated Li I interphase and Li-Ag alloy anode is proposed through in-situ interface chemistry.The IIC is capable of not only regulating charge transport kinetics but also synchronously stabilizing the lithium/electrolyte interface,thereby achieving uniform lithium platting.Therefore,Li||Li symmetric cells with IIC achieve a critical current density of up to 1.6 mA cm^(-2)and achieve stable cycling over 1600 hours at a high current density of 0.5 mA cm^(-2).Moreover,a high discharge capacity of 140.1 mA h g-1at 0.1 C is also obtained for the Li(Ni_(0.6)Co_(0.2)Mn_(0.2))O_(2)(NCM622)full battery with a capacity retention of 65.6%after 300 cycles.This work provides an effective method to synergistically regulate the interface transport kinetics and inhibit lithium dendrite growth for high-performance ASSLMBs.
基金supported by R&D Program of Power Batteries with Low Temperature and High Energy,Science and Technology Bureau of Changchun(19SS013)Key Subject Construction of Physical Chemistry of Northeast Normal University+1 种基金the Fundamental Research Funds for the Central Universities(2412020FZ007,2412020FZ008)National Natural Science Foundation of China(22102020).
文摘Succinonitrile-based plastic crystal electrolytes have emerged for high-energy-density Li metal batteries in terms of their superior ambient ionic conductivity,low flammability,and benign compatibility with high voltage cathode,but are hampered by inherent instabilities toward Li anodes.Constructing hierarchical solid electrolytes structure is a fundamental approach to protect Li anode from succinonitrile attacks,with succinonitrile-based oxidation-resistance layer facing high voltage cathode and reduction-tolerant layer contacting Li anode.However,free succinonitrile molecules in succinonitrile-based electrolyte layer can diffuse across the electrolyte/electrolyte interface and further reach Li anode surface during the battery cycle.This chemical“crosstalk”cause reduction-tolerant electrolyte layer to fail to protect the Li anode from the attacks of free succinonitrile molecules.Nano Li_(6.4)La_(3)Zr_(1.4)Ta_(0.6)O_(12)is introduced creatively into succinonitrile-based electrolyte layer.By taking advantage of the complexation between La atoms in Li_(6.4)La_(3)Zr_(1.4)Ta_(0.6)O_(12)and N atoms in succinonitrile,the free succinonitrile molecules are successfully immobilized in succinonitrile-based electrolyte layer.The resulting low resistance and highly durable solid electrolyte interphase and cathode electrolyte interphase endow NCM622||Li batteries with remarkable cycle stability.Our research provides a new idea for the real application of plastic crystal electrolytes in high voltage solid-state lithium metal batteries.
基金supported by the National Natural Science Foundation of China (51773134)the Sichuan Science and Technology Program (2019YFH0112)+2 种基金the Fundamental Research Funds for the Central UniversitiesInstitutional Research Fund from Sichuan University (2021SCUNL201)the 111 Project (B20001)。
文摘The rapid development and widespread application of lithium-ion batteries(LIBs) have increased demand for high-safety and high-performance LIBs. Accordingly, various additives have been used in commercial liquid electrolytes to severally adjust the solvation structure of lithium ions, control the components of solid electrolyte interphase, or reduce flammability. While it is highly desirable to develop low-cost multifunctional electrolyte additives integrally that address both safety and performance on LIBs, significant challenges remain. Herein, a novel phosphorus-containing organic small molecule, bis(2-methoxyethyl) methylphosphonate(BMOP), was rationally designed to serve as a fluorine-free and multifunctional additive in commercial electrolytes. This novel electrolyte additive is low-toxicity,high-efficiency, low-cost, and electrode-compatible, which shows the significant improvement to both electrochemical performance and fire safety for LIBs through regulating the electrolyte solvation structure, constructing the stable electrode-electrolyte interphase, and suppressing the electrolyte combustion. This work provides a new avenue for developing safer and high-performance LIBs.
