A novel treatment process of lead anode slime bearing high antimony and low silver was developed by a potential-controlled chloridization leaching and continuous distillation.The experimental results show a high Sb 3+...A novel treatment process of lead anode slime bearing high antimony and low silver was developed by a potential-controlled chloridization leaching and continuous distillation.The experimental results show a high Sb 3+ concentration,489.2 g/L,in the leaching solution for two-stage countercurrent leaching process,and the leaching rates of Sb,Cu,Bi more than 99% when the potential is controlled at 450 mV.When the leaching solution is distillated and concentrated at 120°C,almost all the silicon compound is evaporated into the concentration distillate and exists as amorphous hydrated silica.By the continuous distillation,high pure SbCl3 could be prepared,and AsCl3 is enriched in the distillate while metals Bi,Cu are enriched in the continuous distillation residue.As a result,the recovery rate of Sb is more than 95%.展开更多
基金Project(2006BAB02B04-4-1)supported by the National Science and Technology Pillar Program during the 11th Five-Year Plan Period,China
文摘A novel treatment process of lead anode slime bearing high antimony and low silver was developed by a potential-controlled chloridization leaching and continuous distillation.The experimental results show a high Sb 3+ concentration,489.2 g/L,in the leaching solution for two-stage countercurrent leaching process,and the leaching rates of Sb,Cu,Bi more than 99% when the potential is controlled at 450 mV.When the leaching solution is distillated and concentrated at 120°C,almost all the silicon compound is evaporated into the concentration distillate and exists as amorphous hydrated silica.By the continuous distillation,high pure SbCl3 could be prepared,and AsCl3 is enriched in the distillate while metals Bi,Cu are enriched in the continuous distillation residue.As a result,the recovery rate of Sb is more than 95%.