Heat moving source models along with transient heat analysis by finite element method were used to determine weld thermal cycles and isothermal sections obtained from the application of a gas tungsten arc welding bead...Heat moving source models along with transient heat analysis by finite element method were used to determine weld thermal cycles and isothermal sections obtained from the application of a gas tungsten arc welding beads on Inconel 718 plates. Analytical (Rosenthal’s thick plate model) and finite element results show an acceptable approximation with the experimental weld thermal cycles. The isothermal sections determined by numerical simulation show a better approximation with the experimental welding profile for double-ellipse model heat distribution than Gauss model. To analyze the microstructural transformation produced by different cooling rates in the fusion and heat affected zones, Vickers microhardness measurements (profile and mapping representation) were conducted. A hardness decrement for the heat affected zone (~200 HV0.2) and fusion zone (~240 HV0.2) in comparison with base material (~350 HV0.2) was observed. This behavior has been attributed to the heterogeneous solubilization process of the γ″ phase (nickel matrix), which, according to the continuous-cooling-transformation curve, produced the Laves phase,δ and MC transition phases, generating a loss in hardness close to the fusion zone.展开更多
The selection of process parameter in the gas tungsten arc (GTA) welding of titanium alloy was presented for obtaining optimum grain size and hardness. Titanium alloy (Ti-6Al-4V) is one of the most important non-f...The selection of process parameter in the gas tungsten arc (GTA) welding of titanium alloy was presented for obtaining optimum grain size and hardness. Titanium alloy (Ti-6Al-4V) is one of the most important non-ferrous metals which offers great potential application in aerospace, biomedical and chemical industries, because of its low density (4.5 g/cm^3), excellent corrosion resistance, high strength, attractive fracture behaviour and high melting point (1678℃). The preferred welding process for titanium alloy is frequent GTA welding due to its comparatively easier applicability and better economy. In the case of single pass (GTA) welding of thinner section of this alloy, the pulsed current has been found beneficial due to its advantages over the conventional continuous current process. Many considerations come into the picture and one needs to carefully balance various pulse current parameters to reach an optimum combination. Four factors, five level, central composite, rotatable design matrix were used to optimize the required number of experimental conditions. Mathematical models were developed to predict the fusion zone grain size using analysis of variance (ANOVA) and regression analysis. The developed models were optimized using the traditional Hooke and Jeeve's algorithm. Experimental results were provided to illustrate the proposed approach.展开更多
An empirical relationship to predict tensile strength of pulsed current gas tungsten arc welded AZ31B magnesium alloy was developed. Incorporating process parameters such as peak current, base current, pulse frequency...An empirical relationship to predict tensile strength of pulsed current gas tungsten arc welded AZ31B magnesium alloy was developed. Incorporating process parameters such as peak current, base current, pulse frequency and pulse on time were studied. The experiments were conducted based on a four-factor, five-level, central composite design matrix. The developed empirical relationship can be effectively used to predict the tensile strength of pulsed current gas tungsten arc welded AZ31B magnesium alloy joints at 95% confidence level. The results indicate that pulse frequency has the greatest influence on tensile strength, followed by peak current, pulse on time and base current.展开更多
The dissimilar joining of CP-copper to 304 stainless steel was performed by gas tungsten arc welding process using different filler materials. The results indicated the formation of defect free joint by using copper f...The dissimilar joining of CP-copper to 304 stainless steel was performed by gas tungsten arc welding process using different filler materials. The results indicated the formation of defect free joint by using copper filler material. But, the presence of some defects like solidification crack and lack of fusion caused decreasing tensile strength of other joints. In the optimum conditions, the tensile strength of the joint was 96% of the weaker material. Also, this joint was bent till to 180° without any macroscopic defects like separation, tearing or fracture. It was concluded that copper is a new and good candidate for gas tungsten arc welding of copper to 304 stainless steel.展开更多
TiC/TisSi3 composites were fabricated on Ti-5A1-2.5Sn substrates by gas tungsten arc welding (GTAW). Identification of the phases was performed using X-ray diffraction (XRD). The microstructures were analyzed usin...TiC/TisSi3 composites were fabricated on Ti-5A1-2.5Sn substrates by gas tungsten arc welding (GTAW). Identification of the phases was performed using X-ray diffraction (XRD). The microstructures were analyzed using scanning electron microscopy (SEM) combined with energy-dispersive X-ray spectrometry (EDS) and optical microscopy (OM). The Vickers hardness was measured with a micro-hardness tester. The TiC/TisSi3 composites were obtained in a double-layer track, and the Vickers hardness of the track increased by two to three times compared with the Ti-5A1-2.5Sn substrate.展开更多