基金supported by the Jilin Province Science and Technology Department Program(YDZJ202201ZYTS304)the Science and Technology Project of Jilin Provincial Education Department(JJKH20220428KJ)+3 种基金the Jilin Province Science and Technology Department Program(YDZJ202101ZYTS047)the National Natural Science Foundation of China(21905110,21905041,22279045,22102020)the Special foundation of Jilin Province Industrial Technology Research and Development(2019C042)the Fundamental Research Funds for the Central Universities(2412020FZ008)。
文摘Lithium sulfur batteries are regarded as a promising candidate for high-energy-density energy storage devices.However,the lithium metal anode in lithium-sulfur batteries encounters the problem of lithium dendrites and lithium metal consumption caused by polysulfide corrosion.Herein we design a dualfunction PMMA/PPC/LiNO3composite as an artificial solid electrolyte interphase(PMCN-SEI)to protect Li metal anode.This SEI offers multiple sites of C=O for polysulfide anchoring to constrain corrosion of Li metal anode.The lithiated polymer group and Li3N in PMCN-SEI can homogenize lithium-ion deposition behavior to achieve a dendrite-free anode.As a result,the PMCN-SEI protected Li metal anode enables the Li||Li symmetric batteries to maintain over 300 cycles(1300 h)at a capacity of 5 m Ah cm^(-2),corresponding to a cumulative capacity of 3.25 Ah cm^(-2).Moreover,Li-S batteries assembled with 20μm of Li metal anode(N/P=1.67)still deliver an initial capacity of 1166 m A h g-1at 0.5C.Hence,introducing polycarbonate polymer/inorganic composite SEI on Li provides a new solution for achieving the high energy density of Li-S batteries.
基金The support provided by the German Federal Ministry of Education and Research(BMBF)within the project“Benchbatt”(03XP0047B)is gratefully acknowledged.
文摘The solvent-free in situ polymerization technique has the potential to tailor-make conformal interfaces that are essential for developing durable and safe lithium metal polymer batteries(LMPBs).Hence,much attention has been given to the eco-friendly and rapid ultraviolet(UV)-induced in situ photopolymerization process to prepare solid-state polymer electrolytes.In this respect,an innovative method is proposed here to overcome the challenges of UV-induced photopolymerization(UV-curing)in the zones where UV-light cannot penetrate,especially in LMPBs where thick electrodes are used.The proposed frontal-inspired photopolymerization(FIPP)process is a diverged frontal-based technique that uses two classes(dual)of initiators to improve the slow reaction kinetics of allyl-based monomers/oligomers by at least 50%compared with the conventional UV-curing process.The possible reaction mechanism occurring in FIPP is demonstrated using density functional theory calculations and spectroscopic investigations.Indeed,the initiation mechanism identified for the FIPP relies on a photochemical pathway rather than an exothermic propagating front forms during the UV-irradiation step as the case with the classical frontal photopolymerization technique.Besides,the FIPP-based in situ cell fabrication using dual initiators is advantageous over both the sandwich cell assembly and conventional in situ photopolymerization in overcoming the limitations of mass transport and active material utilization in high energy and high power LMPBs that use thick electrodes.Furthermore,the LMPB cells fabricated using the in situ-FIPP process with high mass loading LiFePO_(4)electrodes(5.2 mg cm^(-2))demonstrate higher rate capability,and a 50%increase in specific capacity against a sandwich cell encouraging the use of this innovative process in large-scale solid-state battery production.
基金This research was supported by the Fundamental Research Funds for the Central Universities(0515022GH0202253 and 0515022SH0201253).
文摘Due to its high theoretical capacity(820 mAh g^(−1)),low standard electrode potential(−0.76 V vs.SHE),excellent stability in aqueous solutions,low cost,environmental friendliness and intrinsically high safety,zinc(Zn)-based batteries have attracted much attention in developing new energy storage devices.In Zn battery system,the battery performance is significantly affected by the solid electrolyte interface(SEI),which is controlled by electrode and electrolyte,and attracts dendrite growth,electrochemical stability window range,metallic Zn anode corrosion and passivation,and electrolyte mutations.Therefore,the design of SEI is decisive for the overall performance of Zn battery systems.This paper summarizes the formation mechanism,the types and characteristics,and the characterization techniques associated with SEI.Meanwhile,we analyze the influence of SEI on battery performance,and put forward the design strategies of SEI.Finally,the future research of SEI in Zn battery system is prospected to seize the nature of SEI,improve the battery performance and promote the large-scale application.
