期刊文献+
共找到61,543篇文章
< 1 2 250 >
每页显示 20 50 100
Nanoscale Zero-Valent Iron(nZVI)for Heavy Metal Wastewater Treatment:A Perspective
1
作者 Shaolin Li Lei Li Weixian Zhang 《Engineering》 SCIE EI CAS CSCD 2024年第5期16-20,共5页
Industries such as non-ferrous metal smelting discharge billions of gallons of highly toxic heavy metal wastewater(HMW)worldwide annually,posing a severe challenge to conventional wastewater treatment plants and harmi... Industries such as non-ferrous metal smelting discharge billions of gallons of highly toxic heavy metal wastewater(HMW)worldwide annually,posing a severe challenge to conventional wastewater treatment plants and harming the environment.HMW is traditionally treated via chemical precipitation using lime,caustic,or sulfide,but the effluents do not meet the increasingly stringent discharge standards.This issue has spurred an increase in research and the development of innovative treatment technologies,among which those using nanoparticles receive particular interest.Among such initiatives,treatment using nanoscale zero-valent iron(nZVI)is one of the best developed.While nZVI is already well known for its site-remediation use,this perspective highlights its application in HMW treatment with metal recovery.We demonstrate several advantages of nZVI in this wastewater application,including its multifunctionality in sequestrating a wide array of metal(loid)s(>30 species);its capability to capture and enrich metal(loid)s at low concentrations(with a removal capacity reaching 500 mg·g^(-1)nZVI);and its operational convenience due to its unique hydrodynamics.All these advantages are attributable to nZVI’s diminutive nanoparticle size and/or its unique iron chemistry.We also present the first engineering practice of this application,which has treated millions of cubic meters of HMW and recovered tons of valuable metals(e.g.,Cu and Au).It is concluded that nZVI is a potent reagent for treating HMW and that nZVI technology provides an eco-solution to this toxic waste. 展开更多
关键词 Nanoscale zero-valent iron WASTEWATER Heavy metal Resource recovery
下载PDF
Role of iron ore in enhancing gasification of iron coke:Structural evolution,influence mechanism and kinetic analysis
2
作者 Jie Wang Wei Wang +4 位作者 Xuheng Chen Junfang Bao Qiuyue Hao Heng Zheng Runsheng Xu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS 2025年第1期58-69,共12页
The utilization of iron coke provides a green pathway for low-carbon ironmaking.To uncover the influence mechanism of iron ore on the behavior and kinetics of iron coke gasification,the effect of iron ore on the micro... The utilization of iron coke provides a green pathway for low-carbon ironmaking.To uncover the influence mechanism of iron ore on the behavior and kinetics of iron coke gasification,the effect of iron ore on the microstructure of iron coke was investigated.Furthermore,a comparative study of the gasification reactions between iron coke and coke was conducted through non-isothermal thermogravimetric method.The findings indicate that compared to coke,iron coke exhibits an augmentation in micropores and specific surface area,and the micropores further extend and interconnect.This provides more adsorption sites for CO_(2) molecules during the gasification process,resulting in a reduction in the initial gasification temperature of iron coke.Accelerating the heating rate in non-isothermal gasification can enhance the reactivity of iron coke.The metallic iron reduced from iron ore is embedded in the carbon matrix,reducing the orderliness of the carbon structure,which is primarily responsible for the heightened reactivity of the carbon atoms.The kinetic study indicates that the random pore model can effectively represent the gasification process of iron coke due to its rich pore structure.Moreover,as the proportion of iron ore increases,the activation energy for the carbon gasification gradually decreases,from 246.2 kJ/mol for coke to 192.5 kJ/mol for iron coke 15wt%. 展开更多
关键词 low-carbon ironmaking iron coke GASIFICATION structural evolution kinetic model
下载PDF
Treatment of simulated wastewater containing Reactive Red 195 by zero-valent iron/activated carbon combined with microwave discharge electrodeless lamp/sodium hypochlorite 被引量:6
3
作者 Jie Fu Zhen Xu +4 位作者 Qing-Shan Li Song Chen Shu-Qing An Qing-Fu Zeng Hai-Liang Zhu 《Journal of Environmental Sciences》 SCIE EI CAS CSCD 2010年第4期512-518,共7页
A comparative study of treatment of simulated wastewater containing Reactive Red 195 using zero-valent iron/activated carbon (ZVI/AC), microwave discharge electrodeless lamp/sodium hypochlorite (MDEL/NaCIO) and th... A comparative study of treatment of simulated wastewater containing Reactive Red 195 using zero-valent iron/activated carbon (ZVI/AC), microwave discharge electrodeless lamp/sodium hypochlorite (MDEL/NaCIO) and the combination of ZVI/AC- MDEL/NaCIO was conducted. The preliminary results showed the two steps method of ZVI/AC-MDEL/NaCIO had much higher degradation efficiency than both single steps. The final color removal percentage was nearly up to 100% and the chemical oxygen demand reduction percentage was up to approximately 82%. The effects of operational parameters, including initial pH value of simulated wastewater, ZVI/AC ratio and particle size of ZVI were also investigated. In addition, from the discussion of synergistic effect between ZVI/AC and MEDL/NaCIO, we found that in the ZVI/AC-MEDL/NaCIO process, ZVI/AC could break the azo bond firstly and then MEDLfNaCIO degraded the aromatic amine products effectively. Reversing the order would reduce the degradation efficiency. 展开更多
关键词 activated carbon microwave discharge electrodeless lamp Reactive Red 195 sodium hypochlorite zero-valent iron.
