DOP工业废弃活性炭中回收DOP及废炭再生生产试验 被引量:1
1
作者 龚建平 王灵 《林产化工通讯》 CAS 北大核心 1995年第5期16-17,共2页
本文提出了从DOP废弃活性炭中回收DOP并对废炭进行再生的新工艺。用很低的成本从废炭中可回收30~40%的DOP,并再生得50~60%的活性炭,有着较好的经济收益。
关键词 萃取剂 活性 废炭再生
下载PDF
Recycling of waste carbon residue from spent lithium-ion batteries via constant-pressure acid leaching 被引量:3
2
作者 Xiang-dong ZHU Jin XIAO +3 位作者 Qiu-yun MAO Zhen-hua ZHANG Lei TANG Qi-fan ZHONG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2022年第5期1691-1704,共14页
Waste carbon residue(WCR)was efficiently detoxicated and regenerated to high-purity graphite(PGC)used in lithium-ion batteries through the constant-pressure acid leaching technique.The leaching conditions were optimiz... Waste carbon residue(WCR)was efficiently detoxicated and regenerated to high-purity graphite(PGC)used in lithium-ion batteries through the constant-pressure acid leaching technique.The leaching conditions were optimized by the combination of orthogonal and single-factor experiments.Results show that PGC with 99.5%purity is regenerated at temperature of 60℃,initial acid concentration of 12%,leaching time of 180 min,and liquid-to-solid ratio of 25:1,satisfying the requirements of commercial graphite.Meanwhile,the sodium hydroxide precipitation process was designed to recover valuable components from leachate efficiently.Ni,Co,Mn,and Al recoveries reach 96.92%,87.5%,97.83%,and 92.17%,respectively,at pH=11.Moreover,the co-product NaF can be recovered with purity over 99%via evaporative crystallization.The loss rate of fluorine is less than 0.5%,thereby eliminating the pollution risk of fluorine to the environment.The proposed process shows considerable environmental and economic benefits. 展开更多
关键词 constant-pressure acid leaching waste carbon residue anode material regeneration sodium hydroxide precipitation NAF