This present study applied gas tungsten arc welding in order to join AISI 304 and AISI 201 stainless steels.The objective was to find the optimum welding condition that gave a weld bead in accordance with DIN EN ISO 2...This present study applied gas tungsten arc welding in order to join AISI 304 and AISI 201 stainless steels.The objective was to find the optimum welding condition that gave a weld bead in accordance with DIN EN ISO 25817 quality level B, pitting corrosion potential of the weld metal of not less than that of the AISI304 base metal and a ratio of delta-ferrite in austenite matrix of the weld metal of not lower than 3%.Such a ratio is a criterion widely accepted to protect the weld metal from solidification cracking. At the welding current of 75 A and by using pure argon as a shielding gas 0 to 8 vol.% and applying a welding speed in the range of 2-3.5 mm·s^(-1) was found to give a complete weld bead with an increased depthper-width ratio(promote weldability). For welding speed in the range of 3 and 3.5 mm·s^(-1)(promote corrosion resistance). Increasing the welding speed in such a range decreased the amount of delta-ferrite in the austenite matrix, and increased the pitting corrosion potential of the weld metal to be 302 mV_(SCE).This value was still lower than the pitting corrosion potential of the AISI 304 base metal. Mixing nitrogen in argon shielding gas increased the nitrogen content in the weld. The optimum condition was found when using a welding speed of 3 mm· s^(-1) and mixing 1 vol.% of nitrogen in the argon shielding gas(promote weldability and corrosion resistance). Pitted areas after potentiodynamic test were observed in the austenite in which its Cr content was relatively low.展开更多
Abstract Horizontal welding is important for heavy or huge welding structures. Keyhole mode variable polarity plasma arc welding of aluminum alloy plates with medium thickness was carried out in horizontal position. T...Abstract Horizontal welding is important for heavy or huge welding structures. Keyhole mode variable polarity plasma arc welding of aluminum alloy plates with medium thickness was carried out in horizontal position. The characteristic of welding defects was introduced. Preliminary experiments indicated that the undercut defect could not be eliminated easily. The relationship between welding parameters and the undercut defect showed that this deject could be lessened by using higher heat input. The fluid flow of weld pool was observed by a high speed camera. The fluid flow in weld pool was not symmetric and much of molten metal gathered in the lower part. The fluid flow velocity in the lower part was bigger than that in the upper part. To this end, the formative mechanism of the undercut defect was proposed. The flowability of the molten metal was an influential factor for the undercut defect. A preheating method was designed to verify the formative mechanism.展开更多
Realizing of weld penetration control in gas tungsten arc welding requires establishment of a model describing the relationship between the front-side geometrical parameters of weld pool and the back-side weld width w...Realizing of weld penetration control in gas tungsten arc welding requires establishment of a model describing the relationship between the front-side geometrical parameters of weld pool and the back-side weld width with sufficient accuracy. A neural network model is developed to attain this aim. Welding experiments are conducted to obtain the training data set (including 973 groups of geometrical parameters of the weld pool and back-side weld width) and the verifying data set (108 groups). Two data sets are used for training and verifying the neural network, respectively. The testing results show that the model has sufficient accuracy and can meet the requirements of weld penetration control.展开更多
The mechanical properties of the 2219 aluminum alloy welded joints by vertical-up variant polarity plasma arc welding (VPPAW) with keyhole were analyzed. The tensile strength of welded joints can reach 55% of that of ...The mechanical properties of the 2219 aluminum alloy welded joints by vertical-up variant polarity plasma arc welding (VPPAW) with keyhole were analyzed. The tensile strength of welded joints can reach 55% of that of base metal. The microstructure of weld joints was studied to explain the mechanical properties of the weld. The results show that the intensity of weld center is less than that of HAZ, and the intensity of weld center is the worst. So an advanced welding procedures is presented to reduce the heat input and increase the welding speed. The results in this procedures show that the tensile strength of welded joints reaches more than 60% of that of the parent metal, and the specific elongation does not descend.展开更多
Presents penetration control by weld pool resonance which occurs when the natural frequency of weld pool is equal to the frequency of sine wave current while the weld pool is excited into oscillation by superimposing ...Presents penetration control by weld pool resonance which occurs when the natural frequency of weld pool is equal to the frequency of sine wave current while the weld pool is excited into oscillation by superimposing sine wave current with definite frequency or regular frequency on DC current, and experiments carried out on detecting resonance signals during both stationary and travelling arc welding with variant frequency pulse current, and concludes with experimental results that penetration control can be realized by weld pool resonance when welding speed is lower than 80mm/min, and this control method is applicable to welding thin (0.5~3.0 mm) plates of carbon steel, low alloy steel, high strength steel and superhigh strength steel, and suitable for alternating polarity welding of stainless steel, titanium alloy steel and aluminum alloy.展开更多
