To study the effect of electrolytic concentration,bioactive ceramic films containing Ca and P on the surface of the Ti6Al4V alloy were prepared by micro-arc oxidation(MAO) in aqueous solutions of different concentrati...To study the effect of electrolytic concentration,bioactive ceramic films containing Ca and P on the surface of the Ti6Al4V alloy were prepared by micro-arc oxidation(MAO) in aqueous solutions of different concentrations.Composition,micro-morphology,wettability of the films and their corrosion behavior in a Hank's SBF were studied.Our experimental results show that the film is mainly composed of anatase,rutile and amorphous phases.With an increase in electrolytic concentration,the ratio of rutile in films enlarge and small amounts of calcium phosphate(Ca3(PO4)2) and hydroxyapatite(HA) appear.The number of micropores in films increases but their dimensions decrease and their porosities increase slightly.As the surface roughness of MAO film increases with concentration,the wettablility of the oxide film improves continually,while micro-hardness increases at first and then decreases.MAO treatment clearly improves the corrosion resistance of substrates in a Hank's SBF.展开更多
Nanosized calcium carbonate particles were prepared with a continuous gas-liquid membrane contactor. The effects of Ca(OH)2 concentration, CO2 pressure and liquid flow velocity on the particles morphology, pressure dr...Nanosized calcium carbonate particles were prepared with a continuous gas-liquid membrane contactor. The effects of Ca(OH)2 concentration, CO2 pressure and liquid flow velocity on the particles morphology, pressure drop and membrane fouling were studied. With rising Ca(OH)2 concentrations, the average size of the particles increased. The effects of Ca(OH)2 concentration and CO2 pressure on particles were not apparent under the experimental conditions. When the Ca(OH)2 concentration and liquid flow velocity were high, or the CO2 pressure was low, the fouling on the membrane external surface at the contactor entrance was serious due to liquid leakage, whereas the fouling was slight at exit. The fouling on the membrane inner-surface at entrance was apparent due to adsorption of raw materials. The membrane can be recovered by washing with dilute hydrochloric acid and reused for at least 6 times without performance deterioration.展开更多
基金Projects 50535050 supported by the National Natural Science Foundation of ChinaNCET-06-0479 by the Program for New Century Excellent Talents in University of China
文摘To study the effect of electrolytic concentration,bioactive ceramic films containing Ca and P on the surface of the Ti6Al4V alloy were prepared by micro-arc oxidation(MAO) in aqueous solutions of different concentrations.Composition,micro-morphology,wettability of the films and their corrosion behavior in a Hank's SBF were studied.Our experimental results show that the film is mainly composed of anatase,rutile and amorphous phases.With an increase in electrolytic concentration,the ratio of rutile in films enlarge and small amounts of calcium phosphate(Ca3(PO4)2) and hydroxyapatite(HA) appear.The number of micropores in films increases but their dimensions decrease and their porosities increase slightly.As the surface roughness of MAO film increases with concentration,the wettablility of the oxide film improves continually,while micro-hardness increases at first and then decreases.MAO treatment clearly improves the corrosion resistance of substrates in a Hank's SBF.
基金Supported by the National Natural Science Foundation of China (20676016, 21076024).
文摘Nanosized calcium carbonate particles were prepared with a continuous gas-liquid membrane contactor. The effects of Ca(OH)2 concentration, CO2 pressure and liquid flow velocity on the particles morphology, pressure drop and membrane fouling were studied. With rising Ca(OH)2 concentrations, the average size of the particles increased. The effects of Ca(OH)2 concentration and CO2 pressure on particles were not apparent under the experimental conditions. When the Ca(OH)2 concentration and liquid flow velocity were high, or the CO2 pressure was low, the fouling on the membrane external surface at the contactor entrance was serious due to liquid leakage, whereas the fouling was slight at exit. The fouling on the membrane inner-surface at entrance was apparent due to adsorption of raw materials. The membrane can be recovered by washing with dilute hydrochloric acid and reused for at least 6 times without performance deterioration.