Adopting Poly(ethylene glycol) adipate Dilpoly- (ethylene glycol)] adipate polydiglycol adipate glycol (PDAG), 1,4-butanediol (BDO), hydroxy silicone oil, methylene diphenyl diisocyanate (MDI) as the raw mat...Adopting Poly(ethylene glycol) adipate Dilpoly- (ethylene glycol)] adipate polydiglycol adipate glycol (PDAG), 1,4-butanediol (BDO), hydroxy silicone oil, methylene diphenyl diisocyanate (MDI) as the raw material, a new polyurethane elastic body can be made through prepolymerization. After measurement of the moisture permeability, adsorption quantity and mechanical properties of the membrane made with the elastic body, we also proofed its formula by infrared spectroscopy. The result showed that the moisture permeability of the membrane, with a certain intelligent thermotropic quality, will increase by 3 to 4 times when the temperature is between 25℃-45℃.展开更多
基金Acknowledgments: This work was supported in part by the National Natural Science Foundation of China (No. 20504023).
文摘Adopting Poly(ethylene glycol) adipate Dilpoly- (ethylene glycol)] adipate polydiglycol adipate glycol (PDAG), 1,4-butanediol (BDO), hydroxy silicone oil, methylene diphenyl diisocyanate (MDI) as the raw material, a new polyurethane elastic body can be made through prepolymerization. After measurement of the moisture permeability, adsorption quantity and mechanical properties of the membrane made with the elastic body, we also proofed its formula by infrared spectroscopy. The result showed that the moisture permeability of the membrane, with a certain intelligent thermotropic quality, will increase by 3 to 4 times when the temperature is between 25℃-45℃.