Using highspeed camera image measuring and processing,the contour of the weld pool was extracted accurately in pulsed metal inert gas(P-MIG)welding.Based on this extraction method,time and frequency domain characteris...Using highspeed camera image measuring and processing,the contour of the weld pool was extracted accurately in pulsed metal inert gas(P-MIG)welding.Based on this extraction method,time and frequency domain characteristics at different points along the contour of the weld pool were analyzed for one pulse one droplet and one pulse two droplets,respectively.The results show that,because of the wave super position that was created by the pulsed arc and droplet impacting the weld pool,the oscillation amplitude along the weld pool fluctuated and decreased with an increase in distance from the point to the arc center.The oscillation near the arc center was complex and intense for one pulse two droplets,and the amplitude were relatively small because the oscillation caused by the pulsed arc could be offset by the molten droplet impact.The weld pool oscillation that was caused by the pulsed arc was stronger than that caused by the droplet.展开更多
Laser oscillating welding was employed to fabricate Al-Si coated press-hardened steel(PHS)to improve the element homogeneity in the fusion zone.Laser oscillating welding was employed with various oscillation amplitude...Laser oscillating welding was employed to fabricate Al-Si coated press-hardened steel(PHS)to improve the element homogeneity in the fusion zone.Laser oscillating welding was employed with various oscillation amplitudes(0 mm,0.5 mm and 1.3 mm)in this present.Ni foil of 0.06 mm thickness was used as an interlayer between two tailored PHS welded.The weld morphology,elemental profile,microstructure and tensile strength of welded joints were studied.The results showed that full penetration weld without any weld defects were achieved for any oscillation amplitudes,and weld width increased with increasing oscillation amplitudes.With the oscillation amplitudes increased,Ni and Al had an uneven elemental profile due to strong stirring force,but the Ni and Al content in the weld was decreased and Ni had a sharp descent compared to Al element.Only fewδ-ferrite was presented in fusion line with the oscillation amplitudes increased to 1.3 mm.The oscillation amplitudes did not have an effect on the tensile properties,which was similar to that of base metal.But if keeping increasing the oscillation amplitudes or reducing the thickness of Ni interlayer,it has a potential risk to form more and moreδferrite such that deteriorate the mechnical properties of welded joints.展开更多
基金This work was supported by the National Natural Science Foundation of China(Grant Numbers 51205283).
文摘Using highspeed camera image measuring and processing,the contour of the weld pool was extracted accurately in pulsed metal inert gas(P-MIG)welding.Based on this extraction method,time and frequency domain characteristics at different points along the contour of the weld pool were analyzed for one pulse one droplet and one pulse two droplets,respectively.The results show that,because of the wave super position that was created by the pulsed arc and droplet impacting the weld pool,the oscillation amplitude along the weld pool fluctuated and decreased with an increase in distance from the point to the arc center.The oscillation near the arc center was complex and intense for one pulse two droplets,and the amplitude were relatively small because the oscillation caused by the pulsed arc could be offset by the molten droplet impact.The weld pool oscillation that was caused by the pulsed arc was stronger than that caused by the droplet.
基金National Natural Science Foundation of China(Grant No.52005357)“Qinglan”Project of Jiangsu Province of China,and Jiangsu Provincial Natural Science Foundation of China(Grant No.BK 20180984).
文摘Laser oscillating welding was employed to fabricate Al-Si coated press-hardened steel(PHS)to improve the element homogeneity in the fusion zone.Laser oscillating welding was employed with various oscillation amplitudes(0 mm,0.5 mm and 1.3 mm)in this present.Ni foil of 0.06 mm thickness was used as an interlayer between two tailored PHS welded.The weld morphology,elemental profile,microstructure and tensile strength of welded joints were studied.The results showed that full penetration weld without any weld defects were achieved for any oscillation amplitudes,and weld width increased with increasing oscillation amplitudes.With the oscillation amplitudes increased,Ni and Al had an uneven elemental profile due to strong stirring force,but the Ni and Al content in the weld was decreased and Ni had a sharp descent compared to Al element.Only fewδ-ferrite was presented in fusion line with the oscillation amplitudes increased to 1.3 mm.The oscillation amplitudes did not have an effect on the tensile properties,which was similar to that of base metal.But if keeping increasing the oscillation amplitudes or reducing the thickness of Ni interlayer,it has a potential risk to form more and moreδferrite such that deteriorate the mechnical properties of welded joints.