基金financially supported by the Fundamental Research Funds for the Central Universities of China(No.FRF-BD-19-008A)the Brain Pool program funded by the Ministry of Science and ICT through the National Research Foundation of Korea(No.2019H1D3A2A02100593)the National Research Foundation of Korea(NRF)grant funded by the Korean government(Nos.2019R1C1C 1006310,2020R1I1A1A01072996,2021K2A9A2A06044652,and 2019R1A2C1002844).
文摘In the past few years,the all-solid lithium battery has attracted worldwide attentions,the ionic conductivity of some all-solid lithium-ion batteries has reached 10^(-3)-10^(-2) S/cm,indicating that the transport of lithium ions in solid electrolytes is no longer a major problem.However,some interface issues become research hotspots.Examples of these interfacial issues include the electrochemical decomposition reaction at the electrode-electrolyte interface;the low effective contact area between the solid electrolyte and the electrode etc.In order to solve the issues,researchers have pursued many different approaches.The addition of a buffer layer between the electrode and the solid electrolyte has been at the center of this endeavor.In this review paper,we provide a systematic summarization of the problems on the electrode-solid electrolyte interface and detailed reflection on the latest works of buffer-based therapies,and the review will end with a personal perspective on the improvement of buffer-based therapies.
基金supported by the National Natural Science Foundation of China(51872027)the Fundamental Research Funds for the Central Universities(FRF-TP-20-014A2)。
文摘All-solid-state lithium batteries(ASSLBs) employing sulfide electrolyte and lithium(Li) anode have received increasing attention due to the intrinsic safety and high energy density.However,the thick electrolyte layer and lithium dendrites formed at the electrolyte/Li anode interface hinder the realization of high-performance ASSLBs.Herein,a novel membrane consisting of Li_(6)PS_(5) Cl(LPSCl),poly(ethylene oxide)(PEO) and Li-salt(LiTFSI) was prepared as sulfide-based composite solid electrolyte(LPSCl-PEO3-LiTFSI)(LPSCl:PEO=97:3 wt/wt;EO:Li=8:1 mol/mol),which delivers high ionic conductivity(1.1 × 10^(-3) S cm^(-1)) and wide electrochemical window(4.9 V vs.Li^(+)/Li) at 25 ℃.In addition,an ex-situ artificial solid electrolyte interphase(SEI) film enriched with LiF and Li3 N was designed as a protective layer on Li anode(Li(SEI)) to suppress the growth of lithium dendrites.Benefiting from the synergy of sulfide-based composite solid electrolyte and ex-situ artificial SEI,cells of S-CNTs/LPSCI-PEO3-LiTFSI/Li(SEI) and Al_(2)O_(3)@LiNi_(0.5)Co_(0.3)Mn_(0.2)O_(2)/LPSCl-PEO3-LiTFSI/Li(SEI) are assembled and both exhibit high initial discharge capacity of 1221.1 mAh g^(-1)(135.8 mAh g^(-1)) and enhanced cycling stability with 81.6% capacity retention over 200 cycles at 0.05 C(89.2% over 100 cycles at 0.1 C).This work provides a new insight into the synergy of composite solid electrolyte and artificial SEI for achieving high-performance ASSLBs.
