Surface characteristics of electroless nickel plated electromagnetic shielding wood veneer 被引量:6
1
作者 WANG Li-juan LI Jian LIU Yi-xing 《Journal of Forestry Research》 SCIE CAS CSCD 2005年第3期233-236,共4页
Wood is a kind of porous natural material with very poor electro-conductivity, and it has almost no function of electromagnetic shielding. The method of electroless nickel plating was used to produce wooden material w... Wood is a kind of porous natural material with very poor electro-conductivity, and it has almost no function of electromagnetic shielding. The method of electroless nickel plating was used to produce wooden material with electrical and effective electromagnetic shielding properties. Ni-P alloy layer was obtained on wood surface. The surface feature of plated wood veneer was observed by SEM and the surface composition and microstructure of the layer under different conditions were investigated by EDS and XRD respectively. Meanwhile, the relevant surface resistivity and electromagnetic shielding effectiveness were measured. Correlations of the phosphorous content in the layer to the structure of Ni-P alloy, electro-conductivity and electromagnetic shielding of plated veneers were discussed. SEM photos showed that the surface of electroless nickel plated veneers were covered with Ni-P alloy layer entirely, which made wood veneers more like metal. At the same time, the results showed that with the decreasing of the phosphorous content in the layer, the microstructure of Ni-P alloy layer transformed to be microcrystalline and electro-conductivity and electromagnetic shielding effectiveness were improved. When the phosphorous content was less than 2.37wt pct in the layer, the microstructure of Ni-P alloy layer was microcrystalline structure and its sur- face resistivity and electromagnetic shielding effectiveness were nearly 0.5Ω/□ and 55-60dB respectively. 展开更多