下载PDF
Synthesis of clay-supported nanoscale zero-valent iron using green tea extract for the removal of phosphorus from aqueous solutions 被引量:6
4
作者 Akbar Soliemanzadeh Majid Fekri 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2017年第7期924-930,共7页
This study addresses the synthesis of nanoscale zero-valent iron(n ZVI) in the presence of natural bentonite(B-n ZVI) using green tea extract. The natural bentonite and B-n ZVI were then applied for the removal of pho... This study addresses the synthesis of nanoscale zero-valent iron(n ZVI) in the presence of natural bentonite(B-n ZVI) using green tea extract. The natural bentonite and B-n ZVI were then applied for the removal of phosphorus from aqueous solutions at various concentrations, p H levels and contact time. The desorption of phosphorus(P) from adsorbents was done immediately after sorption at the maximum initial concentration using the successive dilution method. The characterization of FTIR, SEM, and XRD indicated that n ZVI was successfully loaded to the surface of natural bentonite. The sorption of phosphorus on B-n ZVI was observed to be p H-dependent, with maximum phosphorus removal occurring at the p H range of 2 to 5. The results demonstrate that the maximum sorption capacities of natural bentonite and B-n ZVI were 4.61 and 27.63 mg·g^(-1), respectively.Langmuir, Freundlich, and Redlich–Peterson models properly described the sorption isotherm data. For either adsorbent, desorption isotherms did not coincide with their corresponding sorption isotherms, suggesting the occurrence of irreversibility and hysteresis. The average percentages of retained phosphorus released from natural bentonite and B-n ZVI were 80% and 9%, respectively. The results indicated that sorption kinetics was best described by the pseudo-second-order model. The present study suggests that B-n ZVI could be used as a suitable adsorbent for the removal of phosphorus from aqueous solutions. 展开更多
关键词 Green tea Nano zero-valent iron Natural bentonite PHOSPHORUS SORPTION
下载PDF
Biochar Supported Nanoscale Zero-valent Iron Composites for the Removal of Petroleum from Wastewater 被引量:2
5
作者 Qin Feifei Xu Wenfei +3 位作者 Hao Boyu Yin Linghao Song Jiayu Zhang Xiuxia 《China Petroleum Processing & Petrochemical Technology》 SCIE CAS 2021年第4期47-57,共11页
Considering the need for efficiently and rapidly treating oily wastewater while preventing secondary pollution,the nanoscale zero-valent iron(nZVI)was supported on biochar prepared by using a spent mushroom substrate(... Considering the need for efficiently and rapidly treating oily wastewater while preventing secondary pollution,the nanoscale zero-valent iron(nZVI)was supported on biochar prepared by using a spent mushroom substrate(SMS),to produce an iron-carbon composite(SMS-nZVI).The ability of the SMS-nZVI to treat wastewater containing high concentration of oil was then comprehensively evaluated.The morphology,structure,and other properties of the composite were characterized by using scanning electron microscopy,transmission electron microscopy,the Brunauer-Emmett-Teller nitrogen sorption analysis,and the Fourier transform infrared spectroscopy.The results show that the biochar prepared by using the SMS can effectively prevent the agglomeration of nZVI and increase the overall specific surface area,thereby enhancing the absorption of petroleum by the composite.Experiments reveal that compared with the SMS and nZVI,the SMS-nZVI composite removes petroleum faster and more efficiently from wastewater.Under optimized conditions involving an nZVI to biochar mass ratio of 1:5 and a pH value of 4,the efficiency for removal of petroleum from wastewater with an initial petroleum concentration of 1000 mg/L could reach 95%within 5 h.Based on a natural aging treatment involving exposure to air for 30 d,the SMS-nZVI composite retained an oil removal rate of higher than 62%,and this result could highlight its stability for practical applications. 展开更多
关键词 oily wastewater nanoscale zero-valent iron(nZVI) spent mushroom substrate(SMS) SMS-nZVI composite
下载PDF
Eco friendly adsorbents for removal of phenol from aqueous solution employing nanoparticle zero-valent iron synthesized from modified green tea bio-waste and supported on silty clay 被引量:1
6
作者 Shaimaa T.Kadhum Ghayda Yassen Alkindi Talib M.Albayati 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2021年第8期19-28,共10页
