单一分散氧化铁-葡聚糖纳米粒子的制备及超顺磁性 被引量:12
1
作者 杨玉东 梁勇 《无机化学学报》 SCIE CAS CSCD 北大核心 2005年第1期133-136,共4页
Monodispersed Fe3O4-Dextran nano-particles were prepared by chemical co-deposition with average diameter of 16 nm, and a core of diameter of 5.5 nm f or Fe3O4 with a shell of thickness 5 nm for Dextran. The results of... Monodispersed Fe3O4-Dextran nano-particles were prepared by chemical co-deposition with average diameter of 16 nm, and a core of diameter of 5.5 nm f or Fe3O4 with a shell of thickness 5 nm for Dextran. The results of magnetic pro perty determination show that: they have a good magnetization of 76 emu·g-1 whi ch is increased by a factor of 49%. As compared with 51 emu·g-1 for the materia l obtained without the addition of coordination compound in the processing. 展开更多
关键词 氧化铁-葡聚糖 单分散 配体 超顺磁性
下载PDF
葡聚糖中超顺磁氧化铁复合纳米粒子制备影响因素及表征 被引量:4
2
作者 杨玉东 梁勇 +1 位作者 宋志霞 线全刚 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2005年第1期225-229,共5页
利用化学共沉积法在改性葡聚糖体系下制备了以超顺磁性纳米氧化铁为核心,外包葡聚糖的壳核结构复合粒子.对制备过程控制因素进行了详细的研究,实验结果表明:利用改性葡聚糖为表面活性剂,碱源快速滴加,合理的控制反应时间,温度可形成小... 利用化学共沉积法在改性葡聚糖体系下制备了以超顺磁性纳米氧化铁为核心,外包葡聚糖的壳核结构复合粒子.对制备过程控制因素进行了详细的研究,实验结果表明:利用改性葡聚糖为表面活性剂,碱源快速滴加,合理的控制反应时间,温度可形成小核的超顺磁性纳米氧化铁-葡聚糖复合纳米粒子.在优化的实验条件下,得到核心的平均粒径5nm,总体的平均粒径为7.8nm,并利用XRD、TEM和GLS等手段对其结构,形态和粒径分布进行了表征. 展开更多
关键词 超顺磁氧化铁-葡聚糖复合纳米粒子 制备 表征