关键词 wood veneer Electroless nickel plating Phosphorous content MICROSTRUCTURE Electromagnetic shielding
下载PDF
微胶囊释香饰面板的制备及其香气缓释性能评价
2
作者 陈媛 沈云芳 +5 位作者 赵建忠 桂成胜 郝小蒙 范东斌 李改云 吕斌 《福建农林大学学报(自然科学版)》 CAS CSCD 北大核心 2024年第4期570-576,共7页
【目的】制备稳定、持久释香的饰面板,并建立缓释性能评价方法,实现规模化生产。【方法】采用微胶囊和树脂复合包覆方法制备释香型浸渍胶膜纸饰面板;采用固相微萃取-气相-质谱联用技术(solid-phase microextraction-gas chromatography-... 【目的】制备稳定、持久释香的饰面板,并建立缓释性能评价方法,实现规模化生产。【方法】采用微胶囊和树脂复合包覆方法制备释香型浸渍胶膜纸饰面板;采用固相微萃取-气相-质谱联用技术(solid-phase microextraction-gas chromatography-mass spectrometry,SPME-GC-MS),通过人工嗅闻直测法和气味分级法分析了释香饰面板在50℃下480 h的加速释香过程,揭示其香气释放机制,并建立香气缓释性能的快速评价方法。【结果】添加0.75%释香微胶囊的饰面板释香效果最优;微胶囊经热压后仍能均匀分布在胶层的表面和内部,壁材和胶层起到协同缓释香气的作用,且香气主成分(芳樟醇)的释放与温度、时间呈正相关。【结论】制备了持久、稳定释香的饰面板,并通过香气加速释放和干燥器富集法建立了香气缓释性能快速评测方法。 展开更多
关键词 释香浸渍胶膜纸 释香饰面板 微胶囊 释香性能 加速释香
下载PDF
桉木单板背面裂隙率对胶合板性能的影响
3
作者 黄腾华 宋恋环 +3 位作者 黎小波 雷福娟 黄忠良 王军锋 《广西林业科学》 2024年第2期262-267,共6页
为给胶合板生产过程的组坯工艺优化提供理论依据,采用图像处理技术与宏观力学性能试验相结合,分析桉木单板背面裂隙率对胶合板性能的影响,探讨桉木单板背面裂隙率与胶合板性能的相关性。结果表明,不同单板背面裂隙率下,干状、冷水浸泡2... 为给胶合板生产过程的组坯工艺优化提供理论依据,采用图像处理技术与宏观力学性能试验相结合,分析桉木单板背面裂隙率对胶合板性能的影响,探讨桉木单板背面裂隙率与胶合板性能的相关性。结果表明,不同单板背面裂隙率下,干状、冷水浸泡24 h和热水浸泡3 h胶合板的胶合强度及顺纹静曲强度均差异极显著,横纹静曲强度、横纹弹性模量和顺纹弹性模量均差异不显著。随单板背面裂隙率增大,胶合板在3种条件下的胶合强度、顺纹静曲强度和顺纹弹性模量均呈下降趋势。相关性分析表明,单板背面裂隙率与干状胶合强度、冷水浸泡24 h胶合强度和顺纹静曲强度均呈极显著负相关,与顺纹弹性模量呈显著负相关。单板背面裂隙率对胶合板性能的影响表现为冷水浸泡24 h胶合强度>干状胶合强度>顺纹静曲强度>顺纹弹性模量>热水浸泡3 h胶合强度>横纹弹性模量>横纹静曲强度。 展开更多
关键词 单板背面裂隙率 性能 桉木 胶合板
下载PDF
施胶方式和单板厚度对重组木物理力学性能的影响
4
作者 孙忠海 于文吉 +1 位作者 张方达 孙建斌 《林产工业》 北大核心 2024年第9期1-4,共4页
采用不同树种的不同厚度单板制备重组木,考察了单板施胶方式、厚度和树种对重组木耐水性能与抗弯性能的影响。结果表明:在0.7~2.2 mm范围内,树种和单板厚度相同时,采用单板表面喷胶制备重组木的吸水厚度膨胀率低于单板浸胶制备的重组木... 采用不同树种的不同厚度单板制备重组木,考察了单板施胶方式、厚度和树种对重组木耐水性能与抗弯性能的影响。结果表明:在0.7~2.2 mm范围内,树种和单板厚度相同时,采用单板表面喷胶制备重组木的吸水厚度膨胀率低于单板浸胶制备的重组木,静曲强度高于后者。树种相同时,单板越厚制备的重组木耐水性能越差。单板厚度和树种对重组木的静曲强度影响较大。单板厚度相同时,桉木重组木的耐水性能和弹性模量高于杨木重组木,但静曲强度低于后者。本研究可为薄单板制备重组木原料和施胶工艺的选择提供重要参考依据。 展开更多
关键词 重组木 施胶方式 单板厚度 树种 耐水性能 抗弯性能
下载PDF
木质重组材单板卷曲辊压成型平台设计与试验
5
作者 张国梁 沈明哲 +2 位作者 胡继文 邢义虎 李文浩 《农业工程学报》 EI CAS CSCD 北大核心 2024年第11期271-281,共11页