The present research investigated a novel route for the synthesis of nanoparticle zero-valent iron(NZVI)utilizing an aqueous extract of green tea waste as a reductant with ferric chloride.Also,the supported nanopartic... The present research investigated a novel route for the synthesis of nanoparticle zero-valent iron(NZVI)utilizing an aqueous extract of green tea waste as a reductant with ferric chloride.Also,the supported nanoparticle zerovalent iron was synthesized using natural silty clay as a support material(SC-NZVI).The NZVI and SC-NZVI were characterized by infrared spectroscopy(FTIR),scanning electron microscope(SEM),X-ray diffraction(XRD),Brunauer–Emmett–Teller(BET),and zeta potential(ζ).The interpretation of the results demonstrated that the polyphenol and other antioxidants in green tea waste can be used as reduction and capping agents in NZVI synthesis,with silty clay an adequate support.Additionally,the experiments were carried out to explore phenol adsorption by NZVI and SC-NZVI.To determine the optimum conditions,the impact of diverse experimental factors(i.e.,initial pH,adsorbent dose,temperature,and concentration of phenol)was studied.Langmuir,Freundlich,and Tempkin isotherms were used as representatives of adsorption equilibrium.The obtained results indicated that the adsorption processes for both NZVI and SC-NZVI well fitted by the Freundlich isotherm model.The appropriateness of pseudofirstorder and pseudosecondorder kinetics was investigated.The experimental kinetics data were good explained by the second-order model.The thermodynamic parameters(ΔH0,ΔS0,andΔG0)for NZVI and SC-NZVI were determined.The maximum removal rates of phenol at optimum conditions,when adsorbed onto NZVI and SC-NZVI,were found to be 94.8%and 90.1%,respectively. 展开更多
关键词 Wastewater treatment Environment Nano zero-valent iron Silty clay PHENOL Adsorption
下载PDF
Study of diclofenac removal by the application of combined zero-valent iron and calcium peroxide nanoparticles in groundwater 被引量:2
7
作者 Wen Liang Nian-qing Zhou +3 位作者 Chao-meng Dai Yan-ping Duan Lang Zhou Yao-jen Tu 《Journal of Groundwater Science and Engineering》 2021年第3期171-180,共10页
Diclofenac(DCF)is one of the most frequently detected pharmaceuticals in groundwater,posing a great threat to the environment and human health due to its toxicity.To mitigate the DCF contamination,experiments on DCF d... Diclofenac(DCF)is one of the most frequently detected pharmaceuticals in groundwater,posing a great threat to the environment and human health due to its toxicity.To mitigate the DCF contamination,experiments on DCF degradation by the combined process of zero-valent iron nanoparticles(nZVI)and nano calcium peroxide(nCaO_(2))were performed.A batch experiment was conducted to examine the influence of the adding dosages of both nZVI and nCaO_(2)nanoparticles and pH value on the DCF removal.In the meantime,the continuous-flow experiment was done to explore the sustainability of the DCF degradation by jointly adding nZVI/nCaO_(2)nanoparticles in the reaction system.The results show that the nZVI/nCaO_(2)can effectively remove the DCF in the batch test with only 0.05 g/L nZVI and 0.2 g/L nCaO_(2)added,resulting in a removal rate of greater than 90%in a 2-hour reaction with an initial pH of 5.The degradation rate of DCF was positively correlated with the dosage of nCaO_(2),and negatively correlated with both nZVI dosage and the initial pH value.The order of significance of the three factors is identified as pH value>nZVI dosage>nCaO_(2)dosage.In the continuous-flow reaction system,the DCF removal rates remained above 75%within 150 minutes at the pH of 5,with the applied dosages of 0.5 g/L for nZVI and 1.0 g/L for nCaO_(2).These results provide a theoretical basis for the nZVI/nCaO_(2)application to remove DCF in groundwater. 展开更多
关键词 Nanoscale zero-valent iron(nZVI) Nano calcium peroxide(nCaO_(2)) DICLOFENAC Fenton-like reaction Groundwater pollution
下载PDF
Advanced treatment of biologically pretreated coking wastewater by intensified zero-valent iron process(IZVI) combined with anaerobic filter and biological aerated filter(AF/BAF) 被引量:4
8
作者 潘碌亭 韩悦 吴锦峰 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第10期3781-3787,共7页
Experiments were conducted to investigate the behavior of the sequential system of intensified zero-valent iron process(IZVI) and anaerobic filter and biological aerated filter(AF/BAF) reactors for advanced treatment ... Experiments were conducted to investigate the behavior of the sequential system of intensified zero-valent iron process(IZVI) and anaerobic filter and biological aerated filter(AF/BAF) reactors for advanced treatment of biologically pretreated coking wastewater. Particular attention was paid to the performance of the integrated system for the removal of chemical oxygen demand(COD), ammonia nitrogen(NH3-N) and total nitrogen(TN). The average removal efficiencies of COD, NH3-N and TN were 76.28%, 96.76% and 59.97%, with the average effluent mass concentrations of 56, 0.53 and 18.83 mg/L, respectively, reaching the first grade of the national discharge standard. Moreover, the results of gas chromatography/mass spectrum(GC/MS) and gel permeation chromatography(GPC) analysis demonstrated that the refractory organic compounds with high relative molecular mass were partly removed in IZVI process by the function of oxidation-reduction, flocculation and adsorption which could also enhance the biodegradability of the system effluent. The removal efficiencies of NH3-N and TN were achieved mainly in the subsequent AF/BAF reactors by nitrification and denitrification. Overall, the results obtained show that the application of IZVI in combination with AF/BAF is a promising technology for advanced treatment of biologically pretreated coking wastewater. 展开更多
