期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
某浮磷尾矿综合回收钛铁矿试验研究 被引量:6
1
作者 戴新宇 《矿产综合利用》 CAS 2008年第5期38-42,共5页
针对某浮磷尾矿的性质特点,确定采用"弱磁除铁—强磁预选—钛浮选"综合回收工艺流程。结果表明:物料经过Slon-750型脉动高梯度强磁机两段预选,达到钛浮选入选品位要求;采用EM121作为钛铁矿的捕收剂,经过一粗一扫四精,可以得... 针对某浮磷尾矿的性质特点,确定采用"弱磁除铁—强磁预选—钛浮选"综合回收工艺流程。结果表明:物料经过Slon-750型脉动高梯度强磁机两段预选,达到钛浮选入选品位要求;采用EM121作为钛铁矿的捕收剂,经过一粗一扫四精,可以得到钛精矿TiO2品位为45.97%、回收率为51.50%的技术指标。 展开更多
关键词 浮磷尾矿 钛铁 Slon-750型脉动高梯度强磁机
下载PDF
Comparison of mechanical and column flotation performances on recovery of phosphate slimes in presence of nano-microbubbles
2
作者 Fatemeh Taghavi Mohammad Noaparast +1 位作者 Ziaeddin Pourkarimi Fardis Nakhaei 《Journal of Central South University》 SCIE EI CAS CSCD 2022年第1期102-115,共14页
Fine particle flotation has been one of the main problems in many mineral processing plants.The bubble particle collision rate is very low for fine particles,which reduces flotation efficiency.Also,the existence of sl... Fine particle flotation has been one of the main problems in many mineral processing plants.The bubble particle collision rate is very low for fine particles,which reduces flotation efficiency.Also,the existence of slimes is,generally,detrimental to the flotation process,affecting the selectivity and the quality of the concentrates.Besides,it causes an increase in reagents consumption.Hence,in most of processing plants,some of these particles are transmitted to the tailing ponds to reduce the effects of these problems and increase the selectivity of the process.Esfordi phosphate plant in Iran loses more than 30%of its capacity as particles with d 80 finer than 30μm.These fine particles with 15.9%P_(2)O_(5)content are transferred to tailing dam.Processing of fine particles is very important for phosphate industry from economic and environmental aspects.This study addressed the processing of fine tailings(slimes)from a phosphate ore concentrator via flotation,despite the traditional view that ultrafine particles do not float.Phosphate flotation performances in the presence and absence of nanobubbles(NBs)in both mechanical and column cells were compared according to the metallurgical results of the process.NBs(generated by hydrodynamic cavitation)have interesting and exclusive properties such as high stability,durability and high surface area per volume,leading to increase of their utilization in mining-metallurgy and environmental areas.The results of this study revealed that,in the absence of NBs,a concentrate containing 26.9%P_(2)O_(5)with a recovery of 29.13%was obtained using mechanical cells in comparison to 31.6%P_(2)O_(5)with a recovery of 32.74%obtained using column flotation.In the presence of NBs,the recoveries of the concentrate of the mechanical and column flotation increased to 40.49%and 41.26%with 28.47%and 30.43%P_(2)O_(5)contents,respectively.Comparative study showed that the column flotation was almost more efficient for processing the phosphate ore in the presence of the NBs,and had thicker froth layer compared to the mechanical flotation. 展开更多
关键词 column flotation mechanical cell PHOSPHATE TAILINGS SLIME NANOBUBBLE Venturi tube hydrodynamic cavitation
下载PDF
上一页 1 下一页 到第