低品质木制单板制备重组材是其高值化利用的重要途径,研发连续式重组材成型技术有利于提高其生产效率,对促进木材可持续发展和经济社会绿色发展具有重要意义。该研究设计一种木制重组材单板卷曲辊压成型平台,并以木质管道制备为例对工... 低品质木制单板制备重组材是其高值化利用的重要途径,研发连续式重组材成型技术有利于提高其生产效率,对促进木材可持续发展和经济社会绿色发展具有重要意义。该研究设计一种木制重组材单板卷曲辊压成型平台,并以木质管道制备为例对工艺参数进行优化试验研究以测试平台工作性能。设计单板卷曲辊压成型平台的整机机械结构并描述其工作原理,对辊压机构、卷木轴刹车防滑机构、施胶压紧装置等关键部件进行详细设计和理论计算。对物理样机进行性能试验,以芯轴转速、单板厚度、施加压力为试验因素,木质管道的环刚度和轴向压缩强度为试验指标,运用Box-Benhnken试验方法,建立因素与试验指标的回归方程,优化参数组合为芯轴转速16 r/min,单板厚度2.15 mm,施加压力293 N。此时预测木质管道的环刚度为26 016.6 N/m^(2),轴向压缩强度为23.11 MPa验证环刚度与预测值误差为1.07%,轴向压缩强度误差为4.46%。进一步使用优化参数对内径为5.08、7.62、12.70 cm的木质管道进行试验,得到环刚度分别为43 812、32 655、17 532 N/m^(2),轴向压缩强度为25.83、24.71、20.17 MPa。该研究成果可为木质重组材卷曲辊压成型技术及装备的工业化应用提供参考。 展开更多
关键词 单板 辊压成型 木质管道 响应面试验
下载PDF
LVL结构调控及应用研究进展
6
作者 陈武 黄素涌 +2 位作者 王建和 卫佩行 王兴宇 《林产工业》 北大核心 2024年第5期70-76,共7页
在我国木材资源紧缺、人工林材质较差、而竹材资源较为丰富的背景下,单板层积材(Laminated Veneer Lumber,LVL)作为一种生物质工程材料,具备高效利用现有资源的优势,并且以其出色的力学性能可实现标准化、系列化生产,展现出广阔的应用... 在我国木材资源紧缺、人工林材质较差、而竹材资源较为丰富的背景下,单板层积材(Laminated Veneer Lumber,LVL)作为一种生物质工程材料,具备高效利用现有资源的优势,并且以其出色的力学性能可实现标准化、系列化生产,展现出广阔的应用前景。本文结合我国人造板产业的发展现况,概述了LVL的起源和发展,着重从复合材料力学性能的角度分析了LVL的结构特点,对单板分等和LVL组坯特点进行了介绍。同时,综述了酚醛树脂浸渍和纤维材料复合两种LVL增强方式。最后,对比讨论了国内外LVL的评价标准,并针对我国木结构建筑产业的发展现状和LVL应用过程中存在的问题,提出了若干建议。 展开更多
关键词 单板层积材 单板分等 竹木复合 复合材料增强 胶合性能
下载PDF
木皮在汽车智能内饰表面透光性能研究 被引量:1
7
作者 何平 戴晓东 +2 位作者 沈朝梁 余鹏 张学昌 《时代汽车》 2024年第8期136-138,共3页
为满足客户对汽车座舱驾驶性和舒适性需求,汽车内饰研发设计趋向智能化和集成化发展。针对内饰透光表皮材质透光率低及表面图标显示不清晰等问题,以木皮在汽车内饰件应用为研究开展相关透光率实验及图标透光研究。结果表明,木皮的透光... 为满足客户对汽车座舱驾驶性和舒适性需求,汽车内饰研发设计趋向智能化和集成化发展。针对内饰透光表皮材质透光率低及表面图标显示不清晰等问题,以木皮在汽车内饰件应用为研究开展相关透光率实验及图标透光研究。结果表明,木皮的透光性能取决于木皮材料、厚度及表面处理技术。在满足木皮表面图案透光性能条件下,木皮表面孔径及孔距需满足尺寸要求。通过透光性能研究为木皮大量应用于汽车智能内饰提供参考。 展开更多
关键词 木皮 透光率 图标透光 尺寸要求
下载PDF
净醛抗菌饰面人造板分析研究
8
作者 金祥龙 任士超 《科技资讯》 2024年第6期108-110,共3页
研究净醛抗菌组合物与净醛抗菌饰面人造板的制备工艺,分析净醛抗菌饰面人造板的净醛、抗菌、防霉和去TVOC等环保性能。结果表明:以甲壳素、医用级2-咪唑烷酮、N掺杂改性纳米TiO_(2)或纳米硅片为主要原料,经过高速搅拌混合均匀后,按照一... 研究净醛抗菌组合物与净醛抗菌饰面人造板的制备工艺,分析净醛抗菌饰面人造板的净醛、抗菌、防霉和去TVOC等环保性能。结果表明:以甲壳素、医用级2-咪唑烷酮、N掺杂改性纳米TiO_(2)或纳米硅片为主要原料,经过高速搅拌混合均匀后,按照一定比例添加在浸渍胶膜饰面纸浸胶工艺中并将其充分溶解,所制备的净醛抗菌饰面人造板,具有良好的净醛、抗菌、防霉、去TVOC等功效。 展开更多
