In this paper a critical review is presented of the history and current state of the art of J-integral resistance curve testing and experimental evaluation methods in conjunction with a discussion of the development o...In this paper a critical review is presented of the history and current state of the art of J-integral resistance curve testing and experimental evaluation methods in conjunction with a discussion of the development of the plane strain fracture toughness test standard ASTM E1820 developed by American Society for Testing and Materials (ASTM). Early research efforts on this topic are reviewed first. These include the J-integral concept, experimental estimates of the J-integral for stationary cracks, load line displacement (LLD) and crack mouth opening displacement (CMOD) based η factor equations, different formulations of J-integral incremental equations for growing cracks, crack growth corrected J-R curve determination, and experimental test methods. Recent developments in J-R curve testing and evaluation are then described, with emphasis on accurate J-integral incremental equations, a normalization method, a modified basic method, a CMOD direct method with use of incremental equations, relationships of plastic geometry factors, constraint-dependent J-R curve testing and correction approaches. An overview of the present fracture toughness test standard ASTM E1820-08a is then presented. The review shows that after more than 40 years of investigation and development, the J-integral resistance curve test methods in ASTM E1820 have become simpler, more cost-effective and more accurate.展开更多
文摘In this paper a critical review is presented of the history and current state of the art of J-integral resistance curve testing and experimental evaluation methods in conjunction with a discussion of the development of the plane strain fracture toughness test standard ASTM E1820 developed by American Society for Testing and Materials (ASTM). Early research efforts on this topic are reviewed first. These include the J-integral concept, experimental estimates of the J-integral for stationary cracks, load line displacement (LLD) and crack mouth opening displacement (CMOD) based η factor equations, different formulations of J-integral incremental equations for growing cracks, crack growth corrected J-R curve determination, and experimental test methods. Recent developments in J-R curve testing and evaluation are then described, with emphasis on accurate J-integral incremental equations, a normalization method, a modified basic method, a CMOD direct method with use of incremental equations, relationships of plastic geometry factors, constraint-dependent J-R curve testing and correction approaches. An overview of the present fracture toughness test standard ASTM E1820-08a is then presented. The review shows that after more than 40 years of investigation and development, the J-integral resistance curve test methods in ASTM E1820 have become simpler, more cost-effective and more accurate.