Effect of laser shock processing on erosive resistance of 6061-T6 aluminum 被引量:1
1
作者 J.IBARRA E.RODRíGUEZ +4 位作者 O.JIMéNEZ G.GóMEZ-ROSAS M.FLORES J.VERDUZCO J.CHáVEZ 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2016年第6期1522-1530,共9页
Application of laser shock processing (LSP) on 6061-T6 aluminum was made in order to evaluate its response to the erosive wear by silica sand. Impact angles of 15° , 30° , 60° and 90° were tes... Application of laser shock processing (LSP) on 6061-T6 aluminum was made in order to evaluate its response to the erosive wear by silica sand. Impact angles of 15° , 30° , 60° and 90° were tested, two particle speeds (37 and 58 m/s) and two LSP irradiation conditions were used. Erosion marks were characterized by 3D profilometry and SEM analysis was conducted to identify the erosion mechanisms for each tested angle. The results showed a maximum erosive wear at low impact angles (ductile type behavior). Erosion strength and the erosion mechanisms were not affected by the application of LSP and they were attributed to the high strain rate of the erosion phenomena. A few differences encountered on the erosion plots were explained on the basis of the surface roughness left by the LSP process. The maximum mass loss and the maximum erosion penetration happened in different impact angles (15° and 30° , respectively). Finally, a well-defined erosion mechanism transition was observed, from cutting action at low impact angle, to crater formation at 90° of incidence. 展开更多
关键词 6061-T6 aluminum erosive wear laser shock processing
下载PDF
体育器材用X80钢材焊接头疲劳韧性分析
2
作者 蒋佳莲 《贵州工业职业技术学院学报》 2014年第4期19-21,45,共4页
本实验对体育器材用X80钢种在激光冲击焊接工艺下焊接头疲劳韧性进行了研究,钢样疲劳极限强度经激光冲击处理后,较未处理状态显著增强,增强幅度约为11.3%;在裂纹源区,用激光冲击处理后,焊接接头的表面有残存压应力,应力集中得... 本实验对体育器材用X80钢种在激光冲击焊接工艺下焊接头疲劳韧性进行了研究,钢样疲劳极限强度经激光冲击处理后,较未处理状态显著增强,增强幅度约为11.3%;在裂纹源区,用激光冲击处理后,焊接接头的表面有残存压应力,应力集中得到很大程度的抑制,疲劳裂纹源区的位置发生改变,由原来的表层变化到经处理形成的强化层下方;在扩展区,经激光冲击处理后,有很多位错生成于钢样的表层,有效的抑制二次裂纹的扩张;在断裂区,经处理后钢样的分层断裂得到了有效的缓解。 展开更多
关键词 X80钢 疲劳性能 激光冲击焊接工艺