环境化学因素对地基土的长期作用会影响地基土的物理、力学特性。近年来酸性水环境对地基土工程性质的影响受到了工程界的关注。基于试样在常规三轴剪切试验条件下的应力—应变曲线特点,提出了一个可以综合考虑酸性水化学溶蚀效应—荷... 环境化学因素对地基土的长期作用会影响地基土的物理、力学特性。近年来酸性水环境对地基土工程性质的影响受到了工程界的关注。基于试样在常规三轴剪切试验条件下的应力—应变曲线特点,提出了一个可以综合考虑酸性水化学溶蚀效应—荷载损伤效应的非耦合本构模型。模型参数η、α、b为初始损伤参数,主要反映水化学溶蚀效果;模型参数m为反映荷载效应的损伤参数。将采用模型预测的曲线与试验结果曲线进行对比,发现二者趋势基本吻合,表明该模型较客观地反映了酸性水化学环境下花岗岩残积土试样在不同围压条件下的应力—应变关系。 展开更多
关键词 花岗岩残积土 酸性水环境 结构性 水化学溶蚀 损伤参数
下载PDF
Influence of welding speed on corrosion behaviour of friction stir welded AA5086 aluminium alloy 被引量:5
2
作者 Kamran Amini Farhad Gharavi 《Journal of Central South University》 SCIE EI CAS CSCD 2016年第6期1301-1311,共11页
The plates of AA5086 aluminium alloy were joined together by friction stir welding at a fixed rotation speed of 1000 r/min various welding speeds ranging from 63 to 100 mm/min.Corrosion behavior of the parent alloy(PA... The plates of AA5086 aluminium alloy were joined together by friction stir welding at a fixed rotation speed of 1000 r/min various welding speeds ranging from 63 to 100 mm/min.Corrosion behavior of the parent alloy(PA),the heat affected zone(HAZ),and the weld nugget zone(WNZ)of the joints were studied in 3.5%(mass fraction)aerated aqueous Na Cl solution by potentiodynamic polarization and electrochemical impedance spectroscopy(EIS).The corrosion susceptibility of the weldments increases when the welding speed increases to 63 and 100 mm/min.However,the value of corrosion rate in the weldments is lower than that in the PA.Additionally,the corrosion current density increases with increasing the welding speed in the HAZ and the WNZ.On the contrary,the corrosion potential in the WNZ appears more positive than in the HAZ with decreasing the welding speed.The WNZ exhibits higher resistance compared to the HAZ and the PA as the welding speed decreases.The results obtained from the EIS measurements suggest that the weld regions have higher corrosion resistance than the parent alloy.With increasing the welding speed,the distribution and extent of the corroded areas in the WNZ region are lower than those of the HAZ region.In the HAZ region,in addition to the pits in the corroded area,some cracks can be seen around the corroded areas,which confirms that intergranular corrosion is formed in this area.The alkaline localized corrosion and the pitting corrosion are the main corrosion mechanisms in the corroded areas within the weld regions.Crystallographic pits are observed within the weld regions. 展开更多
关键词 friction stir welding aluminum alloy corrosion properties welding speed