Variable polarity plasma arc welding (VPPAW) is one of the most excellent processes used for welding aluminum alloys recently. It combines the advantages of variable polarity welding and plasma arc welding, and can ac...Variable polarity plasma arc welding (VPPAW) is one of the most excellent processes used for welding aluminum alloys recently. It combines the advantages of variable polarity welding and plasma arc welding, and can achieve the most rational heat distribution and cathodic cleaning. With the VPPAW equipment developed by authors, the cathodic cleaning regularity that is one of the most important problems in VPPAW is investigated in this paper. The results will be helpful in realizing the real cleaning mechanism.展开更多
Arc pressure is the key influencing factor to forming of molten pool. Countering the characteristic of tungsten inert gas arc welding with micro gap for tantalum sheet, according to the fundament of arc physics, a dis...Arc pressure is the key influencing factor to forming of molten pool. Countering the characteristic of tungsten inert gas arc welding with micro gap for tantalum sheet, according to the fundament of arc physics, a distribution model of arc pressure and forming mechanism of molten pool with micro butt gap are proposed, and the influences of arc pressure on forming of molten pool are discussed. Experimental researches for the dynamic formation process of weld molten pool by using high-speed vidicon camera show that when butt gap is appropriate, that is from 0. 1 to 0. 15 mm, molten metals formed on two workpiece uplift and grow up first, then are fused and form uniform molten pool finally.展开更多
Temperature distribution and weld bead profiles of constant current and pulsed current gas tungsten arc welded aluminium alloy joints were compared. The effects of pulsed current welding on tensile properties, hardnes...Temperature distribution and weld bead profiles of constant current and pulsed current gas tungsten arc welded aluminium alloy joints were compared. The effects of pulsed current welding on tensile properties, hardness profiles, microstructural features and residual stress distribution of aluminium alloy joints were reported. The use of pulsed current technique is found to improve the tensile properties of the weld compared with continuous current welding due to grain refinement occurring in the fusion zone.展开更多
Double-V butt TIG welding process was performed on two plates of AA6061-T6 using ER5356 filler. The microstructure,mechanical and nanomechanical properties of the joint were evaluated in as-welded and after post weld ...Double-V butt TIG welding process was performed on two plates of AA6061-T6 using ER5356 filler. The microstructure,mechanical and nanomechanical properties of the joint were evaluated in as-welded and after post weld heat treatment (PWHT) usingXRD, FESEM, EBSD, nanoindentation and tensile tests. The results show that PWHT led to microstructural recovery of the heataffected zone (HAZ) in addition to the appearance of β-phase (Al3Mg2) at the grain boundaries of weld zone. The hardness (Hnano) inall zones increased after PWHT while the elastic modulus (Enano) was improved from 69.93 GPa to 81 GPa in weld area. All resultsindicate that PWHT has created a homogenous microstructure in the weld zone in addition to outstanding improvement inmechanical properties for the weld zone which surpass the base metal.展开更多
Keyhole gas tungsten arc welding(K-TIG)of Q345 low alloy steel plates was simulated by using SYSWELD software.The temperature field of the K-TIG welding process was simulated with three different combined heat sources...Keyhole gas tungsten arc welding(K-TIG)of Q345 low alloy steel plates was simulated by using SYSWELD software.The temperature field of the K-TIG welding process was simulated with three different combined heat sources and was compared with the weld profile that was obtained experimentally.The temperature field that was obtained by a combination of a double ellipsoid heat source on the upper half and a three-dimensional Gauss heat source on the lower half was similar to the real situation.The effects of plate thickness,gap and welding speed on the deformation and stress of the K-TIG welded joints were investigated by K-TIG welding numerical simulation.A reduction in the thickness of the weld plates reduced the z-direction deformation and transverse residual stress;an appropriate gap reduced the residual stress and an increase in the welding speed reduced deformation after welding,but did not help to control the residual stress after welding.展开更多
The effects of Sn addition on the microstructure and mechanical properties of gas tungsten arc butt-welded Mg?6Al?0.3Mn (AM60) (mass fraction, %) alloy sheets were investigated by optical microscopy, scanning electron...The effects of Sn addition on the microstructure and mechanical properties of gas tungsten arc butt-welded Mg?6Al?0.3Mn (AM60) (mass fraction, %) alloy sheets were investigated by optical microscopy, scanning electron microscopy, X-ray diffraction, transmission electron microscopy, and microhardness and tensile tests. The results indicate that both the average microhardness and joint efficiency of AM60 are improved by the addition of 1% Sn (mass fraction). The ultimate tensile strength of Mg?6Al?1Sn?0.3Mn (ATM610) reaches up to 96.8% of that of base material. Moreover, fracture occurs in the fusion zone ofATM610 instead of in the heat-affected zone of AM60 welded joint. The improvement in the properties is mainly attributed to the formation of Mg2Sn, which effectively obstructs the grain coarsening in the heat-affected zone, resulting in a relatively finemicrostructure. The addition of 1% Sn improves the mechanical properties of AM60 welded joint展开更多