关键词 净醛 抗菌 饰面人造板 环保性能
下载PDF
CaCO_(3)矿化装饰薄木的制备及其阻燃性能
9
作者 何叶 卢钰鑫 +3 位作者 刘琼瑶 屈熙 方露 唐启恒 《林业工程学报》 CSCD 北大核心 2024年第2期47-54,共8页
装饰薄木的易燃性限制了其在家具饰面、室内装饰等领域的应用。为了提升装饰薄木的阻燃性能,采用仿生呼吸法将氯化钙(CaCl_(2))溶液与碳酸氢钠(NaHCO_(3))溶液分段浸渍于薄木中以制备矿化装饰薄木。通过傅里叶变换红外光谱(FT-IR)和环... 装饰薄木的易燃性限制了其在家具饰面、室内装饰等领域的应用。为了提升装饰薄木的阻燃性能,采用仿生呼吸法将氯化钙(CaCl_(2))溶液与碳酸氢钠(NaHCO_(3))溶液分段浸渍于薄木中以制备矿化装饰薄木。通过傅里叶变换红外光谱(FT-IR)和环境扫描电镜(ESEM)对矿化产物进行了分析,并且采用宏观燃烧试验、热重分析法(TG)与锥形量热仪(CONE),对改性处理后薄木的阻燃性能进行评价。结果表明:矿化处理后薄木表面与内部均原位生成了方解石型CaCO_(3),且CaCO_(3)的生成量随着浸渍溶液浓度增大而增加。附着于薄木表面的CaCO3具有防火屏障功能,当浸渍溶液浓度由0.2 mol/L增加到1.0 mol/L及以上时,矿化薄木的着火时间得到明显延长。CaCO_(3)能催化纤维素热解,有利于产生稳定焦炭,TG结果显示,当浸渍溶液浓度为1.8 mol/L时,矿化薄木残炭率为28.05%,与未处理薄木相比提升了81.55%,阻燃效果最佳。CONE测试结果显示:与未处理薄木相比矿化薄木的热释放速率、有效燃烧热大幅降低,阻燃性能显著提升;但是矿化薄木的横向抗拉强度随浸渍溶液浓度增大而减小,对后续使用存在影响。综合考虑认为采用1.0 mol/L浓度的浸渍溶液对薄木进行矿化处理,可以使其获得良好的阻燃性能,同时保持一定的横向抗拉强度。 展开更多
关键词 装饰薄木 阻燃改性 原位生成法 矿化木材
下载PDF
Preparation of electromagnetic shielding wood-metal composite by electroless nickel plating 被引量:12
10
作者 WANG Li-juan LI Jian LIU Yi-xing 《Journal of Forestry Research》 SCIE CAS CSCD 2006年第1期53-56,共4页
Electrical and electromagnetic shielding wood metal composite was prepared by using electroless nickel plating. The effects of solution amount, plating time and plating temperature on surface resistivity and electroma... Electrical and electromagnetic shielding wood metal composite was prepared by using electroless nickel plating. The effects of solution amount, plating time and plating temperature on surface resistivity and electromagnetic shielding effectiveness were investigated. And P content, microstructure and surface feature of layers obtained at different temperatures were analyzed by energy dispersion spectrometer (EDS), X-ray diffraction (XRI)) and scanning electron microscopy (SEM). The results showed that layers with higher electro-conductivity and electromagnetic shielding effectiveness were obtained under the optimum conditions that plating