期刊文献+
共找到3篇文章
< 1 >
每页显示 20 50 100
曲母线形件旋压成形的数值模拟
1
作者 孟艳梅 《黑龙江科技信息》 2008年第35期69-69,357,共2页
针对曲母线形件的旋压成形工艺,利用大型有限元分析软件ANSYS建立了曲母线形件的数值模型,并模拟了旋压方法加工曲母线形件的工艺过程,最后给出了模拟结果,表明用旋压方法成形是可行的。
关键词 有限元 曲母线形件 旋压 数值模拟
下载PDF
60Si2Mn钢曲母线形件强力热旋压成形技术研究 被引量:1
2
作者 徐恒秋 张锐 +4 位作者 王大力 黄涛 郭丽 郑宏伟 高武林 《新技术新工艺》 2014年第3期14-16,共3页
针对60Si2Mn钢曲母线形件材料利用率低的问题,研究了该类工件的成形工艺。采用旋压工艺替代切削工艺,直接成形曲母线形件,能够提高原材料的利用率,并获得良好的组织性能。分析了高碳钢热旋压工艺难点,开展了旋压试验研究,确定了加热强... 针对60Si2Mn钢曲母线形件材料利用率低的问题,研究了该类工件的成形工艺。采用旋压工艺替代切削工艺,直接成形曲母线形件,能够提高原材料的利用率,并获得良好的组织性能。分析了高碳钢热旋压工艺难点,开展了旋压试验研究,确定了加热强力旋压的工艺方案,试验分析了旋压温度、变形量和上下料时间等工艺参数,掌握了旋压规律,并旋压出了合格产品。对旋压样件进行了性能及金相分析,试验结果达到了产品设计要求,材料利用率由50%提高到了70%。 展开更多
关键词 60SI2MN钢 热旋 错距 曲母线形件
下载PDF
Finite element simulation and microstructure of two-pass inner spinning process of curved-generatrix cone cylindrical parts with annealing/quenching 被引量:2
3
作者 HAO Zeng-liang YANG Zhe-yi) +3 位作者 WEI Wei LIU Lei LUO Jun-ting LIU Jin-heng 《Journal of Central South University》 SCIE EI CAS CSCD 2019年第12期3305-3314,共10页
A two-pass annealing/quenching internal spinning process with small-end rotations is proposed to form a curved generatrix conical thin-walled shell.That is,annealing at 360°C for 2 h followed by the 1st pass spin... A two-pass annealing/quenching internal spinning process with small-end rotations is proposed to form a curved generatrix conical thin-walled shell.That is,annealing at 360°C for 2 h followed by the 1st pass spinning,and finally quenching in ice water after holding for 1 h at 498°C followed by the 2nd pass spinning.ABAQUS finite element software is used to simulate the internal spinning process of the products formed under different forming parameters.The distribution laws of spinning force,the stress and strain under different forming processes were compared and analyzed.The mechanical properties and microstructure of the products are subsequently analyzed.The results show that the strain and the residual stress in the skin area of the formed products under two-pass spinning process more uniform,and the hardness and the mechanical performance are improved.The microstructure of the products formed with the 0.15 mm thickness reduction at the 2nd pass is excellent.And the second phase grain size distributed uniformly in the range of 36μm.Whereas,the second phase particles are broken seriously and the size distribution inhomogeneity is increased when the thickness reduction in the skin area is greater than 0.20 mm at the 2nd pass spinning process. 展开更多
关键词 curved generatrix conical internal spinning process annealing/quenching small-end rotations finite element simulation
下载PDF