The microstructure and mechanical properties of the gas tungsten arc welded cast A356 alloy were investigated with fillers ER1100,ER4043,ER4047 and ER5356 under the pulse frequencies of 1,3 and 5 Hz.Results showed tha...The microstructure and mechanical properties of the gas tungsten arc welded cast A356 alloy were investigated with fillers ER1100,ER4043,ER4047 and ER5356 under the pulse frequencies of 1,3 and 5 Hz.Results showed that the filler metal and pulse frequency affected the grain structure of fusion zone considerably.The highest fraction of eutectic(44%) was formed with filler ER4047.Tensile fracture of all specimens indicated that fracture did not occur in the fusion zone.The greatest impact toughness(about 4 J) was achieved for the welds with filler ER4047 while the largest hardness(HV 90) was obtained with filler ER5356.展开更多
Superior properties of maraging steels make them suitable for the fabrication of components used for military applications like missile covering, rocket motor casing and ship hulls. Welding is the main process for fab...Superior properties of maraging steels make them suitable for the fabrication of components used for military applications like missile covering, rocket motor casing and ship hulls. Welding is the main process for fabrication of these components, while the maraging steels can be fusion welded using gas tungsten arc welding(GTAW) process. All these fabricated components require longer storage life and a major problem in welds is susceptible to stress corrosion cracking(SCC). The present study is aimed at studying the SCC behaviour of MDN 250(18% Ni) steel and its welds with respect to microstructural changes. In the present study, 5.2 mm thick sheets made of MDN 250 steel in the solution annealed condition was welded using GTAW process. Post-weld heat treatments of direct ageing(480 C for 3 h), solutionizing(815 C for 1 h) followed by ageing and homogenizing(1150 C for 1 h) followed by ageing were carried out. A mixture of martensite and austenite was observed in the microstructure of the fusion zone of solutionized and direct aged welds and only martensite in as-welded condition. Homogenization and ageing treatment have eliminated reverted austenite and elemental segregation. Homogenized welds also exhibited a marginal improvement in the corrosion resistance compared to those in the as-welded, solutionized and aged condition. Constant load SCC test data clearly revealed that the failure time of homogenized weld is much longer compared to other post weld treatments, and the homogenization treatment is recommended to improve the SCC life of GTA welds of MDN 250 Maraging steel.展开更多
Variable polarity plasma arc-gas metal arc welding(VPPA-GMAW)integrates the advantages of VPPA and GMAW,and it is particularly applied to weld thick-plates aluminum alloys.High-speed camera and data acquisition system...Variable polarity plasma arc-gas metal arc welding(VPPA-GMAW)integrates the advantages of VPPA and GMAW,and it is particularly applied to weld thick-plates aluminum alloys.High-speed camera and data acquisition system were used to analyze the arc shape and the welding process electrical signal.According to the analysis of arc swing amplitude and the approximate entropy of arc voltage signal denoised by wavelet threshold method,the influence of VPPA frequency on the arc stability was studied.The results show that the approximate entropy of GMAW arc voltage decreases with the increase of VPPA frequency in a certain range,and the stability of the hybrid arc is significantly improved.The spectral analysis shows that the arc stability is reduced due to the resonance effect between the VPPA and the GMAW arc when the VPPA frequency closes to the GMAW arc pulse frequency.The results are helpful to understand hybrid welding mechanism and the selection of welding process parameters.展开更多
Welding polarity has influence on welding stability to some extent, but the specific relationship between welding polarity and weld quality has not been found, especially under the hyperbaric environment. Based on a h...Welding polarity has influence on welding stability to some extent, but the specific relationship between welding polarity and weld quality has not been found, especially under the hyperbaric environment. Based on a hyperbaric dry welding experiment system, gas metal arc welding(GMAW) experiments with direct current electrode positive(DCEP) and direct current electrode negative(DCEN) operations are carried out under the ambient pressures of 0.1 MPa, 0.4 MPa, 0.7 MPa and 1.0 MPa to find the influence rule of different welding polarities on welding spatters and weld bead geometry. The effects of welding polarities on the weld bead geometry such as the reinforcement, the weld width and the penetration are discussed. The experimental results show that the welding spatters gradually grow in quantity and size for GMAW with DCEP, while GMAW with DCEN can produce fewer spatters comparatively with the increase of the ambient pressure. Compared with DCEP, the welding current and arc voltage waveforms for DCEN is more stable and the distribution of welding current probability density for DCEN is more concentrated under the hyperbaric environment. When the ambient pressure is increased from 0.1 MPa to 1.0 MPa, the effects of welding polarities on the reinforcement, the weld width and the penetration are as follows: an increase of 0.8 mm for the weld reinforcement is produced by GMAW with DCEN and 1.3 mm by GMAW with DCEP, a decrease of 7.2 mm for the weld width is produced by DCEN and 6.1 mm by DCEP; and an increase of 3.9 mm for the penetration is produced by DCEN and 1.9 mm by DCEP. The proposed research indicates that the desirable stability in the welding procedure can be achieved by GMAW with DCEN operation under the hyperbaric environment.展开更多