基金supported by the Fundamental Research Funds for Central Universities(SCUT Grant No.2019ZD22)the Guangdong Innovative and Entrepreneurial Research Team Program(No.2016ZT06N569)。
文摘Transition metal selenides have been widely studied as anode materials of sodium ion batteries(SIBs),however,the investigation of solid-electrolyte-interface(SEI)on these materials,which is critical to the electrochemical performance of SIBs,remains at its infancy.Here in this paper,ZnSe@C nanoparticles were prepared from ZIF-8 and the SEI layers on these electrodes with and without reduced graphene oxide(rGO)layers were examined in details by X-ray photoelectron spectroscopies at varied charged/discharged states.It is observed that fast and complicated electrolyte decomposition reactions on ZnSe@C leads to quite thick SEI film and intercalation of solvated sodium ions through such thick SEI film results in slow ion diffusion kinetics and unstable electrode structure.However,the presence of rGO could efficiently suppress the decomposition of electrolyte,thus thin and stable SEI film was formed.ZnSe@C electrodes wrapped by rGO demonstrates enhanced interfacial charge transfer kinetics and high electrochemical performance,a capacity retention of 96.4%,after 1000 cycles at 5 A/g.This study might offer a simple avenue for the designing high performance anode materials through manipulation of SEI film.
基金Subsidy for Hebei Key Laboratory of Applied Chemistry after Operation Performance,Grant/Award Number:22567616HNatural Science Foundation of Hebei Province of China,Grant/Award Number:B2020103028+3 种基金Science Fund for Creative Research Groups of the National Natural Science Foundation of China,Grant/Award Number:21921005National Key Research and Development Program of China,Grant/Award Number:2021YFB2400300Beijing Municipal Natural Science Foundation Project,Grant/Award Number:2222031National Natural Science Foundation of China,Grant/Award Numbers:52174281,21808228。
文摘The specific energy of Li metal batteries(LMBs)can be improved by using high‐voltage cathode materials;however,achieving long‐term stable cycling performance in the corresponding system is particularly challenging for the liquid electrolyte.Herein,a novel pseudo‐oversaturated electrolyte(POSE)is prepared by introducing 1,1,2,2‐tetrafluoroethyl‐2,2,3,3‐tetrafluoropropyl ether(TTE)to adjust the coordination structure between diglyme(G2)and lithium bis(trifluoromethanesulfonyl)imide(LiTFSI).Surprisingly,although TTE shows little solubility to LiTFSI,the molar ratio between LiTFSI and G2 in the POSE can be increased to 1:1,which is much higher than that of the saturation state,1:2.8.Simulation and experimental results prove that TTE promotes closer contact of the G2 molecular with Li^(+)in the POSE.Moreover,it also participates in the formation of electrolyte/electrode interphases.The electrolyte shows outstanding compatibility with both the Li metal anode and typical high‐voltage cathodes.Li||Li symmetric cells show a long life of more than 2000 h at 1 mA cm^(−2),1 mAh cm^(−2).In the meantime,Li||LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2)(NCM811)cell with the POSE shows a high reversible capacity of 134.8 mAh g^(−1 )after 900 cycles at 4.5 V,1 C rate.The concept of POSE can provide new insight into the Li^(+)solvation structure and in the design of advanced electrolytes for LMBs.
基金This work is supported by the Technologies R&D Program of Huzhou City(No.2022JB01)the Key Research and Development Program of Zhejiang Province(No.2023C01127)the Highstar Corporation HSD20210118.
文摘The widespread adoption of lithium-ion batteries has been driven by the proliferation of portable electronic devices and electric vehicles,which have increasingly stringent energy density requirements.Lithium metal batteries(LMBs),with their ultralow reduction potential and high theoretical capacity,are widely regarded as the most promising technical pathway for achieving high energy density batteries.In this review,we provide a comprehensive overview of fundamental issues related to high reactivity and migrated interfaces in LMBs.Furthermore,we propose improved strategies involving interface engineering,3D current collector design,electrolyte optimization,separator modification,application of alloyed anodes,and external field regulation to address these challenges.The utilization of solid-state electrolytes can significantly enhance the safety of LMBs and represents the only viable approach for advancing them.This review also encompasses the variation in fundamental issues and design strategies for the transition from liquid to solid electrolytes.Particularly noteworthy is that the introduction of SSEs will exacerbate differences in electrochemical and mechanical properties at the interface,leading to increased interface inhomogeneity—a critical factor contributing to failure in all-solidstate lithium metal batteries.Based on recent research works,this perspective highlights the current status of research on developing high-performance LMBs.
