A new method--the inverse strain method(ISM)for preventing welding hot cracking of high strength aluminium alloy LY12CZ
1
作者 Tian Xitang Zhang Xiuzhi Liu weiping Harbin Institute of Technology 《China Welding》 EI CAS 1992年第2期128-134,共7页
In this paper a new method for preventing welding hot cracking—the inverse strain method(ISM)is developed on the principle of welding mechan- ics.Effectiveness and feasiblity of method in preventing welding hot crack... In this paper a new method for preventing welding hot cracking—the inverse strain method(ISM)is developed on the principle of welding mechan- ics.Effectiveness and feasiblity of method in preventing welding hot cracking of high strength aluminum alloy LY12CZ by synchronous rolling during welding (SRDW)along both sides of the weld at a suitable distance behind the welding arc are examined.Experimental resulte indicate that welding hot cracking of LY12CY can be effectively prevented and the mechanical properties of welded joint can also be improved by the method.It is an important new solution for preventing hot cracking in welding of sheet metal. 展开更多
关键词 weld hot cracking 2024alloy inverse strain method synchronous rolling
下载PDF
Controlling of weld hot cracks of aluminum alloy sheets by transverse pre-stressing 被引量:1
2
作者 LIU Xuesong,ZHOU Guangtao,WANG Ping,and FANG Hongyuan State Key Laboratory of Advanced Welding Technology Production,Harbin Institute of Technology,Harbin 150001,China 《Rare Metals》 SCIE EI CAS CSCD 2007年第S1期157-161,共5页
A new ideological and theoretical model—a technology to control weld hot cracks by transverse compressive pre-stress in the welding of aluminum alloy was put forward,which was further proved by the subsequent self-de... A new ideological and theoretical model—a technology to control weld hot cracks by transverse compressive pre-stress in the welding of aluminum alloy was put forward,which was further proved by the subsequent self-designed test setup.Experiments are conducted on the fishbone shaped specimen under conventional welding and welding with various pre-stress values.The experimental results turn out that,the initiation rate of the weld hot cracks decreases with increasing values of the compressive pre-stress.When the pre-stress reaches 0.3-0.4 of the yield stress,the cracks even disappear.In mechanical viewpoint,the researches here develop a new way to control weld cracks. 展开更多
关键词 welding with transverse pre-stress weld hot cracks crack initiation rate