聚乙烯热熔涂塑粉的研制
1
作者 张文林 张瑞 王润珩 《陕西化工》 CSCD 1995年第3期33-34,共2页
聚乙烯热熔涂塑粉的研制张文林,张瑞,王润珩(河北工学院化工系天津300130)1前言粉末涂料由于具有施工迅速、无毒、不污染环境等优点,在涂料行业受到普遍重视 ̄[1]。目前已在金属制品,特别是家用电器的表面涂覆中大量应... 聚乙烯热熔涂塑粉的研制张文林,张瑞,王润珩(河北工学院化工系天津300130)1前言粉末涂料由于具有施工迅速、无毒、不污染环境等优点,在涂料行业受到普遍重视 ̄[1]。目前已在金属制品,特别是家用电器的表面涂覆中大量应用,如环氧型、聚酯型、环氧—聚酯型... 展开更多
关键词 聚乙烯涂塑粉 末涂料 热熔涂塑粉 涂塑粉
下载PDF
Fracture Behavior Characteristic of Ceramic Reinforced Metal-Base Coatings
2
作者 马崇 荆洪阳 徐连勇 《Transactions of Tianjin University》 EI CAS 2009年第1期50-55,共6页
The fracture behavior of a ceramic reinforced metal-base coating prepared by high velocity arc spray-ing (HVAS) technology in three-point bending test was studied. Moreover, finite element analysis (FEA) was adopted t... The fracture behavior of a ceramic reinforced metal-base coating prepared by high velocity arc spray-ing (HVAS) technology in three-point bending test was studied. Moreover, finite element analysis (FEA) was adopted to analyze the stress distribution in the crack front. It can be found that the crack normal to the interface in the coatings occurred at the location where a fixed moment of force was reached. So the critical moment can be taken as the coating cracking criterion, which was confirmed by FEA results. In addition, the stress levels at three different locations where cracks occurred near the interface are almost the same. The results will provide reference for the design of coatings and the structure integrity evaluation of coating/substrate systems. 展开更多
关键词 COATINGS interface fracture behavior finite element analysis