Degradability of absorbable sutures in tendon grafts following anterior cruciate ligament reconstruction
1
作者 张力 《外科研究与新技术》 2011年第2期121-121,共1页
Objective To observe the degradability of absorbable sutures in tendon grafts and the histology of tendon healing in a rabbit model.Methods Semitendinosus tendons were harvested from 15 healthy adult New Zealand rabbi... Objective To observe the degradability of absorbable sutures in tendon grafts and the histology of tendon healing in a rabbit model.Methods Semitendinosus tendons were harvested from 15 healthy adult New Zealand rabbits in this study. 展开更多
关键词 Degradability of absorbable sutures in tendon grafts following anterior cruciate ligament reconstruction
下载PDF
Novel hybrid biocomposites for tendon grafts:The addition of silk to polydioxanone and poly(lactide-co-caprolactone)enhances material properties,in vitro and in vivo biocompatibility
2
作者 Behzad Shiroud Heidari Emma Muiños Lopez +10 位作者 Emma Harrington Rui Ruan Peilin Chen Seyed Mohammad Davachi Benjamin Allardyce Rangam Rajkhowa Rodney Dilley Froilán Granero-Moltó Elena M.De-Juan-Pardo Minghao Zheng Barry Doyle 《Bioactive Materials》 SCIE CSCD 2023年第7期291-306,共16页
Biopolymers play a critical role as scaffolds used in tendon and ligament(TL)regeneration.Although advanced biopolymer materials have been proposed with optimised mechanical properties,biocompatibility,degradation,and... Biopolymers play a critical role as scaffolds used in tendon and ligament(TL)regeneration.Although advanced biopolymer materials have been proposed with optimised mechanical properties,biocompatibility,degradation,and processability,it is still challenging to find the right balance between these properties.Here,we aim to develop novel hybrid biocomposites based on poly(p-dioxanone)(PDO),poly(lactide-co-caprolactone)(LCL)and silk to produce high-performance grafts suitable for TL tissue repair.Biocomposites containing 1-15%of silk were studied through a range of characterisation techniques.We then explored biocompatibility through in vitro and in vivo studies using a mouse model.We found that adding up to 5%silk increases the tensile properties,degradation rate and miscibility between PDO and LCL phases without agglomeration of silk inside the composites.Furthermore,addition of silk increases surface roughness and hydrophilicity.In vitro experiments show that the silk improved attachment of tendon-derived stem cells and proliferation over 72 h,while in vivo studies indicate that the silk can reduce the expression of pro-inflammatory cytokines after six weeks of implantation.Finally,we selected a promising biocomposite and created a prototype TL graft based on extruded fibres.We found that the tensile properties of both individual fibres and braided grafts could be suitable for anterior cruciate ligament(ACL)repair applications. 展开更多
关键词 BIOCOMPOSITE tendon graft SILK Fibre extrusion Biodegradable scaffolds Anterior cruciate ligament