solution was 500 mL, plating time was 30 min and plating temperature was 62℃. The results showed by EDS analysis; that P content increased gradually in a small extent with plating temperature increased. It was showed by XRD and SEM analysis that layers plated at different temperatures were all microcrystalline structure and uniform and successive, which had noticeable metal luster. Those indicated that plating temperature had little influence on microstructure and surface feature under pH value invariable. 展开更多
关键词 wood veneer Electroless plating COMPOSITE Surface resistivity Electromagnetic shielding
下载PDF
补片形状对修补的杨木单板力学性能的影响 被引量:2
11
作者 刘诚 刘伟 +1 位作者 花军 司竹君 《东北林业大学学报》 CAS CSCD 北大核心 2023年第2期123-127,137,共6页
以同一批次旋切杨木单板为试验对象,设计船形、菱形、锯齿形、双圆形、蝶形5种补片(为与仿真试验进行对比,试验单板及补片的尺寸均依据相关标准及仿真尺寸进行设计),用环氧树脂胶黏剂进行粘贴,制备静态拉伸试验试件;按照国家标准GB/T 36... 以同一批次旋切杨木单板为试验对象,设计船形、菱形、锯齿形、双圆形、蝶形5种补片(为与仿真试验进行对比,试验单板及补片的尺寸均依据相关标准及仿真尺寸进行设计),用环氧树脂胶黏剂进行粘贴,制备静态拉伸试验试件;按照国家标准GB/T 36408—2018《木结构用单板层积材》、GB/T 14017—2009《木材横纹抗拉强度实验方法》,应用济南试金WDW-300E微机控制电子式万能试验机,对5种补片每组设置的20个单板试样进行木材顺纹抗拉试验,测定补片修补单板断裂应力值、应用扫描电子显微镜观测补片修补单板断裂的微观形态。应用数值模拟方法,依据汉克森(Hankinson)失效理论,对设计的5种补片形状的修补单板仿真模型进行拉伸模拟试验,计算5种不同补片形状修补单板仿真模型的断裂失效应力值。对比实测与仿真试验结果,检验仿真的有效性,分析木质单板缺陷挖补技术中补片形状对修补的木质单板力学性能的影响及单板的断裂模式。结果表明:①5种补片中,除菱形补片外,其余单板的失效单元均沿45°方向延伸,在电镜观测下试样断裂位置显示有多处细胞壁发生断裂,这些细胞与板壁的断裂细胞壁相连形成了宏观裂缝。②在数值模拟与实测中,蝶形、菱形补片修补后单板的承载能力均较大,其失效载荷值分别为31.3、29.7 MPa;菱形、锯齿形、双圆形、蝶形4种形状的补片,比船形补片的承载能力提升了25.52%~30.18%;蝶形补片的承载能力最大且与节子形状契合度最高。③仿真与实测,差值均在12.1%以内,验证了仿真的可行性。 展开更多
关键词 杨木 木材单板 补片形状 单板力学性能
下载PDF
新型纤维化单板高性能木质重组材料制造工艺研究进展 被引量:2
12
作者 郭明辉 钟昊 张浩 《生物质化学工程》 CAS 2023年第3期1-7,共7页
简述了木质重组材料的起源与发展,主要对我国提出的新型纤维化单板高性能木质重组材料制造工艺具体环节的研究进展进行了综述。在原始木材碾压疏解阶段,随着疏解度的提高,木质重组材料的物理力学性能也随之增强。在纤维化单板改性阶段,... 简述了木质重组材料的起源与发展,主要对我国提出的新型纤维化单板高性能木质重组材料制造工艺具体环节的研究进展进行了综述。在原始木材碾压疏解阶段,随着疏解度的提高,木质重组材料的物理力学性能也随之增强。在纤维化单板改性阶段,改性处理提高了木质重组材料的防火、防霉性能,赋予了木质重组材料多功能性。总结了不同树种在浸胶阶段,浸胶方法和浸胶量对木质重组材料力学强度和功能性的差异。分析了组坯阶段的组坯方式和设备对木质重组材料强度及尺寸稳定性的影响。归纳了压制阶段中热压法和冷压热固化法两种压制方式各自的优势与不足。最终围绕木质重组材料的缺陷和现有的木质材料高附加值利用案例,针对提高木质重组材料的强度以及拓宽其应用提出了一些新设想。 展开更多