关键词 advanced treatment coking wastewater intensified zero valent iron BIOFILTER
下载PDF
Enhanced degradation of carbon tetrachloride by surfactant-modified zero-valent iron
9
作者 MENG Ya-feng GUAN Bao-hong WU Zhong-biao WANG Da-hui 《Journal of Zhejiang University-Science B(Biomedicine & Biotechnology)》 SCIE CAS CSCD 2006年第9期702-707,共6页
Sorption of carbon tetrachloride (CT) by zero-valent iron (ZVI) is the rate-limiting step in the degradation of CT, so the sorption capacity of ZVl is of great importance. This experiment was aimed at enhancing th... Sorption of carbon tetrachloride (CT) by zero-valent iron (ZVI) is the rate-limiting step in the degradation of CT, so the sorption capacity of ZVl is of great importance. This experiment was aimed at enhancing the sorption of CT by ZVI and the degradation rate of CT by modification of surfactants. This study showed that ZVI modified by cationic surfactants has favorable synergistic effect on the degradation of CT. The CT degradation rate of ZVI modified by cetyl pyridinium bromide (CPB) was higher than that of the unmodified ZVI by 130%, and the CT degradation rate of ZVI modified by cetyl trimethyl ammonium bromide (CTAB) was higher than that of the unmodified ZVI by 81%. This study also showed that the best degradation effect is obtained at the near critical micelle concentrations (CMC) and that high loaded cationic surfactant does not have good synergistic effect on the degradation due to its hydrophilicity and the block in surface reduction sites. Furthermore degradation of CT by ZVI modified by nonionic surfactant has not positive effect on the degradation as the ionic surfactant and the ZVI modified by anionic surfactant has hardly any obvious effects on the degradation. 展开更多
关键词 Enhanced degradation SORPTION SURFACTANTS Synergistic effect zero-valent iron (ZVI)
下载PDF
Assessing the effectiveness of nanoscale zero-valent iron particles produced by green tea for Cr(VI)-contaminated groundwater remediation 被引量:2
10
作者 Hui Li Zhan-tao Han +2 位作者 Qiang Deng Chun-xiao Ma Xiang-ke Kong 《Journal of Groundwater Science and Engineering》 2023年第1期55-67,共13页
Nanoscale zero-valent iron particles(NZVI) produced by using green tea(GT) extract as a reductant can remove Cr(Ⅵ) from water effectively,which can be utilized in groundwater remediation.In order to define the reacti... Nanoscale zero-valent iron particles(NZVI) produced by using green tea(GT) extract as a reductant can remove Cr(Ⅵ) from water effectively,which can be utilized in groundwater remediation.In order to define the reaction mechanism and removal effect in the aquifer,in this study,GT-NZVI particles were prepared and measured by some characterization methods to define their surface performance,and then batch and one-dimensional experiments were carried out to reveal the reaction properties of GT-NZVI and Cr(Ⅵ) in groundwater.The results showed that the prepared GT-NZVI particles were regular spherical with a diameter of 10-20 nm,which could disperse in water stably.The main component of GT-NZVI wasα-Fe with superficial polyphenols as a stabilizer.GT-NZVI suspension had good ability to reduce the Cr(Ⅵ) to Cr(Ⅲ) in water.When the concentration of GT-NZVI was 1 g/L,the removal efficiency of Cr(Ⅵ)with an initial concentration of 100 mg/L reached 92.8% in 1 h reaction.In column tests,GT-NZVI passed through the natural sand column successfully with an average outflow percentage of 71.2%.The simulated in-situ reaction zone(IRZ) with GT-NZVI was used to remediate Cr(Ⅵ) contaminated groundwater.The oufflow concentration of Cr(Ⅵ) kept in 0.14-0.32 mg/L corresponding to the outflow rate below 0.32%within 15 days,and the removal efficiency of Cr(Ⅵ) by IRZ with GT-NZVI decreased with the increase of aquifer medium particle size,groundwater flow rate and ionic strength.Most of Cr(Ⅲ) as reduzate was adsorbed or immobilized on the surface or in the lattice of GT-NZVI,which indicated effective immobilization for chromium. 展开更多
关键词 Nanoscale iron particles Green tea Hexavalent chromium Groundwater remediation
下载PDF