基金CONACyT-México for the scholarship providedCONACyT (Project 736)SIP-IPN are also acknowledged for funds given to conduct this research
文摘Heat moving source models along with transient heat analysis by finite element method were used to determine weld thermal cycles and isothermal sections obtained from the application of a gas tungsten arc welding beads on Inconel 718 plates. Analytical (Rosenthal’s thick plate model) and finite element results show an acceptable approximation with the experimental weld thermal cycles. The isothermal sections determined by numerical simulation show a better approximation with the experimental welding profile for double-ellipse model heat distribution than Gauss model. To analyze the microstructural transformation produced by different cooling rates in the fusion and heat affected zones, Vickers microhardness measurements (profile and mapping representation) were conducted. A hardness decrement for the heat affected zone (~200 HV0.2) and fusion zone (~240 HV0.2) in comparison with base material (~350 HV0.2) was observed. This behavior has been attributed to the heterogeneous solubilization process of the γ″ phase (nickel matrix), which, according to the continuous-cooling-transformation curve, produced the Laves phase,δ and MC transition phases, generating a loss in hardness close to the fusion zone.
文摘The selection of process parameter in the gas tungsten arc (GTA) welding of titanium alloy was presented for obtaining optimum grain size and hardness. Titanium alloy (Ti-6Al-4V) is one of the most important non-ferrous metals which offers great potential application in aerospace, biomedical and chemical industries, because of its low density (4.5 g/cm^3), excellent corrosion resistance, high strength, attractive fracture behaviour and high melting point (1678℃). The preferred welding process for titanium alloy is frequent GTA welding due to its comparatively easier applicability and better economy. In the case of single pass (GTA) welding of thinner section of this alloy, the pulsed current has been found beneficial due to its advantages over the conventional continuous current process. Many considerations come into the picture and one needs to carefully balance various pulse current parameters to reach an optimum combination. Four factors, five level, central composite, rotatable design matrix were used to optimize the required number of experimental conditions. Mathematical models were developed to predict the fusion zone grain size using analysis of variance (ANOVA) and regression analysis. The developed models were optimized using the traditional Hooke and Jeeve's algorithm. Experimental results were provided to illustrate the proposed approach.
文摘An empirical relationship to predict tensile strength of pulsed current gas tungsten arc welded AZ31B magnesium alloy was developed. Incorporating process parameters such as peak current, base current, pulse frequency and pulse on time were studied. The experiments were conducted based on a four-factor, five-level, central composite design matrix. The developed empirical relationship can be effectively used to predict the tensile strength of pulsed current gas tungsten arc welded AZ31B magnesium alloy joints at 95% confidence level. The results indicate that pulse frequency has the greatest influence on tensile strength, followed by peak current, pulse on time and base current.
文摘The dissimilar joining of CP-copper to 304 stainless steel was performed by gas tungsten arc welding process using different filler materials. The results indicated the formation of defect free joint by using copper filler material. But, the presence of some defects like solidification crack and lack of fusion caused decreasing tensile strength of other joints. In the optimum conditions, the tensile strength of the joint was 96% of the weaker material. Also, this joint was bent till to 180° without any macroscopic defects like separation, tearing or fracture. It was concluded that copper is a new and good candidate for gas tungsten arc welding of copper to 304 stainless steel.
基金financially supported by the Foundation of Education Department of Guangdong Province,China (No. 2010A090200034)
文摘TiC/TisSi3 composites were fabricated on Ti-5A1-2.5Sn substrates by gas tungsten arc welding (GTAW). Identification of the phases was performed using X-ray diffraction (XRD). The microstructures were analyzed using scanning electron microscopy (SEM) combined with energy-dispersive X-ray spectrometry (EDS) and optical microscopy (OM). The Vickers hardness was measured with a micro-hardness tester. The TiC/TisSi3 composites were obtained in a double-layer track, and the Vickers hardness of the track increased by two to three times compared with the Ti-5A1-2.5Sn substrate.
