冲击作用下斜接修补CFRP层间分层和胶层的损伤机制及参数分析 被引量:2
1
作者 冯威 徐绯 《复合材料学报》 EI CAS CSCD 北大核心 2018年第4期1024-1031,共8页
首先,针对斜接修补CFRP抗冲击性能差的问题,分别使用基于接触的内聚力模型(SCZM)和基于单元的内聚力模型(ECZM)描述层间分层和斜接胶层破坏,研究CFRP层板的冲击响应和两种失效的演化规律。然后,分析了冲击能量、斜接角度和预拉伸作用对... 首先,针对斜接修补CFRP抗冲击性能差的问题,分别使用基于接触的内聚力模型(SCZM)和基于单元的内聚力模型(ECZM)描述层间分层和斜接胶层破坏,研究CFRP层板的冲击响应和两种失效的演化规律。然后,分析了冲击能量、斜接角度和预拉伸作用对两种失效的影响。结果表明:层间分层起始时间早于胶层破坏,与冲击能量无关;分层和胶层破坏面积随冲击能量增加而增大,胶层破坏面积增加的更明显;斜接角度主要影响胶层破坏,对分层面积几乎无影响;预拉伸作用对两种失效均具有负面作用。最后,进一步讨论分层对胶层破坏的影响,通过与只考虑胶层破坏的情况进行对比,发现层间分层使胶层破坏的面积降低,延缓了胶层的最终失效。 展开更多
关键词 修补 分层 胶层破坏 斜接角度 预拉伸
原文传递
Effect of tool tilt angle on strength and microstructural characteristics of friction stir welded lap joints of AA2014-T6 aluminum alloy 被引量:3
2
作者 C.RAJENDRAN K.SRINIVASAN +2 位作者 V.BALASUBRAMANIAN H.BALAJI P.SELVARAJ 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2019年第9期1824-1835,共12页
Friction stir welding(FSW)has been extensively adopted to fabricate aluminium alloy joints by incorporating various welding parameters that include welding speed,rotational speed,diameters of shoulder and pin and tool... Friction stir welding(FSW)has been extensively adopted to fabricate aluminium alloy joints by incorporating various welding parameters that include welding speed,rotational speed,diameters of shoulder and pin and tool tilt angle.FSW parameters significantly affect the weld strength.Tool tilt angle is one of the significant process parameters among the weld parameters.The present study focused on the effect of tool tilt angle on strength of friction stir lap welding of AA2014-T6 aluminium alloy.The tool tilt angle was varied between 0°and 4°with an equal increment of 1°.Other process parameters were kept constant.Macrostructure and microstructure analysis,microhardness measurement,scanning electron micrograph,transmission electron micrograph and energy dispersive spectroscopy analysis were performed to evaluate the lap shear strength of friction stir lap welded joint.Results proved that,defect-free weld joint was obtained while using a tool tilt angle of 1°to 3°.However,sound joints were welded using a tool tilt angle of 2°,which had the maximum lap shear strength of 14.42 kN and microhardness of HV 132.The joints welded using tool tilt angles of 1°and 3°yielded inferior lap shear strength due to unbalanced material flow in the weld region during FSW. 展开更多
关键词 AA2014 aluminium alloy friction stir lap welding tool tilt angle lap shear strength microstructure