基于矫顽力的钢板应力集中区域检测方法 被引量:7
1
作者 杨理践 周玙 高松巍 《沈阳工业大学学报》 EI CAS 北大核心 2015年第5期536-541,共6页
针对铁磁性材料由于应力集中导致裂纹、断裂甚至失效等问题,研究了应力对铁磁性材料磁化强度取向的影响以及铁磁性材料矫顽力与所受应力的关系,提出了通过测量铁磁性材料的矫顽力实现应力检测的方法.采用U型探头进行测量,由U型探头上激... 针对铁磁性材料由于应力集中导致裂纹、断裂甚至失效等问题,研究了应力对铁磁性材料磁化强度取向的影响以及铁磁性材料矫顽力与所受应力的关系,提出了通过测量铁磁性材料的矫顽力实现应力检测的方法.采用U型探头进行测量,由U型探头上激励线圈中的电流信号和检测线圈中产生的电压信号描绘出不同外力条件下钢板的磁滞回线,从而得到钢板矫顽力的值.结果表明,外力使钢板内部产生应力,导致矫顽力减小,通过测量铁磁性材料的矫顽力实现对应力集中区域的检测,有效预防了工件由于应力集中造成的断裂等问题. 展开更多
关键词 矫顽力 应力集中区域 铁磁性材料 磁化强度取向 U型探头 激励线圈 检测线圈 磁滞回线
下载PDF
Microstructure characteristics and effect of grain orientation on magnetic properties of Fe_(63)Co_(32)Gd_5 alloy ribbons
2
作者 姚文静 王楠 LEE Je-hyun 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第6期2014-2019,共6页
By using the melt spinning techniques, the Fe63Co32Gd5 alloy ribbons with 15-50 m in thickness and 3-7 mm in width were prepared at the wheel speeds of 15, 20, 25 and 35 m/s. The rapid solidification microstructures w... By using the melt spinning techniques, the Fe63Co32Gd5 alloy ribbons with 15-50 m in thickness and 3-7 mm in width were prepared at the wheel speeds of 15, 20, 25 and 35 m/s. The rapid solidification microstructures were characterized by three layers, the middle layer of which reaches 80% thickness and forms the column grain of(Fe,Co) solid with Gd solution. Grain refinement takes place with the increase of the wheel speed. And after 0.5 h heat treatment at 823 K, the ribbon thickness becomes larger and the middle layer of column grain is very orderly perpendicular to the ribbon plane. The coercivity of quenched and annealed Fe63Co32Gd5 ribbons both have the inflection point at the wheel speed of 20 m/s, and the tendency is declining. The heat treatment processing makes the coercivity become lower by improving the order of(Fe,Co)17Gd2 compound. The saturation magnetization of quenched ribbons increases with the enhancement of wheel speed, whereas that of annealed ones decreases firstly and then increases. The minimum coercivity is 5.30×103 A/m and the maximum saturation magnetization is 163.62 A·m2/kg, which is obtained in the conditions of the wheel speed of 35 m/s and 0.5 h heat treatment at the temperature of 823 K. 展开更多
关键词 Fe-Co-Gd alloy ribbon rapid solidification phase composition magnetic properties