钛合金中氢化物析出惯习面的研究 被引量:4
1
作者 施金美 陈业新 万晓景 《上海大学学报(自然科学版)》 CAS CSCD 2003年第5期405-409,共5页
该文用光学显微镜、透射电子显微镜(TEM)观察了α-Ti合金及近α-Ti合金的原始组织及充氢后氢化物形貌,用迹线分析的方法标定了氢化物析出的惯习面.结果表明,Ti-2Al-2.5Zr的惯习面为{1121}或{2021},Ti-4Al-2V的惯习面为{1013}或{1125}.
关键词 α—ti合金 氢化物 迹线分析 惯习面
下载PDF
Effect ofαphase morphology on fatigue crack growth behavior of Ti−5Al−5Mo−5V−1Cr−1Fe alloy 被引量:10
2
作者 Kui-wai CHEN Su-ping PAN +1 位作者 Hui-qun LIU Yong JIANG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2020年第9期2459-2471,共13页
Taking a Ti−5Al−5Mo−5V−1Cr−1Fe alloy as exemplary case,the fatigue crack growth sensitivity and fracture features with various tailoredαphase morphologies were thoroughly investigated using fatigue crack growth rate(... Taking a Ti−5Al−5Mo−5V−1Cr−1Fe alloy as exemplary case,the fatigue crack growth sensitivity and fracture features with various tailoredαphase morphologies were thoroughly investigated using fatigue crack growth rate(FCGR)test,optical microscopy(OM)and scanning electron microscopy(SEM).The tailored microstructures by heat treatments include the fine and coarse secondaryαphase,as well as the widmanstatten and basket weave features.The sample with coarse secondaryαphase exhibits better comprehensive properties of good crack propagation resistance(with long Paris regime ranging from 15 to 60 MPa·m1/2),high yield strength(1113 MPa)and ultimate strength(1150 MPa),and good elongation(11.6%).The good crack propagation resistance can be attributed to crack deflection,long secondary crack,and tortuous crack path induced by coarse secondaryαphase. 展开更多
关键词 ti−5Al−5Mo−5V−1Cr−1Fe alloy αphase fatigue crack growth fracture feature
下载PDF