Failure may occur catastrophically by fracture along grain boundaries when temper embrittlement induced by non-equilibrium grain-boundary segregation (NGS) of phosphorus atoms. Temper embrittlement control technigue b...Failure may occur catastrophically by fracture along grain boundaries when temper embrittlement induced by non-equilibrium grain-boundary segregation (NGS) of phosphorus atoms. Temper embrittlement control technigue based on the theory of NGS and deformation induced phase transformation method was studied in this paper. Grain refinement technique by deformation induced phase transformation in low-alloy steel,12Cr1MoV( which is used in steam pipeline of ships),was experimentally investigated. A single-pass hot rolling process by using a Gleeble-1500 system was performed and the experimental results showed that the grain sizes were obviously affected by the deforming temperature,strain,strain rate and the quenching cooling rate. Temper embrittlement may be controlled and obviously improved by grain refinement.展开更多
In order to reasonably utilize the abundant resources of high-phosphorus iron ore and ilmenite in China, the technology of top-blown smelting reduction with oxygen enrichment was used to smelt the mixed ore of high-ph...In order to reasonably utilize the abundant resources of high-phosphorus iron ore and ilmenite in China, the technology of top-blown smelting reduction with oxygen enrichment was used to smelt the mixed ore of high-phosphorus iron and ilmenite. The effect, which is related to basicity, reduction temperature, carbon-oxygen ratio and time of ventilated oxygen to iron recovery, dephosphorization rate, content of iron, phosphorus, sulfur and titanium in pig iron, was investigated in the experiment. The results show that an ideal outcome can be gained in condition of 6:4 ration on Mengqiao concentrate and Huimin iron ore, temperature of 1 500℃, basicity of 1.3, 1.0 on molar ration of carbon to oxygen, time of 10 min on blowing-oxygen. The outcome is that there is no foamy slag in generation, a good separation of slag and iron, iron recovery with 91.41%, content of phosphorus with 0.27% and tilanium content less than 0.001%, The atmosphere of strong oxidizing in the upper of reduction container and high potential of oxygen in the composition of slag in this technique bring phosphorus, titanium and silicon into slag, which ensures less content of impurity in pig iron.展开更多
文摘Failure may occur catastrophically by fracture along grain boundaries when temper embrittlement induced by non-equilibrium grain-boundary segregation (NGS) of phosphorus atoms. Temper embrittlement control technigue based on the theory of NGS and deformation induced phase transformation method was studied in this paper. Grain refinement technique by deformation induced phase transformation in low-alloy steel,12Cr1MoV( which is used in steam pipeline of ships),was experimentally investigated. A single-pass hot rolling process by using a Gleeble-1500 system was performed and the experimental results showed that the grain sizes were obviously affected by the deforming temperature,strain,strain rate and the quenching cooling rate. Temper embrittlement may be controlled and obviously improved by grain refinement.
基金Project(51064015) supported by the National Natural Science Foundation of ChinaProject(ZD2010001) supported by the Key Project of Yunnan Province Education of China
文摘In order to reasonably utilize the abundant resources of high-phosphorus iron ore and ilmenite in China, the technology of top-blown smelting reduction with oxygen enrichment was used to smelt the mixed ore of high-phosphorus iron and ilmenite. The effect, which is related to basicity, reduction temperature, carbon-oxygen ratio and time of ventilated oxygen to iron recovery, dephosphorization rate, content of iron, phosphorus, sulfur and titanium in pig iron, was investigated in the experiment. The results show that an ideal outcome can be gained in condition of 6:4 ration on Mengqiao concentrate and Huimin iron ore, temperature of 1 500℃, basicity of 1.3, 1.0 on molar ration of carbon to oxygen, time of 10 min on blowing-oxygen. The outcome is that there is no foamy slag in generation, a good separation of slag and iron, iron recovery with 91.41%, content of phosphorus with 0.27% and tilanium content less than 0.001%, The atmosphere of strong oxidizing in the upper of reduction container and high potential of oxygen in the composition of slag in this technique bring phosphorus, titanium and silicon into slag, which ensures less content of impurity in pig iron.