铝及铝合金晶粒细化剂变质相形貌的控制 被引量:10
1
作者 钟毅 苏云生 林大超 《昆明理工大学学报(理工版)》 1999年第3期23-27,共5页
介绍熔盐化学反应法生产铝及铝合金晶粒细化剂变质相形貌的控制工艺.通过工艺研究指出,反应温度、时间、搅拌速度、静置温度和时间、加盐的比例、钛的加入量是控制变质相形貌尺寸的关键.优化工艺后获得的块状 Ti Al3 变质相尺... 介绍熔盐化学反应法生产铝及铝合金晶粒细化剂变质相形貌的控制工艺.通过工艺研究指出,反应温度、时间、搅拌速度、静置温度和时间、加盐的比例、钛的加入量是控制变质相形貌尺寸的关键.优化工艺后获得的块状 Ti Al3 变质相尺寸为7 ~125 μm ,较进口的 L S M 公司产品变质相15 ~50 μm 细. 展开更多
关键词 铝合金 晶粒细化剂 组织 变质相形貌
下载PDF
Effect of Sr modification on microstructure and thermal conductivity of hypoeutectic Al−Si alloys 被引量:18
2
作者 Jun-qi GAN Yu-jian HUANG +1 位作者 Cheng WEN Jun DU 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2020年第11期2879-2890,共12页
Trace amount of Sr(0.05 wt.%)was added into the hypoeutectic Al−Si(3−12 wt.%Si)alloys to modify their microstructure and improve thermal conductivity.The results showed that the thermal conductivity of hypoeutectic Al... Trace amount of Sr(0.05 wt.%)was added into the hypoeutectic Al−Si(3−12 wt.%Si)alloys to modify their microstructure and improve thermal conductivity.The results showed that the thermal conductivity of hypoeutectic Al−Si alloys was improved by Sr modification,and the increment and increasing rate of the thermal conductivity gradually increased with Si content increasing.The improvement of thermal conductivity was primarily related to the morphology variation of eutectic Si phases.In Sr-modified Al−Si alloys,the morphology of eutectic Si phases was a mixed morphology of fiber structure and fine flaky structure,and the proportion of the fine flaky eutectic Si phases gradually decreased with Si content increasing.Under the Si content reaching 9 wt.%,the proportion of fine flaky eutectic Si phases was nearly negligible in Sr-modified alloys.Correspondingly,the increment and increasing rate of thermal conductivity of Sr-modified alloys reached the maximum and tended to be stable. 展开更多
关键词 hypoeutectic Al−Si alloy Sr modification eutectic Si morphology thermal conductivity Al/Si interface
下载PDF