铈锆摩尔比对Ce_(0.3+x)Zr_(0.6-x)Y_(0.1)O_(1.95)系列储氧材料性能的影响 被引量:7
1
作者 毛小波 陈耀强 +3 位作者 钟俊波 王健礼 赵明 龚茂初 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2007年第3期559-561,共3页
A series of materials Ce0.3+xZr0.6-xY0.1O1.95 were prepared by co-precipitation routine and the property of these materials was studied by means of oxygen storage capacity, temperature programming reduction, X-ray dif... A series of materials Ce0.3+xZr0.6-xY0.1O1.95 were prepared by co-precipitation routine and the property of these materials was studied by means of oxygen storage capacity, temperature programming reduction, X-ray diffraction, transmission electronic microscope, and X-ray photoelectron spectroscopy. The results indicate that the materials with a low Ce/Zr molar ratio possess higher cerium atom utilization ratio, reducibility and thermal stability than the materials with a high Ce/Zr ratio, and Ce0.35Zr0.55Y0.1O1.95 possesses the best properties. 展开更多
关键词 材料(osm) 量(OSC) 铈锆比[n(Ce)/n(Zr)] 铈原子利用率
下载PDF
高性能Ce_(0.35)Zr_(0.55)Y_(0.1)O_(1.95)稀土储氧材料的研究 被引量:9
2
作者 毛小波 陈耀强 龚茂初 《无机化学学报》 SCIE CAS CSCD 北大核心 2006年第8期1521-1524,共4页
The oxygen storage material (OSM) Ce0.35Zr0.55Y0.1O1.95 was prepared by co-precipitation routine and studied by means of TEM, XRD, XPS, BET, H2-TPR and oxygen storage capacity (OSC) measurements. The results indicated... The oxygen storage material (OSM) Ce0.35Zr0.55Y0.1O1.95 was prepared by co-precipitation routine and studied by means of TEM, XRD, XPS, BET, H2-TPR and oxygen storage capacity (OSC) measurements. The results indicated that this material possessed plenty of Ce3+ and lattice oxygen vacancy (percentage of Ce3+ was 59.6%) and high cerium atom utilization ratio (80.04%). The porous material was with an average BET surface area of 97 m2·g-1 and pore volume of 0.26 mL·g-1. After aged at 1 000 ℃ in air for 5 h, the sample still possessed plenty of Ce3+ and lattice oxygen vacancy (percentage of Ce3+ was 57.1%), and showed high cerium atom utilization ratio (78.25%), and high thermal stability. 展开更多
关键词 程序升温还原(H2-TPR) 材料(osm) 量(OSC) 铈原子利用率
下载PDF
整体式Pt基催化剂上CH_4选择性催化还原NO的研究 被引量:7
3
作者 房华 蔡黎 +4 位作者 刘萍 赵明 张丽娟 龚茂初 陈耀强 《物理化学学报》 SCIE CAS CSCD 北大核心 2006年第8期1004-1009,共6页
以La-Al2O3(La稳定的!-Al2O3)、Ce0.63Zr0.37O2(OSM1)及Ce0.5Zr0.3Mn0.2O2(OSM2)为载体,Pt为活性组分,制备了Pt质量分数为1%的整体式催化剂.研究了不同载体负载的催化剂对CH4选择催化还原NO反应的性能,并利用XRD、H2-TPR和XPS对催化剂... 以La-Al2O3(La稳定的!-Al2O3)、Ce0.63Zr0.37O2(OSM1)及Ce0.5Zr0.3Mn0.2O2(OSM2)为载体,Pt为活性组分,制备了Pt质量分数为1%的整体式催化剂.研究了不同载体负载的催化剂对CH4选择催化还原NO反应的性能,并利用XRD、H2-TPR和XPS对催化剂进行了表征.结果表明,Pt/OSM1和Pt/OSM2催化剂在氧含量为0.8%时对CH4催化还原NO具有优异的净化性能,Pt/OSM1催化剂上500℃时,CH4和NO均达到100%转化;Pt/OSM2催化剂上500℃时,CH4和NO的转化率分别达到73%和100%;而Pt/La-Al2O3催化剂只在O2含量较低时(0.4%以下)具有较好活性,500℃以上才可使CH4和NO完全转化.H2-TPR结果表明,Pt与OSM1和OSM2存在的相互作用导致低温还原物相生成.Pt与OSM的相互作用及OSM的储氧性能使催化剂在过量氧存在下对CH4催化还原NO具有优异性能. 展开更多
关键词 材料(osm) La-Al2O3 PT 选择性催化还原 整体式催化剂
下载PDF
负载型Pd三效催化剂:载体CeO_2-ZrO_2-BaO的制备及催化性能(英文) 被引量:3
4
作者 蔡黎 陈山虎 +3 位作者 赵明 龚茂初 史忠华 陈耀强 《无机化学学报》 SCIE CAS CSCD 北大核心 2009年第3期474-479,共6页
制备了不同BaO含量的CeO2-ZrO2储氧材料,并以此材料为载体浸渍H2PdCl6制得三效催化剂。结果表明,不论新鲜还是1000℃老化状态下,以10%BaO添加CeO2-ZrO2储氧材料制备的Pd三效催化剂活性最佳,起燃和完全转化温度最低。XPS结果证实,10%BaO... 制备了不同BaO含量的CeO2-ZrO2储氧材料,并以此材料为载体浸渍H2PdCl6制得三效催化剂。结果表明,不论新鲜还是1000℃老化状态下,以10%BaO添加CeO2-ZrO2储氧材料制备的Pd三效催化剂活性最佳,起燃和完全转化温度最低。XPS结果证实,10%BaO添加,通过稳定PdO活性组分并改变其电子环境使得催化剂有最佳活性。而随着BaO含量持续增加,Pd活性组分相对处于较氧化状态。储氧量、低温N2吸附-脱附测试以及XRD测试结果均表明10%BaO添加的材料储氧量,比表面积以及孔容均最大,而且有适应三效催化的孔径。这些结果均有助于以其制备的Pd三效催化剂获得更好的活性以及热稳定性。 展开更多