基金the Thai Government scholarship given via Rajamangala University of Technology Krungthep (UTK), Bangkok, Thailand, for their financial support through this funded research project
文摘This present study applied gas tungsten arc welding in order to join AISI 304 and AISI 201 stainless steels.The objective was to find the optimum welding condition that gave a weld bead in accordance with DIN EN ISO 25817 quality level B, pitting corrosion potential of the weld metal of not less than that of the AISI304 base metal and a ratio of delta-ferrite in austenite matrix of the weld metal of not lower than 3%.Such a ratio is a criterion widely accepted to protect the weld metal from solidification cracking. At the welding current of 75 A and by using pure argon as a shielding gas 0 to 8 vol.% and applying a welding speed in the range of 2-3.5 mm·s^(-1) was found to give a complete weld bead with an increased depthper-width ratio(promote weldability). For welding speed in the range of 3 and 3.5 mm·s^(-1)(promote corrosion resistance). Increasing the welding speed in such a range decreased the amount of delta-ferrite in the austenite matrix, and increased the pitting corrosion potential of the weld metal to be 302 mV_(SCE).This value was still lower than the pitting corrosion potential of the AISI 304 base metal. Mixing nitrogen in argon shielding gas increased the nitrogen content in the weld. The optimum condition was found when using a welding speed of 3 mm· s^(-1) and mixing 1 vol.% of nitrogen in the argon shielding gas(promote weldability and corrosion resistance). Pitted areas after potentiodynamic test were observed in the austenite in which its Cr content was relatively low.
基金This research is supported by the National Natural Science Foundation of China (Grant No. 51475105).
文摘Abstract Horizontal welding is important for heavy or huge welding structures. Keyhole mode variable polarity plasma arc welding of aluminum alloy plates with medium thickness was carried out in horizontal position. The characteristic of welding defects was introduced. Preliminary experiments indicated that the undercut defect could not be eliminated easily. The relationship between welding parameters and the undercut defect showed that this deject could be lessened by using higher heat input. The fluid flow of weld pool was observed by a high speed camera. The fluid flow in weld pool was not symmetric and much of molten metal gathered in the lower part. The fluid flow velocity in the lower part was bigger than that in the upper part. To this end, the formative mechanism of the undercut defect was proposed. The flowability of the molten metal was an influential factor for the undercut defect. A preheating method was designed to verify the formative mechanism.
基金the Shandong Provincial Natural Science Foundation of China (No. Z2003F05 ).
文摘Realizing of weld penetration control in gas tungsten arc welding requires establishment of a model describing the relationship between the front-side geometrical parameters of weld pool and the back-side weld width with sufficient accuracy. A neural network model is developed to attain this aim. Welding experiments are conducted to obtain the training data set (including 973 groups of geometrical parameters of the weld pool and back-side weld width) and the verifying data set (108 groups). Two data sets are used for training and verifying the neural network, respectively. The testing results show that the model has sufficient accuracy and can meet the requirements of weld penetration control.
文摘The mechanical properties of the 2219 aluminum alloy welded joints by vertical-up variant polarity plasma arc welding (VPPAW) with keyhole were analyzed. The tensile strength of welded joints can reach 55% of that of base metal. The microstructure of weld joints was studied to explain the mechanical properties of the weld. The results show that the intensity of weld center is less than that of HAZ, and the intensity of weld center is the worst. So an advanced welding procedures is presented to reduce the heat input and increase the welding speed. The results in this procedures show that the tensile strength of welded joints reaches more than 60% of that of the parent metal, and the specific elongation does not descend.
文摘Presents penetration control by weld pool resonance which occurs when the natural frequency of weld pool is equal to the frequency of sine wave current while the weld pool is excited into oscillation by superimposing sine wave current with definite frequency or regular frequency on DC current, and experiments carried out on detecting resonance signals during both stationary and travelling arc welding with variant frequency pulse current, and concludes with experimental results that penetration control can be realized by weld pool resonance when welding speed is lower than 80mm/min, and this control method is applicable to welding thin (0.5~3.0 mm) plates of carbon steel, low alloy steel, high strength steel and superhigh strength steel, and suitable for alternating polarity welding of stainless steel, titanium alloy steel and aluminum alloy.
文摘Variable polarity plasma arc welding (VPPAW) is one of the most excellent processes used for welding aluminum alloys recently. It combines the advantages of variable polarity welding and plasma arc welding, and can achieve the most rational heat distribution and cathodic cleaning. With the VPPAW equipment developed by authors, the cathodic cleaning regularity that is one of the most important problems in VPPAW is investigated in this paper. The results will be helpful in realizing the real cleaning mechanism.