Characterization of the adsorption behavior of aqueous cadmium on nanozero-valent iron based on orthogonal experiment and surface complexation modeling 被引量:2
11
作者 Dongmei Liu Huan Tang +2 位作者 Ying Zhao Fuyi Cui Jing Lu 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2016年第9期1270-1274,共5页
Polyvinylpyrrolidone K-30(PVP) was introduced into the preparation of nanozero-valent iron(n ZVI) and the traditional liquid-phase reduction was improved. The introduction of PVP simplified the traditional method.The ... Polyvinylpyrrolidone K-30(PVP) was introduced into the preparation of nanozero-valent iron(n ZVI) and the traditional liquid-phase reduction was improved. The introduction of PVP simplified the traditional method.The n ZVI prepared with this new approach showed excellent surface characters and high performance on the removal of cadmium. TEM results showed that the aggregates of n ZVI can reach to several micrometers in length but less than 100 nm in diameter. The iron particles that were enclosed by a layer of oxide film that is less than10 nm, demonstrated that the n ZVI possesses a core–shell structure. BET results indicate that the specific surface area of the n ZVI was 20.3159 m^2g^(-1). A three factor and three level orthogonal experiment was employed to find out the dominant factor that affects the removal rate of cadmium by n ZVI. Based on the range values, the prominence order of each factor was: initial p H of the solution N initial concentration of cadmium N dosage of n ZVI, the range was 96.453, 3.294 and 1.747, respectively. A simulation was performed under the same condition and a same conclusion was derived, this consistence confirmed the validity of the conclusion that p H is the most significant factor that affects the adsorption efficiency. 展开更多
关键词 Cadmium Nanozero-valent iron Synthesis Polyvinylpyrrolidone Orthogonal experiment Diffuse layer model
下载PDF
H<sub>2</sub>Gas Charging of Zero-Valent Iron and TCE Degradation
12
作者 Chen Zhao Eric J. Reardon 《Journal of Environmental Protection》 2012年第3期272-279,共8页
Granular zero-valent iron (ZVI) has been widely used to construct permeable reactive barriers (PRB) for the in situ remediation of groundwater contaminated with halogenated hydrocarbons. In the anaerobic condition of ... Granular zero-valent iron (ZVI) has been widely used to construct permeable reactive barriers (PRB) for the in situ remediation of groundwater contaminated with halogenated hydrocarbons. In the anaerobic condition of most groundwater flow systems, iron undergoes corrosion by water and results in hydrogen gas generation. Several studies have shown that some of the hydrogen gas generated at the iron/water interface can diffuse into the iron lattice. Hydrogen gas also can be an electron donor for dechlorination of chlorinated compounds. In this study, the possibility of hydrogen gas bound in the lattice of ZVI playing a role in dehalogenation and improving the degradation efficiency of ZVI was evaluated. Two different granular irons were tested: one obtained from Quebec Metal Powders Ltd (QMP) and the other from Connelly-GPM. Ltd. For each type of iron, two samples were mixed with water and sealed in testing cells. Since the rate of hydrogen entry varies directly with the square root of the hydrogen pressure, one sample was maintained for several weeks under near-vacuum conditions to minimize the amount of hydrogen entering the iron lattice. The other sample was maintained for the same period at a hydrogen pressure of over 400 kPa to maximize the amount of hydrogen entering the iron lattice. The degradation abilities of the reacted ironsand the original iron materials were tested by running several sets of batch tests. The results of this study show little to no improvement of inorganic TCE degradation reactions due to the presence of lattice-stored hydrogen in iron material. This is probably due to the high energiesrequired to release hydrogen trapped in the iron lattice. However, there are certain chemical compounds that can promote hydrogen release from the iron lattice, and there may be bacteria that can utilize lattice-bound hydrogen to carry out dechlorination reactions. 展开更多
关键词 GRANULAR zero-valent iron Hydrogen TCE REMEDIATION GROUNDWATER
下载PDF
Remediation of Nitrate and ChromiumContaminated Groundwater by Zero-valent IronPRB
13
《环境科学前沿(中英文版)》 2015年第2期39-45,共7页
