In order to provide a new way for waste cooking oil(WCO) resource utilization, several diester derivatives were obtained from WCO through a three-step chemical modifications, viz.: transesterification, epoxidation and...In order to provide a new way for waste cooking oil(WCO) resource utilization, several diester derivatives were obtained from WCO through a three-step chemical modifications, viz.: transesterification, epoxidation and oxirane ring opening with carboxylic acids. The effects of the chain length of side chain groups on the viscosity, acid value, low temperature fluidity, thermo-oxidative stability, tribological properties and surface tension of diester derivatives were investigated. The results showed that increasing the chain length of side chain groups had a positive influence on the viscosity, viscosity index, acid value, pour point, friction coefficient and wear scar diameter along with a negative influence on the oxidation onset temperature, volatile loss, insoluble deposit, maximum non-seizure load and surface tension. These diester derivatives exhibited improved physicochemical and tribological properties that make themselves promising environmentally friendly biolubricant basestocks.展开更多
A new kind of silicon-based biological lubricating base oil with good viscosity-temperature behavior,viscosity index,thermostability,oxidation stability and wear resistance performance was synthesized as a derivative ...A new kind of silicon-based biological lubricating base oil with good viscosity-temperature behavior,viscosity index,thermostability,oxidation stability and wear resistance performance was synthesized as a derivative of methyl oleate.Trimethylsilylation reaction was introduced to further improve methyl oleate oxidation stability and lubricity after epoxidation and open-ring reactions.The order of effectiveness of acid binding agent was N,N-diisopropylethylamine(DIEA) > pyridine > diethylamine > triethylamine,and the effects of various parameters on the trimethylsilylation reaction as well as on the silicon-oxygen bond stability and reaction yield were studied.A maximum yield of 34.54%was achieved at hydroxyl/trimethyl chlorosilane/DIEA molar ratio of1:1.25:1,reaction temperature 40℃,reaction time 1.5 h.展开更多
基金the financial support from the Natural Science Foundation of Chongqing(Project No.cstc2014jcyj A90013)
文摘In order to provide a new way for waste cooking oil(WCO) resource utilization, several diester derivatives were obtained from WCO through a three-step chemical modifications, viz.: transesterification, epoxidation and oxirane ring opening with carboxylic acids. The effects of the chain length of side chain groups on the viscosity, acid value, low temperature fluidity, thermo-oxidative stability, tribological properties and surface tension of diester derivatives were investigated. The results showed that increasing the chain length of side chain groups had a positive influence on the viscosity, viscosity index, acid value, pour point, friction coefficient and wear scar diameter along with a negative influence on the oxidation onset temperature, volatile loss, insoluble deposit, maximum non-seizure load and surface tension. These diester derivatives exhibited improved physicochemical and tribological properties that make themselves promising environmentally friendly biolubricant basestocks.
基金Supported by the National Natural Science Foundation of China(21306088)National Key Technologies R&D Program of China(2015BAD15B07)+1 种基金State Key Laboratory of Chemical Engineering(SKL-Ch E-13A01,Tsinghua University,China)Priority Academic Program Development of Jiangsu Higher Education Institutions(PAPD,China)
文摘A new kind of silicon-based biological lubricating base oil with good viscosity-temperature behavior,viscosity index,thermostability,oxidation stability and wear resistance performance was synthesized as a derivative of methyl oleate.Trimethylsilylation reaction was introduced to further improve methyl oleate oxidation stability and lubricity after epoxidation and open-ring reactions.The order of effectiveness of acid binding agent was N,N-diisopropylethylamine(DIEA) > pyridine > diethylamine > triethylamine,and the effects of various parameters on the trimethylsilylation reaction as well as on the silicon-oxygen bond stability and reaction yield were studied.A maximum yield of 34.54%was achieved at hydroxyl/trimethyl chlorosilane/DIEA molar ratio of1:1.25:1,reaction temperature 40℃,reaction time 1.5 h.