高碱度烧结矿粉化的控制与冀东地区精矿粉的合理品位 被引量:2
1
作者 何福珠 《烧结球团》 北大核心 1998年第5期13-16,共4页
高碱度烧结矿粉比的主要原因在于烧结矿中SiO2和FeO高.提高精矿品位、控制FeO含量或配入抑制剂都可以抑制粉化.冀东地区磁铁矿结晶颗粒大,易磨易选,对精矿进行细磨以提高品位,不但可以抑制粉比.而且可使选矿和炼铁都得到非常好的... 高碱度烧结矿粉比的主要原因在于烧结矿中SiO2和FeO高.提高精矿品位、控制FeO含量或配入抑制剂都可以抑制粉化.冀东地区磁铁矿结晶颗粒大,易磨易选,对精矿进行细磨以提高品位,不但可以抑制粉比.而且可使选矿和炼铁都得到非常好的经济效益. 展开更多
关键词 高碱度烧结矿 粉化抑制 精矿品位 烧结矿
下载PDF
太钢烧结矿自然粉化机理研究 被引量:5
2
作者 戎玉萍 蔡湄夏 《烧结球团》 北大核心 2001年第1期18-20,共3页
介绍了太钢烧结矿自然粉化的状况 ,借助矿相显微镜研究了烧结矿粉化的机理 。
关键词 烧结矿 矿物组成 矿相结构 粉化抑制
下载PDF
Hydrolysis of Raw Corn Starch Granules by Glucoamylase and Product Inhibition During the Hydrolysis
3
作者 王金鹏 曾爱武 +2 位作者 刘振 袁希钢 吴少敏 《Transactions of Tianjin University》 EI CAS 2005年第3期199-203,共5页
Raw corn starch granules were hydrolysized by glucoamylase in a chemostat. The hydro- lysis of three different-sized granules shows that smaller granules undergo more hydrolyzation than larger ones. After 78 h, 9700 o... Raw corn starch granules were hydrolysized by glucoamylase in a chemostat. The hydro- lysis of three different-sized granules shows that smaller granules undergo more hydrolyzation than larger ones. After 78 h, 9700 of the granules was hydrolysized with diameter between 0.15 mm and 0.3 mm at 50 ℃. When corn starch concentration increased from 100 g/L to 250 g/L, the amount of reducing sugar produced was proportional to the initial substrate concentration and no substrate inhibition phenomenon appeared. In order to study the product inhibition exactly, the product from hydrolysis reaction itself was added into the hydrolysis system at the beginning of starch hydrolysis. Product inhibition with different quantities of product added were studied in the initial several hours, during which period enzyme inactivation could be neglected and product inhibition could be studied separately. The experiments indicate that product inhibition happens when the additional quantity exceeds 9.56 g/L. 展开更多
关键词 HYDROLYSIS starch granules GLUCOAMYLASE product inhibition
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部