Through continuous flow experimentation, the reactivity characteristics of zero-valent iron (Fe0)-PRB with ground watercontaminated by nitrate, chromium and the combination of nitrate and chromium were investigated.... Through continuous flow experimentation, the reactivity characteristics of zero-valent iron (Fe0)-PRB with ground watercontaminated by nitrate, chromium and the combination of nitrate and chromium were investigated. The results showed thatnitrate could be effectively deoxidized by zero-valent iron. NO^2- -N was the transitional deoxidization product, while NH4+-Nwas the main final product in the effluent. Chromium could be deoxidized by zero-valent iron more effectively for the chromiumcontaminated ground water which was treated by PRB. The redox products such as Fe3+ and Cr(III) precipitated on the packingmedia during the process. For the treatment of ground water contaminated by both nitrate and chromium, the results showed thatthe Cr(VI) removal efficiency by the zero-valent iron was not affected by the co-existence of NO^3- -N, while the NO^3- -N removalefficiency decreased with the existence of Cr(VI). 展开更多
关键词 zero-valent iron PERMEABLE Reactive Barrier(PRB) Ground Water NITRATE CHROMIUM
下载PDF
Revealing the atomic mechanism of diamond–iron interfacial reaction 被引量:1
14
作者 Yalun Ku Kun Xu +6 位作者 Longbin Yan Kuikui Zhang Dongsheng Song Xing Li Shunfang Li Shaobo Cheng Chongxin Shan 《Carbon Energy》 SCIE EI CAS CSCD 2024年第3期255-263,共9页
Diamond,with ultrahigh hardness,high wear resistance,high thermal conductivity,and so forth,has attracted worldwide attention.However,researchers found emergent reactions at the interfaces between diamond and ferrous ... Diamond,with ultrahigh hardness,high wear resistance,high thermal conductivity,and so forth,has attracted worldwide attention.However,researchers found emergent reactions at the interfaces between diamond and ferrous materials,which significantly affects the performance of diamond-based devices.Herein,combing experiments and theoretical calculations,taking diamond–iron(Fe)interface as a prototype,the counter-diffusion mechanism of Fe/carbon atoms has been established.Surprisingly,it is identified that Fe and diamond first form a coherent interface,and then Fe atoms diffuse into diamond and prefer the carbon vacancies sites.Meanwhile,the relaxed carbon atoms diffuse into the Fe lattice,forming Fe_(3)C.Moreover,graphite is observed at the Fe_(3)C surface when Fe_(3)C is over-saturated by carbon atoms.The present findings are expected to offer new insights into the atomic mechanism for diamondferrous material's interfacial reactions,benefiting diamond-based device applications. 展开更多
关键词 coherent interface counter-diffusion DIAMOND iron phase transition
下载PDF
Diffusion and reaction mechanism of limestone and quartz in fluxed iron ore pellet roasting process 被引量:1
15
作者 Yufeng Guo Jinlai Zhang +5 位作者 Shuai Wang Jianjun Fan Haokun Li Feng Chen Kuo Liu Lingzhi Yang 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第3期485-497,共13页
The increase to the proportion of fluxed pellets in the blast furnace burden is a useful way to reduce the carbon emissions in the ironmaking process.In this study,the interaction between calcium carbonate and iron or... The increase to the proportion of fluxed pellets in the blast furnace burden is a useful way to reduce the carbon emissions in the ironmaking process.In this study,the interaction between calcium carbonate and iron ore powder and the mineralization mechanism of fluxed iron ore pellet in the roasting process were investigated through diffusion couple experiments.Scanning electron microscopy with energy dispersive spectroscopy was used to study the elements’diffusion and phase transformation during the roasting process.The results indicated that limestone decomposed into calcium oxide,and magnetite was oxidized to hematite at the early stage of preheating.With the increase in roasting temperature,the diffusion rate of Fe and Ca was obviously accelerated,while the diffusion rate of Si was relatively slow.The order of magnitude of interdiffusion coefficient of Fe_(2)O_(3)-CaO diffusion couple was 10^(−10) m^(2)·s^(−1) at a roasting temperature of 1200℃for 9 h.Ca_(2)Fe_(2)O_(5) was the initial product in the Fe_(2)O_(3)-CaO-SiO_(2) diffusion interface,and then Ca_(2)Fe_(2)O_(5) continued to react with Fe_(2)O_(3) to form CaFe_(2)O_(4).With the expansion of the diffusion region,the sillico-ferrite of calcium liquid phase was produced due to the melting of SiO_(2) into CaFe_(2)O_(4),which can strengthen the consolidation of fluxed pellets.Furthermore,andradite would be formed around a small part of quartz particles,which is also conducive to the consolidation of fluxed pellets.In addition,the principle diagram of limestone and quartz diffusion reaction in the process of fluxed pellet roasting was discussed. 展开更多
关键词 fluxed iron ore pellet LIMESTONE HEMATITE QUARTZ diffusion reaction
下载PDF
Regulatory mechanisms of iron homeostasis in maize mediated by ZmFIT 被引量:1
16
作者 Suzhen Li Shuai Ma +6 位作者 Zizhao Song Yu Li Xiaoqing Liu Wenzhu Yang Tianyu Wang Xiaojin Zhou Rumei Chen 《The Crop Journal》 SCIE CSCD 2024年第5期1426-1436,共11页
