The microstructure evolution and strengthening mechanisms of Mg-10Gd-1Er-1Zn-0.6Zr(wt.%) alloy were focused in the view of the size parameters and volume fraction(fp) of dual phases(long period stacking ordered(LPSO) ...The microstructure evolution and strengthening mechanisms of Mg-10Gd-1Er-1Zn-0.6Zr(wt.%) alloy were focused in the view of the size parameters and volume fraction(fp) of dual phases(long period stacking ordered(LPSO) structures and β’ precipitates).Results show that two types of LPSO phases with different morphologies formed,and the morphology and size of both LPSO phases varied with the solution conditions.However,the volume fraction decreased monotonously with increasing solution temperature,which in turn raised the volume fraction of β’ phase during aging.The alloy exhibited an ultimate tensile strength of 352 MPa,a yield strength of 271 MPa,and an elongation of 3.5% after solution treatment at 500℃ for 12 h and aging at 200℃ for 114 h.In contrast to the LPSO phase,the β’ phase seems to play a more important role in enhancing the yield strength,and consequently,a decreased fLPSO/fβ’,ratio results in an increased yield strength.展开更多
基金Project(2016YFB0301101)supported by the National Key Research and Development Program of ChinaProject(Z161100002116033)supported by Beijing Municipal Science and Technology Commission,China+1 种基金Project(KZ201810005005)supported by Key Science and Technology Program of Beijing Municipal Commission of Education,ChinaProject(2172013)supported by Beijing Natural Science Foundation,China
文摘The microstructure evolution and strengthening mechanisms of Mg-10Gd-1Er-1Zn-0.6Zr(wt.%) alloy were focused in the view of the size parameters and volume fraction(fp) of dual phases(long period stacking ordered(LPSO) structures and β’ precipitates).Results show that two types of LPSO phases with different morphologies formed,and the morphology and size of both LPSO phases varied with the solution conditions.However,the volume fraction decreased monotonously with increasing solution temperature,which in turn raised the volume fraction of β’ phase during aging.The alloy exhibited an ultimate tensile strength of 352 MPa,a yield strength of 271 MPa,and an elongation of 3.5% after solution treatment at 500℃ for 12 h and aging at 200℃ for 114 h.In contrast to the LPSO phase,the β’ phase seems to play a more important role in enhancing the yield strength,and consequently,a decreased fLPSO/fβ’,ratio results in an increased yield strength.