MM—聚合金属陶瓷的研究
1
作者 陈琦 党庆波 +2 位作者 陈辉 陈红 王晓光 《煤矿机械》 1998年第4期8-10,共3页
通过试验的方法,详细研究了德国美特铁公司生产的一种新的粘接粘涂材料——聚合金属陶瓷的技术性能、主要特点和应用情况。
关键词 聚合金属陶瓷 粘接粘涂材料 强度
下载PDF
MM──美特铁聚合金属陶瓷的试验研究与应用
2
作者 刘建卡 陈政国 陈璐 《中国修船》 北大核心 1997年第5期33-37,共5页
本文介绍试验研究的一种新的同分子聚合材料──美特铁聚合金属陶瓷,并对其的技术性能、主要特点和应用进行了阐述。
关键词 聚合金属陶瓷 粘接粘涂 船舶 维修 美特铁 试验
下载PDF
Multiple Coatings can Improve the Bond Durability of One-step Self-etching Adhesive to Primary Dentin
3
作者 Lin Ma Jian-feng Zhou +2 位作者 Quan Jing Ji-zhi Zhao Kuo Wan 《Chinese Medical Sciences Journal》 CAS CSCD 2012年第2期106-111,共6页
Objective To investigate whether multiple coatings can improve the bond durability of one-step self-etching adhesive to primary dentin. Methods Twelve caries-free human primary molars were randomly divided into 2 gro... Objective To investigate whether multiple coatings can improve the bond durability of one-step self-etching adhesive to primary dentin. Methods Twelve caries-free human primary molars were randomly divided into 2 groups. In group 1, each tooth was hemisected into 2 halves. One half was assigned to the control subgroup 1, which was bonded with a commercially available one-step self-etching adhesive according to the manufacturer's instruc- tions; the other half was assigned to experimental subgroup 1, in which the adhesive was applied three times before light curing. In group 2, one split half tooth was bonded with a commercially available one-step self-etching adhesive according to the manufacturer's instructions; for the other half, three layers of adhesive were applied with each successive layer of light curing. Specimens were stored in 0.9% NaC1 containing 0.02% sodium azide at 37℃ for 18 months and then were subjected to microtensile bond strength test and the fracture mode analysis. Results When the adhesive was applied three times before light curing, the bond strength of the ex- perimental subgroup 1 was significantly higher than that of the control subgroup 1 (47.46__+13.91 vs. 38.12+11.21 MPa, P〈O.05). When using the technique of applying multiple layers of adhesive with each successive layer of light curing, no difference was observed in bond strength between the control subgroup and the experimental subgroup (39.40+8.87 vs. 40.87-+9.33 MPa, P〉O.05). Conclusion Multiple coatings can improve the bond durability of one-step self-etching adhesive to primary dentin when using the technique of light-curing after applying 3 layers of adhesive. 展开更多
关键词 self-etching adhesive microtensile bond strength test primary dentin multiple coatings
下载PDF
应用于设备修复的美特铁聚合金属陶瓷材料
4
作者 刘建卡 《机械工艺师》 CSCD 2000年第7期28-30,共3页
介绍一种国外金属冷焊材料—美特铁高分子聚合金属陶瓷系列产品的技术性能以及美特铁产品的主要特点和工业应用。