基金support by the National Natural Science Foundation of China(grant no.51772206).
文摘Solid polymer electrolytes(SPEs)are highly promising for realizing high-capacity,low-cost,and safe Li metal batteries.However,the Li dendritic growth and side reactions between Li and SPEs also plague these systems.Herein,a fluorinated lithium salt coating(FC)with organic-inorganic gradient and soft–rigid feature is introduced on Li surface as an artificial protective layer by the in-situ reaction between Li metal and fluorinated carboxylic acid.The FC layer can improve the interface stability and wettability between Li and SPEs,assist the transport of Li ions,and guide Li nucleation,contributing to a dendrite-free Li deposition and long-lifespan Li metal batteries.The symmetric cell with FC-Li anodes exhibits a high areal capacity of 1 mAh cm^(-2)at 0.5 mA cm^(-2),and an ultra-long lifespan of 2000 h at a current density of 0.1 mA cm^(-2).Moreover,the full cell paired with the LiFePO4 cathode exhibits improved cycling stability,remaining 83.7%capacity after 500 cycles at 1 C.When matching with the S cathode,the FC layer can prevent the shuttle effect,contributing to stable and high-capacity Li–S battery.This work provided a promising way for the construction of stable all-solid-state lithium metal batteries with prolonged lifespan.
基金supported by the National Natural Science Foundation of China(51872196)the Natural Science Foundation of Tianjin,China(17JCJQJC44100)。
文摘Owing to its low potential, crustal abundances and environmental friendliness, calcium metal anode(CMA) is emerging as a powerful contender in post-lithium era. However, the passivation of CMA fatally hinders its development. Recently, several feasible electrolytes have been developed. Nevertheless, as a pivotal part, the solid electrolyte interface(SEI) formed on CMA has not been paid enough attention to. In this review, based on the passivation mechanism of CMA, the favorable composition of SEI is emphasized with the corresponding electrolytes. It is considered that boron-containing and organic–inorganic hybrid SEI might be preferred. By comparing electrolytes and SEI on CMA with lithium and magnesium metal anodes, the root causes of CMA passivation are further elaborated, enlightening rational design rules of suitable SEI. Furthermore, some noteworthy details when assembling secondary calcium metal batteries(CMBs) are put forward. It is expected that deeper understanding of SEI on CMA will promote the development of CMBs.
基金supported by the National High Technology Research and Development Program of China(Grant No.2013AA050906)the National Natural Science Foundation of China(Grant Nos.51172250 and 51202265)+1 种基金the Strategic Priority Research Program of the Chinese Academy of Sciences(Grant No.XDA09010201)Zhejiang Province Key Science and Technology Innovation Team,China(Grant No.2013PT16)
文摘The scientific basis of all-solid-state lithium batteries with inorganic solid electrolytes is reviewed briefly, touching upon solid electrolytes, electrode materials, electrolyte/electrode interface phenomena, fabrication, and evaluation. The challenges and prospects are outlined as well.
基金supported by National Key Research and Development Program(2016YFA0202500)the National Natural Science Foundation of China(21776019)Beijing Natural Science Foundation(L182021)。
文摘Lithium-ion battery has greatly changed our lifestyle and the solid electrolyte interphase(SEI)covered on the graphite anode determines the service life of a battery.The formation method and the formation temperature at initial cycle of a battery determine the feature of the SEI.Herein,we investigate the gap of formation behavior in both a half cell(graphite matches with lithium anode)and a full cell(graphite matches with NCM,short for LiNixCoyMn1-x-yO2)at different temperatures.We conclude that high temperature causes severe side reactions and low temperature will result in low ionic conductive SEI layer,the interface formed at room temperature owns the best ionic conductivity and stability.