文摘Arc pressure is the key influencing factor to forming of molten pool. Countering the characteristic of tungsten inert gas arc welding with micro gap for tantalum sheet, according to the fundament of arc physics, a distribution model of arc pressure and forming mechanism of molten pool with micro butt gap are proposed, and the influences of arc pressure on forming of molten pool are discussed. Experimental researches for the dynamic formation process of weld molten pool by using high-speed vidicon camera show that when butt gap is appropriate, that is from 0. 1 to 0. 15 mm, molten metals formed on two workpiece uplift and grow up first, then are fused and form uniform molten pool finally.
文摘Temperature distribution and weld bead profiles of constant current and pulsed current gas tungsten arc welded aluminium alloy joints were compared. The effects of pulsed current welding on tensile properties, hardness profiles, microstructural features and residual stress distribution of aluminium alloy joints were reported. The use of pulsed current technique is found to improve the tensile properties of the weld compared with continuous current welding due to grain refinement occurring in the fusion zone.
基金the financial support for this study from the Malaysian Ministry of Higher Education(MOHE) through the Fundamental Research Grant Scheme and Exploratory Research Grant Scheme
文摘Double-V butt TIG welding process was performed on two plates of AA6061-T6 using ER5356 filler. The microstructure,mechanical and nanomechanical properties of the joint were evaluated in as-welded and after post weld heat treatment (PWHT) usingXRD, FESEM, EBSD, nanoindentation and tensile tests. The results show that PWHT led to microstructural recovery of the heataffected zone (HAZ) in addition to the appearance of β-phase (Al3Mg2) at the grain boundaries of weld zone. The hardness (Hnano) inall zones increased after PWHT while the elastic modulus (Enano) was improved from 69.93 GPa to 81 GPa in weld area. All resultsindicate that PWHT has created a homogenous microstructure in the weld zone in addition to outstanding improvement inmechanical properties for the weld zone which surpass the base metal.
基金Key Research and Development Project of Shandong Province(2016ZDJS05B03)Key Research and Development Project of Shandong Province(2017CXGC0812)。
文摘Keyhole gas tungsten arc welding(K-TIG)of Q345 low alloy steel plates was simulated by using SYSWELD software.The temperature field of the K-TIG welding process was simulated with three different combined heat sources and was compared with the weld profile that was obtained experimentally.The temperature field that was obtained by a combination of a double ellipsoid heat source on the upper half and a three-dimensional Gauss heat source on the lower half was similar to the real situation.The effects of plate thickness,gap and welding speed on the deformation and stress of the K-TIG welded joints were investigated by K-TIG welding numerical simulation.A reduction in the thickness of the weld plates reduced the z-direction deformation and transverse residual stress;an appropriate gap reduced the residual stress and an increase in the welding speed reduced deformation after welding,but did not help to control the residual stress after welding.
基金Project(51474043)supported by the National Natural Science Foundation of ChinaProject(2014DFG52810)supported by the Ministry of Science and Technology of China+2 种基金Projects(SRFDR 20130191110018,CDJZR13130086)supported by the Ministry of Education of ChinaProject(CSTC2013JCYJC60001)supported by the Chongqing Municipal Government,ChinaProjects(CSTC2012gg B50003,CSTC2013jj B50006)supported by the Natural Science Foundation of Chongqing Science and Technology Commission,China
文摘The effects of Sn addition on the microstructure and mechanical properties of gas tungsten arc butt-welded Mg?6Al?0.3Mn (AM60) (mass fraction, %) alloy sheets were investigated by optical microscopy, scanning electron microscopy, X-ray diffraction, transmission electron microscopy, and microhardness and tensile tests. The results indicate that both the average microhardness and joint efficiency of AM60 are improved by the addition of 1% Sn (mass fraction). The ultimate tensile strength of Mg?6Al?1Sn?0.3Mn (ATM610) reaches up to 96.8% of that of base material. Moreover, fracture occurs in the fusion zone ofATM610 instead of in the heat-affected zone of AM60 welded joint. The improvement in the properties is mainly attributed to the formation of Mg2Sn, which effectively obstructs the grain coarsening in the heat-affected zone, resulting in a relatively finemicrostructure. The addition of 1% Sn improves the mechanical properties of AM60 welded joint
基金the financial support of Shahid Chamran University through the Grant Number EN-636410
文摘The microstructure and mechanical properties of the gas tungsten arc welded cast A356 alloy were investigated with fillers ER1100,ER4043,ER4047 and ER5356 under the pulse frequencies of 1,3 and 5 Hz.Results showed that the filler metal and pulse frequency affected the grain structure of fusion zone considerably.The highest fraction of eutectic(44%) was formed with filler ER4047.Tensile fracture of all specimens indicated that fracture did not occur in the fusion zone.The greatest impact toughness(about 4 J) was achieved for the welds with filler ER4047 while the largest hardness(HV 90) was obtained with filler ER5356.