Regulation of iron homeostasis in maize remains unclear,despite the known roles of FER-Like Fe deficiency-induced transcription factor(FIT)in Arabidopsis and rice.ZmFIT,like At FIT and Os FIT,interacts with iron-relat... Regulation of iron homeostasis in maize remains unclear,despite the known roles of FER-Like Fe deficiency-induced transcription factor(FIT)in Arabidopsis and rice.ZmFIT,like At FIT and Os FIT,interacts with iron-related transcription factors 2(ZmIRO2).Here,we investigate the involvement of ZmFIT in iron homeostasis.Mutant ZmFIT lines exhibiting symptoms of Fe deficiency had reduced shoot iron content.Transcriptome analysis revealed downregulation of Fe deficiency-responsive genes in the roots of a Zmfit mutant.ZmFIT facilitates the nuclear translocation of ZmIRO2 to activate transcription of downstream genes under Fe-deficient conditions.Our findings suggest that ZmFIT,by interaction with ZmIRO2,mediates iron homeostasis in maize.Notably,the binding and activation mechanisms of ZmFIT resemble those in Arabidopsis but differ from those in rice,whereas downstream genes regulated by ZmFIT show similarities to rice but differences from Arabidopsis.In brief,ZmFIT,orthgologs of Os FIT and At FIT in rice and maize,respectively,regulates iron uptake and homeostasis in maize,but with variations. 展开更多
关键词 iron homeostasis Transcription activation complex Zea mays ZmFIT
下载PDF
Iron and ferritin effects on intensive care unit mortality:A metaanalysis 被引量:1
17
作者 Deng-Can Yang Bo-Jun Zheng +1 位作者 Jian Li Yi Yu 《World Journal of Clinical Cases》 SCIE 2024年第16期2803-2812,共10页
BACKGROUND The effect of serum iron or ferritin parameters on mortality among critically ill patients is not well characterized.AIM To determine the association between serum iron or ferritin parameters and mortality ... BACKGROUND The effect of serum iron or ferritin parameters on mortality among critically ill patients is not well characterized.AIM To determine the association between serum iron or ferritin parameters and mortality among critically ill patients.METHODS Web of Science,Embase,PubMed,and Cochrane Library databases were searched for studies on serum iron or ferritin parameters and mortality among critically ill patients.Two reviewers independently assessed,selected,and abstracted data from studies reporting on serum iron or ferritin parameters and mortality among critically ill patients.Data on serum iron or ferritin levels,mortality,and demographics were extracted.RESULTS Nineteen studies comprising 125490 patients were eligible for inclusion.We observed a slight negative effect of serum ferritin on mortality in the United States population[relative risk(RR)1.002;95%CI:1.002-1.004].In patients with sepsis,serum iron had a significant negative effect on mortality(RR=1.567;95%CI:1.208-1.925).CONCLUSION This systematic review presents evidence of a negative correlation between serum iron levels and mortality among patients with sepsis.Furthermore,it reveals a minor yet adverse impact of serum ferritin on mortality among the United States population. 展开更多
关键词 iron FERRITIN MORTALITY Critically ill Meta analysis
下载PDF
Responses of growth performance,antioxidant function,small intestinal morphology and mRNA expression of jejunal tight junction protein to dietary iron in yellow-feathered broilers 被引量:1
18
作者 Kaiwen Lei Hao Wu +4 位作者 Jerry W Spears Xi Lin Xi Wang Xue Bai Yanling Huang 《Journal of Integrative Agriculture》 SCIE CAS CSCD 2024年第4期1329-1337,共9页
This study aimed to investigate the dose-effect of iron on growth performance,antioxidant function.intestinal morphology,and mRNA expression of jejunal tight junction protein in 1-to21-d-old yellow-feathered broilers.... This study aimed to investigate the dose-effect of iron on growth performance,antioxidant function.intestinal morphology,and mRNA expression of jejunal tight junction protein in 1-to21-d-old yellow-feathered broilers.A total of 7201-d-old yellow-feathered maleb roilers were allocated to 9 treatments with 8 replicate cages of 10 birds per cage.The dietary treatments were consisted of a basal diet(contained 79.6 mg Fe kg^(-1))supplemented with 0,20,40,60,80,160,320,640,and 1,280 mg Fe kg^(-1)in the form of FeSO_(4)·7H_(2)O.Compared with the birds in the control group,birds supplemented with 20mg Fe kg^(-1)had higher average daily gain(ADG)(P<0.0001).Adding 640 and 1,280 mg Fe kg^(-1)significantly decreased ADG(P<0.0001)and average daily feed intake(ADFI)(P<0.0001)compared with supplementation of 20mg Fe kg^(-1).Malondialdehyde(MDA)concentration in plasma and duodenum increased linearly(P<0.0001),but MDA concentration in liver and jejunum increased linearly(P<0.05)or quadratically(P<0.05)with increased dietary Fe concentration.The villus height(VH)in