关键词 木质重组材料 纤维化单板 胶黏剂
下载PDF
米级透明木单板的制备及性能
13
作者 唐启恒 邹淼 +3 位作者 张镭 郭文静 常亮 高黎 《木材科学与技术》 北大核心 2023年第5期47-52,共6页
透明木材现有的制造工艺技术只能制备出小尺寸样品,距离产业化应用较远。本研究以桦木(Betula sp.)单板为原料,采用漂白工艺制备大幅面脱色木单板,在真空条件下浸渍环氧树脂,固化后可制得长度达1 m的透明木单板。研究结果表明,透明木单... 透明木材现有的制造工艺技术只能制备出小尺寸样品,距离产业化应用较远。本研究以桦木(Betula sp.)单板为原料,采用漂白工艺制备大幅面脱色木单板,在真空条件下浸渍环氧树脂,固化后可制得长度达1 m的透明木单板。研究结果表明,透明木单板具有良好的透光性能,其平均透光率约为76.7%,雾度为81.4%;因环氧树脂浸入木材细胞中,透明木单板纵、横向的拉伸强度均大于处理前单板的强度;最后对米级透明木单板的制备工艺及成本进行分析。透明木材可应用于建筑天井、汽车天窗、办公室和卫生间的门窗、隔断等隐蔽空间,研究成果可为透明木材的工业化应用奠定理论基础。 展开更多
关键词 米级透明木单板 环氧树脂 制造工艺
下载PDF
水性环氧树脂制备桉木单板层积材及性能研究 被引量:3
14
作者 陈淼文 郑霞 +2 位作者 李新功 吴义强 沈昕祎 《林产工业》 北大核心 2023年第4期1-7,共7页
选用双组分水性环氧树脂为胶黏剂,速生桉木单板为基材,热压制备结构用桉木单板层积材。采用单因素试验法研究了施胶量、热压温度、热压时间、热压压力对水性环氧树脂单板层积材弹性模量、静曲强度、水平剪切强度、含水率和浸渍剥离率等... 选用双组分水性环氧树脂为胶黏剂,速生桉木单板为基材,热压制备结构用桉木单板层积材。采用单因素试验法研究了施胶量、热压温度、热压时间、热压压力对水性环氧树脂单板层积材弹性模量、静曲强度、水平剪切强度、含水率和浸渍剥离率等物理力学性能的影响。结果表明:水性环氧树脂以水为分散剂,在木质单板表面延展性良好。当施胶量为230 g/m^(2),热压温度为120℃,热压时间为1.0 min/mm,热压压力为2 MPa时,单板层积材各项性能较优,符合GB/T20241—2006《单板层积材》要求。提出的以水性环氧树脂为胶黏剂的层积材制备工艺适合工业化生产,产品力学性能优良且无醛/低醛释放,绿色环保,具有积极的推广意义。 展开更多
关键词 桉木 水性环氧树脂 单板层积材 性能 热压工艺
下载PDF
阻燃板贴木皮胶粘剂的制备 被引量:1
15
作者 张伟 周健 +5 位作者 次立杰 苏翠伟 胡江浦 陈石 王康 许炳琨 《煤炭与化工》 CAS 2023年第7期122-126,130,共6页
为了解决阻燃板与木皮粘接不牢的问题,通过分析阻燃板的表面形貌和界面特征,提出了一种新型聚丙烯酸酯胶粘剂的解决方案。通过由自由基聚合合成得到的带有羟基的聚丙烯酸酯预聚物与异氰酸酯固化剂复配,得到双组分聚氨酯型胶粘剂,通过配... 为了解决阻燃板与木皮粘接不牢的问题,通过分析阻燃板的表面形貌和界面特征,提出了一种新型聚丙烯酸酯胶粘剂的解决方案。通过由自由基聚合合成得到的带有羟基的聚丙烯酸酯预聚物与异氰酸酯固化剂复配,得到双组分聚氨酯型胶粘剂,通过配方调试,使该胶粘剂在杨木木皮饰面与阻燃板之间形成良好的粘接效果,并通过间接法(剪切强度)和直接法(木皮残留率)2种方法进行评价。研究结果表明:所合成的丙烯酸酯预聚物的玻璃化转变温度(Tg)在20℃、羟值为25 mgKOH/g,主固比为5∶1、纳米钙填料用量为30%时,粘接效果最佳,其剪切强度可以达到3.10 MPa,木皮残留率为85%。 展开更多
关键词 阻燃板 薄木饰面 聚丙烯酸酯 胶粘剂 粘接强度
下载PDF
装饰单板漂白染色的色差调控 被引量:2
16
作者 何盛 吴再兴 +2 位作者 丁永欢 卢晓相 陈玉和 《林业工程学报》 CSCD 北大核心 2023年第1期189-194,共6页
