Rheological properties of warm mix asphalt binder by DSR test at medium temperature 被引量:6
1
作者 张久鹏 刘国强 +2 位作者 杜慧 裴建中 马学军 《Journal of Southeast University(English Edition)》 EI CAS 2015年第3期384-388,共5页
The rheological properties including the complex modulus G* and the phase angle δof matrix and warm mix asphalt (WMA)binders were measured by using the dynamic shear rheometer (DSR ) test at the medium temperatu... The rheological properties including the complex modulus G* and the phase angle δof matrix and warm mix asphalt (WMA)binders were measured by using the dynamic shear rheometer (DSR ) test at the medium temperature ranging from 16 to 40 ℃,and the relationships between the fatigue factor G* sinδand the matrix binder property,WMA additive and test temperature were established.It is found that G* decreases with the increasing temperature while δincreases inversely,and G* of the asphalt binder with high WMA additive dosage is large,and δis small.G*sinδexponentially decreases with the increasing temperature and linearly increases with the increase in additive dosage,and the amplitudes of variation are large at low temperatures and high additive dosages.The effect of WMA additive on the rheological property is more remarkable for the matrix asphalt binder with low G*.Besides,aging has a great effect on the property of matrix asphalt binder,and a slight effect on the interaction between asphalt and additive.The high additive dosage can increase the fatigue cracking potential of the asphalt binder. 展开更多
关键词 warm mix asphalt dynamic shear rheometer (DSR test medium temperature rheological property fatigue factor
下载PDF
两类型沥青混合料粗集料微观轨迹分析 被引量:1
2
作者 王可 《公路工程》 北大核心 2016年第3期242-246,共5页
基于数字图像处理(DIP)技术,对AC-13和SMA-13两类型沥青混合料进动态行剪切疲劳性试验,通过对试验前后试件进行CT扫描,并对CT图像进行细观特征参数参数提取,对比分析2类型混合料破坏前后的粗颗粒的运动轨迹。结果表明,破坏后AC-13级配... 基于数字图像处理(DIP)技术,对AC-13和SMA-13两类型沥青混合料进动态行剪切疲劳性试验,通过对试验前后试件进行CT扫描,并对CT图像进行细观特征参数参数提取,对比分析2类型混合料破坏前后的粗颗粒的运动轨迹。结果表明,破坏后AC-13级配混合料粗集料位移量L比SMA-13级配大,AC-13级配粗颗粒位移平动角在所有层位的平均值分布均值波动大于SMA-13级配,各层位粗集料面积均值AC-13级配面积差变化比SMA-13大,面积差较大都是出现在中间层位,AC-13粗集颗粒取向角整体变化差值较SMA-13级配较为明显。 展开更多
关键词 沥青混合料 数字图像处理技术 动态剪切疲劳试验 CT扫描 粗集料运动轨迹
下载PDF