duodenum and jejunum,and the ratio of villus height to crypt depth(V/C)in duodenum decreased linearly(P?0.05)as dietary Feincreased.As dietary Fe increased,the jejunal relative mRNA abundance of claudin-1 decreased linearly(P=0.001),but the jejunal relative mRNA abundance of zona occludens-1(ZO-1)and occludin decreased linearly(P?0.05)or quadratically(P?0.05).Compared with the supplementation of 20 mg Fe kg^(-1),the supplementation of640 mg Fe kg^(-1)or higher increased(P?0.05)MDA concentrations in plasma,duodenum,and jejunum,decreased VH in the duodenum and jejunum,and the addition of 1,280 mg Fe kg^(-1)reduced(P?0.05)the jejunal tight junction protein(claudin-1,ZO-1,occludin)mRNA abundance.In summary,640 mg of supplemental Fe kg^(-1)or greater was associated with decreased growth performance,increased oxidative stress,disrupted intestinal morphology,and reduced mRNA expression of jejunal tight junction protein. 展开更多
关键词 iron yellow-feathered broiler antioxidant function intestinal morphology tight junction protein
下载PDF
Synthesis of nanoscale zero-valent iron supported on exfoliated graphite for removal of nitrate 被引量:10
19
作者 张环 金朝晖 +1 位作者 韩璐 秦承华 《中国有色金属学会会刊:英文版》 CSCD 2006年第B01期345-349,共5页
Nano ZVI particles supported on micro-scale exfoliated graphite were prepared by using KBH4 as reducing agent in the H2O/ethanol system. The supported ZVI materials generally have higher activity and greater flexibili... Nano ZVI particles supported on micro-scale exfoliated graphite were prepared by using KBH4 as reducing agent in the H2O/ethanol system. The supported ZVI materials generally have higher activity and greater flexibility for environmental remediation applications. The exfoliated graphite as the support was treated beforehand to hydrophilic material. Nano iron particles are deposited onto the rough graphite surface while those were formed by borohydride reduction. The possible nitrate reduction pathways were proposed. The TEM image shows that iron particles are highly dispersed on the surface of graphite and several of iron particles are imbedded in the pit of support surface. In this synthesis, iron particles have a nearly spherical shape with a grain size of 50?100 nm. The surface areas of materials with different iron loadings of 3.5%, 7.0%, 10.0%, 15.0% and 20.0%(mass fraction) are 2.89, 9.55, 8.45, 23.8 and 6.18 m2·g?1 by BET surface analyzer. The chemical reduction of nitrate by supported nano ZVI in aqueous solution were tested in series batch experiments. Experiment results suggest that NO3? can be more rapidly reduced to NH4+ at neutral pH and anaerobic conditions by supported nano ZVI than unsupported nano ZVI or ZVI scraps. The 15% nano Fe/graphite shows the best reduction efficiency contrasted with other Fe loading particles. 展开更多
关键词 纳米级0价铁粒子 合成 片状剥落石墨 载体 硝酸盐脱除
下载PDF
Effect of safety valve types on the gas venting behavior and thermal runaway hazard severity of large-format prismatic lithium iron phosphate batteries 被引量:2
20
作者 Zhuangzhuang Jia Yuanyuan Min +5 位作者 Peng Qin Wenxin Mei Xiangdong Meng Kaiqiang Jin Jinhua Sun Qingsong Wang 《Journal of Energy Chemistry》 SCIE EI CAS CSCD 2024年第2期195-207,I0006,共14页
The safety valve is an important component to ensure the safe operation of lithium-ion batteries(LIBs).However,the effect of safety valve type on the thermal runaway(TR)and gas venting behavior of LIBs,as well as the ... The safety valve is an important component to ensure the safe operation of lithium-ion batteries(LIBs).However,the effect of safety valve type on the thermal runaway(TR)and gas venting behavior of LIBs,as well as the TR hazard severity of LIBs,are not known.In this paper,the TR and gas venting behavior of three 100 A h lithium iron phosphate(LFP)batteries with different safety valves are investigated under overheating.Compared to previous studies,the main contribution of this work is in studying and evaluating the effect of gas venting behavior and TR hazard severity of LFP batteries with three safety valve types.Two significant results are obtained:(Ⅰ)the safety valve type dominates over gas venting pressure of battery during safety venting,the maximum gas venting pressure of LFP batteries with a round safety valve is 3320 Pa,which is one order of magnitude higher than other batteries with oval or cavity safety valve;(Ⅱ)the LFP battery with oval safety valve has the lowest TR hazard as shown by the TR hazard assessment model based on gray-fuzzy analytic hierarchy process.This study reveals the effect of safety valve type on TR and gas venting,providing a clear direction for the safety valve design. 展开更多
关键词 Lithium iron phosphate battery Safety valve Thermal runaway Gas venting behavior Thermal runaway hazard severity Gray-fuzzy analytic hierarchy process
下载PDF