弧形支座支承的含裂纹圆环动态断裂模式的DYNA3D数值分析
1
作者 方竞 姚学锋 《工程力学》 EI CSCD 1996年第A01期1-9,共9页
本文利用DYNA3D大型非线性程序对冲击载荷作用下受刚性弧形支座支承的含裂纹圆环的动态怕裂模式进行了数值模拟分析,表明了冲击过程中含裂纹圆环的几个变形特征,冲击变形,反弹变形,弯曲变形,撕裂破坏,研究位于圆环外表面不... 本文利用DYNA3D大型非线性程序对冲击载荷作用下受刚性弧形支座支承的含裂纹圆环的动态怕裂模式进行了数值模拟分析,表明了冲击过程中含裂纹圆环的几个变形特征,冲击变形,反弹变形,弯曲变形,撕裂破坏,研究位于圆环外表面不同位置裂纹的动态行为对冲击载荷的敏感性以及裂纹敏感区与冲击速度的依赖关系,同时在冲量一定情况下,分析了冲击速度,质量以及支座弧度的变化对裂纹敏感区域的影响。 展开更多
关键词 裂纹敏感区域 动态失效模式 冲击载荷 数值分析
下载PDF
Testing Studies on Rock Failure Modes of Statically Loads Under Dynamic Loading 被引量:4
2
作者 叶洲元 李夕兵 +2 位作者 刘希灵 马春德 尹土兵 《Transactions of Tianjin University》 EI CAS 2008年第B10期530-535,共6页
By means of the improved split Hopkionson pressure bar(SHPB) with axial pre-pressure and confined pressure, two series of experiments on sandstone are carried out to research the failure mode of rock during the course... By means of the improved split Hopkionson pressure bar(SHPB) with axial pre-pressure and confined pressure, two series of experiments on sandstone are carried out to research the failure mode of rock during the course of exploitation of resources in deep. One is under the conditions that the con-fining pressure is fixed and the axial pressure is changeable. The other is under the conditions that the confining pressure becomes and the axial pressure is fixed. It is found that samples break up evenly after impacting when axial static pressures are low, there is great disparity in size of fragments when axial static pressures are high, and the main bodies of samples after the tests under the combination of dy-namic and static loads frequently show the type of V or X. The samples are more close-grained at the elastic stage and impacts make many cracks be generated and developed, as makes samples more crackable. At the initial phase of damage stage, the static pressures make some cracks in the samples which are undeveloped and the impacts′ role is similar to that at the elastic stage. At the metaphase or anaphase of damage stage, these cracks in the samples develop adequately and the impacts mainly accelerate samples′ failure. The main bodies of samples show the type of V or X after impacting due to the confining pressures′ restraining samples′ lateral formation at the elastic stage or the initial phase of damage stage, the main bodies of samples have almost formed at the stage loading static pressures and the results after impacting usually are similar to those under the axial pressures tests. 展开更多
关键词 Hopkinson combination of static and dynamic loads DAMAGE failure mode