低抗压强度煤体工作面冲击地压危险性修正应力因数评价方法
1
作者 秦帅 刘懿 《采矿技术》 2017年第6期50-54,58,共6页
综合分析讨论了目前国内评价冲击地压危险性时采用的一般方法,在此基础上指出采用单轴抗压强度指标作为主要依据的应力泛定量评价法在评价矿井冲击危险性以及指导现场支护和冲击地压治理方面的优势,针对该方法在评价低抗压强度煤体工作... 综合分析讨论了目前国内评价冲击地压危险性时采用的一般方法,在此基础上指出采用单轴抗压强度指标作为主要依据的应力泛定量评价法在评价矿井冲击危险性以及指导现场支护和冲击地压治理方面的优势,针对该方法在评价低抗压强度煤体工作面时存在的评价结果偏于保守,冲击危险性结论高于真实结果的问题,提出了引入应力修正因数指标对评价结果进行修正。以最新的煤体冲击倾向性鉴定国家标准为理论依据,建立了煤体单轴抗压强度与应力修正因数之间的函数关系式,完善了冲击危险性应力泛定量评价法,构建了可用于低抗压强度煤体矿井的冲击危险性评价方法,扩大了应力泛定量评价法的适用范围。 展开更多
关键词 软煤 低抗压强度 冲击地压 危险性评价 修正应力因数
下载PDF
锦屏一级水电站岩锚梁施工技术 被引量:3
2
作者 董学元 马丰云 《隧道建设》 2011年第2期235-239,245,共6页
为解决高地应力、低抗压强度地质条件下岩锚梁开挖成型困难及岩锚梁混凝土浇筑后出现裂缝等技术难题,结合锦屏一级水电站岩锚梁施工技术,详细介绍了岩锚梁开挖方案、超前支护参数、高强锚杆施工工艺、混凝土浇筑时段及方法等。保证了锦... 为解决高地应力、低抗压强度地质条件下岩锚梁开挖成型困难及岩锚梁混凝土浇筑后出现裂缝等技术难题,结合锦屏一级水电站岩锚梁施工技术,详细介绍了岩锚梁开挖方案、超前支护参数、高强锚杆施工工艺、混凝土浇筑时段及方法等。保证了锦屏一级水电站岩锚梁顺利、优质地完成。 展开更多
关键词 锦屏一级水电站 高地应力 低抗压强度 岩锚梁施工
下载PDF
Analysis of the mechanical property of mudstone/shale in paralic coal measures and its influence factors 被引量:2
3
作者 Zhao-ping MENG Xian-mingXIAN 《Journal of Coal Science & Engineering(China)》 2013年第1期1-7,共7页
The mechanical property of mudstone/shale in coal measures is a key factor of engineering mechanics that influences the development of shale gas. A rock mechanics test was performed in order to analyze the complete st... The mechanical property of mudstone/shale in coal measures is a key factor of engineering mechanics that influences the development of shale gas. A rock mechanics test was performed in order to analyze the complete stress-strain mechanic characteristics and influence factors of mudstone/shale in paralic coal measures, from the Carboniferous-Permian periods in a coal field of Northern China. The relationship between the mechanical properties of mudstone/shale in coal measures, and its chemical component, water content are established, and their models are constructed. Research results show that mud- stone/shale has low mechanical strength, low elastic modulus and a high Poisson's ratio. The complete stress-strain curve has apparent elastoplastic deformation characteristics, and after reaching peak strength, it exhibits obvious strain softening characteristics. The uniaxial compressive strength of mudstone/shale and its elastic modulus increases exponentially with the increase of SiO2 content, and as the ignition loss increases, the uniaxial compressive strength and elastic modulus of mudstone/shale will decrease according to the law of power function. The compressive strength of mudstone/shale and its elastic modulus will decrease with the increase of water content in mudstone/shale. 展开更多
关键词 coal measure mudstone/shale mechanical property influence factors
下载PDF
Hydration and Mechanical Properties of Portland Cement Blended with Low-CaO Steel Slag
4
作者 Eugene Atiemo Kwabena Appiah Boakye James Sarfo-Ansah 《Journal of Physical Science and Application》 2014年第7期444-449,共6页
The hydration and mechanical properties of Portland cement blended with low-CaO steel slag were studied and reported. The steel slag was used to replace cement up to 30% and then blended cement powder, paste and morta... The hydration and mechanical properties of Portland cement blended with low-CaO steel slag were studied and reported. The steel slag was used to replace cement up to 30% and then blended cement powder, paste and mortar samples prepared for the experiment. The quantitative analysis of XRD shows that ettringite formation is greatly reduced by incorporation of steel slag but there was a relatively low reduction of portlandite. Thermal analysis by TG shows that slag injection reduced portlandite content in the cement by at least 50%. Generally, the slag cement pastes required less water to form a workable paste compared to the reference cement, reducing as the slag content was increased. However, the setting times were higher than the reference. The permeability of the blended cement samples were lower than the control. The incorporation of 5% slag could not have an effect on the compressive strength of the concrete. The results confirmed that whilst cements with up to 15% slag content satisfied the strength requirements of class 42.5 N and those containing 20%-30% produce Class 32.5R cement. 展开更多
关键词 HYDRATION cement low-CaO steel slag ETTRINGITE portlandite permeability.
下载PDF
Square concrete columns strengthened with carbon fiber reinforced plastics sheets at low temperatures 被引量:1
5
作者 马芹永 卢小雨 《Journal of Central South University》 SCIE EI CAS 2009年第5期835-840,共6页
Twenty-one square concrete columns were constructed and tested. The testing results indicate that bonded carbon fiber reinforced plastics(CFRP) sheets can be used to increase the strength and improve the serviceabilit... Twenty-one square concrete columns were constructed and tested. The testing results indicate that bonded carbon fiber reinforced plastics(CFRP) sheets can be used to increase the strength and improve the serviceability of damaged concrete columns at low temperatures. The failure of the specimens,in most cases,takes place within the middle half of the columns. And the failure of strengthened columns is sudden and explosive. The CFRP sheets increase both the axial load capacity and the ultimate concrete compressive strain of the columns. The ultimate loads of strengthened columns at-10,0 and 10 ℃ increase averagely by 9.09%,6.63% and 17.83%,respectively,as compared with those of the control specimens. The axial compressive strength of strengthened columns is related to the curing temperatures. The improvement of axial compressive strength decreases with reducing temperature,and when the temperature drops to a certain value,the improvement increases with falling temperature. 展开更多
关键词 carbon fiber reinforced plastics (CFRP) sheet square concrete column stress--strain model