基金Financial assistance from Defence Research Development Organization (DRDO)
文摘Superior properties of maraging steels make them suitable for the fabrication of components used for military applications like missile covering, rocket motor casing and ship hulls. Welding is the main process for fabrication of these components, while the maraging steels can be fusion welded using gas tungsten arc welding(GTAW) process. All these fabricated components require longer storage life and a major problem in welds is susceptible to stress corrosion cracking(SCC). The present study is aimed at studying the SCC behaviour of MDN 250(18% Ni) steel and its welds with respect to microstructural changes. In the present study, 5.2 mm thick sheets made of MDN 250 steel in the solution annealed condition was welded using GTAW process. Post-weld heat treatments of direct ageing(480 C for 3 h), solutionizing(815 C for 1 h) followed by ageing and homogenizing(1150 C for 1 h) followed by ageing were carried out. A mixture of martensite and austenite was observed in the microstructure of the fusion zone of solutionized and direct aged welds and only martensite in as-welded condition. Homogenization and ageing treatment have eliminated reverted austenite and elemental segregation. Homogenized welds also exhibited a marginal improvement in the corrosion resistance compared to those in the as-welded, solutionized and aged condition. Constant load SCC test data clearly revealed that the failure time of homogenized weld is much longer compared to other post weld treatments, and the homogenization treatment is recommended to improve the SCC life of GTA welds of MDN 250 Maraging steel.
基金supported by the National Natural Science Foundation of China(51665044)Natural Science Foundation of Inner Mongolia(2019LH05017)+1 种基金Science and Technology Programs of Inner Mongolia(2020GG0313)Major Basic Research Open Subjects of Inner Mongolia Autonomous Region.
文摘Variable polarity plasma arc-gas metal arc welding(VPPA-GMAW)integrates the advantages of VPPA and GMAW,and it is particularly applied to weld thick-plates aluminum alloys.High-speed camera and data acquisition system were used to analyze the arc shape and the welding process electrical signal.According to the analysis of arc swing amplitude and the approximate entropy of arc voltage signal denoised by wavelet threshold method,the influence of VPPA frequency on the arc stability was studied.The results show that the approximate entropy of GMAW arc voltage decreases with the increase of VPPA frequency in a certain range,and the stability of the hybrid arc is significantly improved.The spectral analysis shows that the arc stability is reduced due to the resonance effect between the VPPA and the GMAW arc when the VPPA frequency closes to the GMAW arc pulse frequency.The results are helpful to understand hybrid welding mechanism and the selection of welding process parameters.
基金Supported by National Natural Science Foundation of China(Grant No.51275051)Innovation and Improvement Plan of Beijing Education Commission,China(Grant No.TJSHG201510017023)
文摘Welding polarity has influence on welding stability to some extent, but the specific relationship between welding polarity and weld quality has not been found, especially under the hyperbaric environment. Based on a hyperbaric dry welding experiment system, gas metal arc welding(GMAW) experiments with direct current electrode positive(DCEP) and direct current electrode negative(DCEN) operations are carried out under the ambient pressures of 0.1 MPa, 0.4 MPa, 0.7 MPa and 1.0 MPa to find the influence rule of different welding polarities on welding spatters and weld bead geometry. The effects of welding polarities on the weld bead geometry such as the reinforcement, the weld width and the penetration are discussed. The experimental results show that the welding spatters gradually grow in quantity and size for GMAW with DCEP, while GMAW with DCEN can produce fewer spatters comparatively with the increase of the ambient pressure. Compared with DCEP, the welding current and arc voltage waveforms for DCEN is more stable and the distribution of welding current probability density for DCEN is more concentrated under the hyperbaric environment. When the ambient pressure is increased from 0.1 MPa to 1.0 MPa, the effects of welding polarities on the reinforcement, the weld width and the penetration are as follows: an increase of 0.8 mm for the weld reinforcement is produced by GMAW with DCEN and 1.3 mm by GMAW with DCEP, a decrease of 7.2 mm for the weld width is produced by DCEN and 6.1 mm by DCEP; and an increase of 3.9 mm for the penetration is produced by DCEN and 1.9 mm by DCEP. The proposed research indicates that the desirable stability in the welding procedure can be achieved by GMAW with DCEN operation under the hyperbaric environment.