A new kind of silicon-based biological lubricating base oil with good viscosity-temperature behavior,viscosity index,thermostability,oxidation stability and wear resistance performance was synthesized as a derivative ...A new kind of silicon-based biological lubricating base oil with good viscosity-temperature behavior,viscosity index,thermostability,oxidation stability and wear resistance performance was synthesized as a derivative of methyl oleate.Trimethylsilylation reaction was introduced to further improve methyl oleate oxidation stability and lubricity after epoxidation and open-ring reactions.The order of effectiveness of acid binding agent was N,N-diisopropylethylamine(DIEA) > pyridine > diethylamine > triethylamine,and the effects of various parameters on the trimethylsilylation reaction as well as on the silicon-oxygen bond stability and reaction yield were studied.A maximum yield of 34.54%was achieved at hydroxyl/trimethyl chlorosilane/DIEA molar ratio of1:1.25:1,reaction temperature 40℃,reaction time 1.5 h.展开更多
基金Supported by the National Natural Science Foundation of China(21306088)National Key Technologies R&D Program of China(2015BAD15B07)+1 种基金State Key Laboratory of Chemical Engineering(SKL-Ch E-13A01,Tsinghua University,China)Priority Academic Program Development of Jiangsu Higher Education Institutions(PAPD,China)
文摘A new kind of silicon-based biological lubricating base oil with good viscosity-temperature behavior,viscosity index,thermostability,oxidation stability and wear resistance performance was synthesized as a derivative of methyl oleate.Trimethylsilylation reaction was introduced to further improve methyl oleate oxidation stability and lubricity after epoxidation and open-ring reactions.The order of effectiveness of acid binding agent was N,N-diisopropylethylamine(DIEA) > pyridine > diethylamine > triethylamine,and the effects of various parameters on the trimethylsilylation reaction as well as on the silicon-oxygen bond stability and reaction yield were studied.A maximum yield of 34.54%was achieved at hydroxyl/trimethyl chlorosilane/DIEA molar ratio of1:1.25:1,reaction temperature 40℃,reaction time 1.5 h.