Basicity has an important effect on the sinter quality, especially for low-titanium vanadium-titanium sinter. The effect of basieity on sintering behavior of low-titanium vanadium-titanium mixture, and the transferenc...Basicity has an important effect on the sinter quality, especially for low-titanium vanadium-titanium sinter. The effect of basieity on sintering behavior of low-titanium vanadium-titanium mixture, and the transference and distribution of element in sintering process were researched by sinter pot test, mineralogical analysis, scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) analysis. The results show that CaO preferentially reacts with TiO2, generating pervoskite, so that the total liquid phase content of the sinter is low. There is an increase in the perovskite concentration of the sinter with the basicity ranging from 1.9:1 to 2.7:1. With increasing the basicity, the calcium ferrite content increases slightly and then rises rapidly, while the silicate content decreases and the metallurgical property of the sinter is improved. As for the distribution of these elements in the sinter, Ti occurs mainly in perovskite, V occurs mainly in silicate, and Fe occurs mainly in magnetite and hematite. The most abundant occurrence of Ca and Si occurs in silicate and perovskite. With increasing the basicity, the contents of A1 and Mg increase in calcium ferrite, while they decrease in other minerals.展开更多
The effects of basicity and temperature on the reduction process of Hongge high-chromium vanadium-titanium magnetite(HCVTM)sinter were investigated in this work.The main characterization methods of X-ray fluorescence(...The effects of basicity and temperature on the reduction process of Hongge high-chromium vanadium-titanium magnetite(HCVTM)sinter were investigated in this work.The main characterization methods of X-ray fluorescence(XRF),X-ray diffraction(XRD),scanning electron microscope(SEM),and metallographic microscope were employed in this study.In this work,the reduction of HCVTM sinter with different temperature and basicity were experimented.The Fe,FeO,and TiO in reductive samples increase with increasing basicity and temperatures.The increase of basicity and temperature is favorable to the reduction of HCVTM sinter.The Fe phase has out-migration tendency to the surface of sinter while the perovskite and silicate phases have in-migration tendency to the inside of sinter.The reduction degradation index(RDI)decreases while the reduction index(RI)increases with increasing basicity.The RI increases from 67.14%to 82.09%with increasing temperature from 1073 K to 1373 K.展开更多
基金Projects(2012AA062302,2012AA062304) supported by the National High Technology Research and Development Program of China(863 Program)Projects(51090384,51174051) supported by the National Natural Science Foundation of ChinaProject(2012DFR60210) supported by the International Cooperation of Ministry of China
文摘Basicity has an important effect on the sinter quality, especially for low-titanium vanadium-titanium sinter. The effect of basieity on sintering behavior of low-titanium vanadium-titanium mixture, and the transference and distribution of element in sintering process were researched by sinter pot test, mineralogical analysis, scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) analysis. The results show that CaO preferentially reacts with TiO2, generating pervoskite, so that the total liquid phase content of the sinter is low. There is an increase in the perovskite concentration of the sinter with the basicity ranging from 1.9:1 to 2.7:1. With increasing the basicity, the calcium ferrite content increases slightly and then rises rapidly, while the silicate content decreases and the metallurgical property of the sinter is improved. As for the distribution of these elements in the sinter, Ti occurs mainly in perovskite, V occurs mainly in silicate, and Fe occurs mainly in magnetite and hematite. The most abundant occurrence of Ca and Si occurs in silicate and perovskite. With increasing the basicity, the contents of A1 and Mg increase in calcium ferrite, while they decrease in other minerals.
基金Project(2013CB632603)supported by the National Basic Research Program of ChinaProject(2015BAB19B02)supported by the National Key Technology R&D Program of ChinaProjects(51674084,51174051,51574082)supported by National Natural Science Foundation of China
文摘The effects of basicity and temperature on the reduction process of Hongge high-chromium vanadium-titanium magnetite(HCVTM)sinter were investigated in this work.The main characterization methods of X-ray fluorescence(XRF),X-ray diffraction(XRD),scanning electron microscope(SEM),and metallographic microscope were employed in this study.In this work,the reduction of HCVTM sinter with different temperature and basicity were experimented.The Fe,FeO,and TiO in reductive samples increase with increasing basicity and temperatures.The increase of basicity and temperature is favorable to the reduction of HCVTM sinter.The Fe phase has out-migration tendency to the surface of sinter while the perovskite and silicate phases have in-migration tendency to the inside of sinter.The reduction degradation index(RDI)decreases while the reduction index(RI)increases with increasing basicity.The RI increases from 67.14%to 82.09%with increasing temperature from 1073 K to 1373 K.