针对装饰单板因色差导致降等,产品附加值降低问题,采用漂白染色处理方法对装饰单板进行色差调控,分析不同处理条件下单板色度和色差变化及其色差调控机理。研究结果显示,漂白处理对白蜡木、黑胡桃的色差调控效果较好,其中白蜡木色差从8... 针对装饰单板因色差导致降等,产品附加值降低问题,采用漂白染色处理方法对装饰单板进行色差调控,分析不同处理条件下单板色度和色差变化及其色差调控机理。研究结果显示,漂白处理对白蜡木、黑胡桃的色差调控效果较好,其中白蜡木色差从8.80降至0.74,黑胡桃从11.51降至2.97。深色染料处理的色差调控效果最佳(色差小于4.0)。方差分析和多重比较结果显示,处理条件、树种与处理条件的交互作用对色差调控结果影响极显著(P<0.05)。对照样与漂白、浅色与深色染料染色后单板色差差异明显,浅色染料染色与漂白处理样和深色染色处理样色差差异不明显。漂白染色处理对单板色差调控机理主要是漂白处理过程中对木质素和内含物中发色基团的降解,以及染色过程中染料对单板底色形成良好的覆盖。研究成果可实现在不遮盖单板纹理条件下装饰单板色彩均一化,减小色差,同时赋予单板丰富的色彩,为低等级装饰单板的高值化利用提供技术和理论支撑。 展开更多
关键词 装饰单板 漂白染色 色差调控 调控机理
下载PDF
高性能重组木研究进展及应用建议 被引量:1
17
作者 陈松武 刘晓玲 +1 位作者 陈桂丹 何林韩 《林产工业》 北大核心 2023年第9期57-62,共6页
重组木作为一种“小材大用、劣材优用”的绿色木质材料,是人工林速生材未来极具发展前景的加工利用途径之一,能够有效缓解我国木材的供需矛盾。本文围绕重组木的高性能化制备,重点阐述了不同处理工艺条件对其性能的影响,总结了其在工业... 重组木作为一种“小材大用、劣材优用”的绿色木质材料,是人工林速生材未来极具发展前景的加工利用途径之一,能够有效缓解我国木材的供需矛盾。本文围绕重组木的高性能化制备,重点阐述了不同处理工艺条件对其性能的影响,总结了其在工业化进程中面临的难题,并提出了相应解决方法。其中,着重针对重组木产品应用的高值化与功能化短缺的现状,根据重组木的性能特点构思了“重组木材色定向调控”及“高性能木质强化玻璃”的新概念,以期为我国速生材资源高值化利用的产业升级提供解决思路和途径。 展开更多
关键词 重组木 高性能 小径材 疏解单板 综述
下载PDF
三聚氰胺胶膜纸复贴科技木皮甲醛释放量研究 被引量:1
18
作者 栾洁 李东飞 +2 位作者 冯沁雄 曾永明 陈松武 《热带林业》 2023年第4期90-92,95,共4页
三聚氰胺胶膜纸复贴科技木皮中含有甲醛,可采用干燥器法收集甲醛,用分光光度计法测试甲醛释放量。该研究通过多组实验数据分析,确定样品的数量、测试的时间、温度,得到测试甲醛释放量的最优检测条件,对控制三聚氰胺胶膜纸复贴科技木皮... 三聚氰胺胶膜纸复贴科技木皮中含有甲醛,可采用干燥器法收集甲醛,用分光光度计法测试甲醛释放量。该研究通过多组实验数据分析,确定样品的数量、测试的时间、温度,得到测试甲醛释放量的最优检测条件,对控制三聚氰胺胶膜纸复贴科技木皮的甲醛释放量有重要意义,推动人造板产业高质量发展。 展开更多
关键词 甲醛 三聚氰胺胶膜纸复贴科技木皮 甲醛测试
下载PDF
澳大利亚与新西兰结构用单板层积材标准要求解读 被引量:10
19
作者 李文强 李杰 +1 位作者 王兴军 王豪 《森林防火》 2023年第4期161-167,共7页
基于澳大利亚与新西兰结构用单板层积材产品标准AS/NZS 4357.0-2022 Structural laminated veneer lumber Part 0:Specification,对结构用单板层积材的木单板等级分等、胶合性能、甲醛释放量、F-Grade等级划分与计算等方面的要求进行了... 基于澳大利亚与新西兰结构用单板层积材产品标准AS/NZS 4357.0-2022 Structural laminated veneer lumber Part 0:Specification,对结构用单板层积材的木单板等级分等、胶合性能、甲醛释放量、F-Grade等级划分与计算等方面的要求进行了讨论,试制国产马尾松结构用单板层积材样品并按照标准要求进行了型式检测。检测结果表明国产马尾松结构用单板层积材产品性能满足标准AS/NZS 4357.0-2022中规定的F14级限量值要求。 展开更多
关键词 结构用单板层积材 国产马尾松 工程木制材料 检测认证 产品标准
下载PDF
实木复合地板低等级面板利用优化技术研究
20
作者 徐卫东 冯迪 +1 位作者 潘悦 李鑫 《中国人造板》 2023年第4期12-15,共4页
实木复合地板的面板价格是决定实木复合地板生产成本的关键因素。本文研究低等级面板利用优化技术,通过压花、印木射线涂装、辊印、数码打印4项工艺提升低等级面板的利用率,创造实木复合地板的成本优势,提高企业市场竞争力。
关键词 实木复合地板 面板 利用优化技术