熔融态钒渣氧化钙化后酸浸研究 被引量:6
1
作者 李昆 宋文臣 +1 位作者 郑权 李宏 《钢铁钒钛》 CAS 北大核心 2013年第5期15-18,22,共5页
把钒渣加热到熔融态直接加入CaO并吹氧,将渣中钒氧化为四价或五价与CaO形成钒酸钙,然后酸浸其中的钒,研究了钙钒比、硫酸浓度和固液比对浸出率的影响。结果表明:生成以CaV2O5为主的钒酸钙盐,在70%钒渣粒度小于0.074 mm、钙钒比0.5~0.9... 把钒渣加热到熔融态直接加入CaO并吹氧,将渣中钒氧化为四价或五价与CaO形成钒酸钙,然后酸浸其中的钒,研究了钙钒比、硫酸浓度和固液比对浸出率的影响。结果表明:生成以CaV2O5为主的钒酸钙盐,在70%钒渣粒度小于0.074 mm、钙钒比0.5~0.9、浸出温度90℃、反应时间120 min、固液比1∶5、硫酸浓度20%的条件下,钒浸出率可以达到88%以上。 展开更多
关键词 熔融态钒渣 钙化焙烧 吹氧 酸钙 酸浸
原文传递
Extraction of vanadium from molten vanadium bearing slag by oxidation with pure oxygen in the presence of CaO 被引量:13
2
作者 宋文臣 李宏 +2 位作者 朱福兴 李昆 郑权 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第8期2687-2694,共8页
A novel process of vanadium extraction from vanadium slag in its molten state was conducted at the laboratory scale by oxidation with pure oxygen in the presence of CaO. The effect of mass ratio of CaO to V2O5 on the ... A novel process of vanadium extraction from vanadium slag in its molten state was conducted at the laboratory scale by oxidation with pure oxygen in the presence of CaO. The effect of mass ratio of CaO to V2O5 on the recovery of vanadium was studied. The sintered samples were leached by H2SO4 solution and characterized by XRD, XPS, SEM and EDS techniques. Compared with the roasting process, the energy saving effect of the proposed process was also discussed. The results showed that vanadium-rich phases were formed and vanadium mainly existed in the forms of CaV2O5 and Ca2V2O7. The formation mechanism of calcium vanadates in the molten vanadium bearing slag was explained. The XRD and XPS results implied that there was a limit to the oxidation reaction of V(IV) to V(V) under the high temperatures even though oxygen-supply was sufficient. An increase in the CaO content led to an increase in the formation of Ca2V2O7. About 90%of the vanadium recovery was obtained under optimal experiment conditions (mass ratio of CaO to V2O5 of 0.6, particle size 120 to 150μm, leaching temperature 90 °C, leaching time 2 h, H2SO4 concentration 20%, liquid to solid ratio 5:1 mL/g, stirring speed 500 r/min). The energy of 1.85×106 kJ could be saved in every 1000 kg of vanadium bearing slag using the proposed process from the theoretical calculation results. Recovery of vanadium from the molten vanadium bearing slag and utilisation of its heat energy are important not only for saving metal resources, but also for energy saving and emission reduction. 展开更多
关键词 molten vanadium bearing slag CAO OXIDATION acid leaching vanadium recovery energy saving effect
下载PDF