This research is showing the effect of increasing an Fe extracting from the compression strength, tension and bending moment. The variations in this experiment are the increasing of Fe extracting 0.5%, 1% and 1.5% of ...This research is showing the effect of increasing an Fe extracting from the compression strength, tension and bending moment. The variations in this experiment are the increasing of Fe extracting 0.5%, 1% and 1.5% of concrete volume. Water Cement Ratio (WCR) variation of 0.48, 0.56 and 0.60. The result of increasing 1.5% Fe extracting causes the increasing of tension strength 44.028 kN/cm2, the increasing of slit tension strength 2.226 kN/cm2, the increasing of bending moment 14.81 kN/cm2 from normal concrete. 0.48 WCR produces tension strength, slit tension strength and bending moment more than 0.56 and 0.60 WCR. The increasing of Fe extracting with the distribution variation area and the spread concrete in the tension concrete area produce 3.705 kN/cm2 bending moment higher than the spread fiber in all of concrete area. The 4 cm fiber length produces the higher bending moment than the 2 cm fiber length. The difference is equally 5.185 kN/cm2. The combination result of the examined acting varieties by continuation statistic test gives the result to get the maximum tension and split tensile. It is a concrete combination of increasing 1.5% fiber percentage, 0.48 WCR, full spreading area and the 4 cm fiber length. The maximum bending moment is the increasing of 0.5% fiber percentage, 0.48 WCR, full spreading area and the 4 cm fiber length.展开更多
文摘This research is showing the effect of increasing an Fe extracting from the compression strength, tension and bending moment. The variations in this experiment are the increasing of Fe extracting 0.5%, 1% and 1.5% of concrete volume. Water Cement Ratio (WCR) variation of 0.48, 0.56 and 0.60. The result of increasing 1.5% Fe extracting causes the increasing of tension strength 44.028 kN/cm2, the increasing of slit tension strength 2.226 kN/cm2, the increasing of bending moment 14.81 kN/cm2 from normal concrete. 0.48 WCR produces tension strength, slit tension strength and bending moment more than 0.56 and 0.60 WCR. The increasing of Fe extracting with the distribution variation area and the spread concrete in the tension concrete area produce 3.705 kN/cm2 bending moment higher than the spread fiber in all of concrete area. The 4 cm fiber length produces the higher bending moment than the 2 cm fiber length. The difference is equally 5.185 kN/cm2. The combination result of the examined acting varieties by continuation statistic test gives the result to get the maximum tension and split tensile. It is a concrete combination of increasing 1.5% fiber percentage, 0.48 WCR, full spreading area and the 4 cm fiber length. The maximum bending moment is the increasing of 0.5% fiber percentage, 0.48 WCR, full spreading area and the 4 cm fiber length.