High-efficiency recovery of Zn and Pb from silicon-rich zinc leaching residues is realized in a rotary kiln.Characterizations by means of XRD,SEM,EDS and ICP reveal that the leaching residue contains 12.4 wt.%SiO_(2),...High-efficiency recovery of Zn and Pb from silicon-rich zinc leaching residues is realized in a rotary kiln.Characterizations by means of XRD,SEM,EDS and ICP reveal that the leaching residue contains 12.4 wt.%SiO_(2),16.1 wt.%Zn,and 7.4 wt.%Pb.Thermodynamic analysis shows that metallic vapor of Zn and Pb can be easily generated from the zinc leaching residue at 1150-1250°C inside the rotary kiln.Viscosities and melting points of 13 slag compositions were analyzed and three slag compositions(47wt.%SiO_(2)-23wt.%CaO-30wt.%FeO,40wt.%SiO_(2)-28wt.%CaO-32wt.%FeO,and 40wt.%SiO_(2)-30wt.%CaO-30wt.%FeO)possessed the desirable physical properties,with the melting point and viscosity in the range of 1150-1280°C and 0.2-0.5 Pa·s,respectively.The industrial tests show that adopting the optimized slag composition can contribute to very high recovery rates of Zn and Pb(97.3%for Zn and 94.5%for Pb),corresponding to slags with very low average contents of Zn and Pb(0.51 wt.%Zn and 0.45 wt.%Pb).The National-Standard leaching tests of the water-quenched slags result in 1.82 mg/L Zn,~0.01 mg/L Cu,0.0004 mg/L As,~0.01 mg/L Cd,0.08 mg/L Pb,and~0.02 mg/L Hg in the leachate,verifying the detoxification of the zinc leaching residue at the same time.展开更多
In order to solve transport problems of industry solid,firstly,a new applicationnotion of pipeline transport was presented,that is to say,combining pretreatment andtransport with disposal techniques of industry solid ...In order to solve transport problems of industry solid,firstly,a new applicationnotion of pipeline transport was presented,that is to say,combining pretreatment andtransport with disposal techniques of industry solid waste.Secondly,the integrated dis-posal and transport system for industry solid waste was introduced,in particular,the oper-ating principles,equipment set-up,key technology and technical parameters.Next,thispaper illustrated the application of this integrated system.Such as it can transport coalsludge with sufficiently high solids content(about 72%~77%)and high apparent viscosity(about 1 000~3 000 Pa.s)directly by pipeline having no use for water and addition agent.Generally,the transport distance is about 1 000 m.This system has been successfullyused in innocuous disposition and efficient utilization of other industrial byproducts or solidwastes,such as city sludge and paper making waste.The integrated system causes nopollution to the environment for its complete seal and realizes protecting the environment,conserving the energy,promoting the development of cycling economic.Finally,the paperdiscussed the research works that were needed for studying such pipeline transport sys-tem and narrates the relevant condition and application status.展开更多
基金the funding support from the National Natural Science Foundation of China (Nos. 51804221, 51874101)the National Key R&D Program of China (No. 2019YFF0217102)the China Postdoctoral Science Foundation (Nos. 2018M642906, 2019T120684)
文摘High-efficiency recovery of Zn and Pb from silicon-rich zinc leaching residues is realized in a rotary kiln.Characterizations by means of XRD,SEM,EDS and ICP reveal that the leaching residue contains 12.4 wt.%SiO_(2),16.1 wt.%Zn,and 7.4 wt.%Pb.Thermodynamic analysis shows that metallic vapor of Zn and Pb can be easily generated from the zinc leaching residue at 1150-1250°C inside the rotary kiln.Viscosities and melting points of 13 slag compositions were analyzed and three slag compositions(47wt.%SiO_(2)-23wt.%CaO-30wt.%FeO,40wt.%SiO_(2)-28wt.%CaO-32wt.%FeO,and 40wt.%SiO_(2)-30wt.%CaO-30wt.%FeO)possessed the desirable physical properties,with the melting point and viscosity in the range of 1150-1280°C and 0.2-0.5 Pa·s,respectively.The industrial tests show that adopting the optimized slag composition can contribute to very high recovery rates of Zn and Pb(97.3%for Zn and 94.5%for Pb),corresponding to slags with very low average contents of Zn and Pb(0.51 wt.%Zn and 0.45 wt.%Pb).The National-Standard leaching tests of the water-quenched slags result in 1.82 mg/L Zn,~0.01 mg/L Cu,0.0004 mg/L As,~0.01 mg/L Cd,0.08 mg/L Pb,and~0.02 mg/L Hg in the leachate,verifying the detoxification of the zinc leaching residue at the same time.
基金Science and Technology Corporation Innovation Fund of China(02C26211100499) PH.D Program Fund(20020290011)
文摘In order to solve transport problems of industry solid,firstly,a new applicationnotion of pipeline transport was presented,that is to say,combining pretreatment andtransport with disposal techniques of industry solid waste.Secondly,the integrated dis-posal and transport system for industry solid waste was introduced,in particular,the oper-ating principles,equipment set-up,key technology and technical parameters.Next,thispaper illustrated the application of this integrated system.Such as it can transport coalsludge with sufficiently high solids content(about 72%~77%)and high apparent viscosity(about 1 000~3 000 Pa.s)directly by pipeline having no use for water and addition agent.Generally,the transport distance is about 1 000 m.This system has been successfullyused in innocuous disposition and efficient utilization of other industrial byproducts or solidwastes,such as city sludge and paper making waste.The integrated system causes nopollution to the environment for its complete seal and realizes protecting the environment,conserving the energy,promoting the development of cycling economic.Finally,the paperdiscussed the research works that were needed for studying such pipeline transport sys-tem and narrates the relevant condition and application status.