1案例资料 1.1简要案情 死者,男性,40岁。2009年6月14日因哮喘发作就医。主诉反复咳嗽、气促30余年,近半月加重。无其他特殊现病史。查体:呼吸稍促、双肺呼吸音粗伴哮鸣音。肺功能报告:FEVl/FVC(第一秒用力呼气容积/用力肺活... 1案例资料 1.1简要案情 死者,男性,40岁。2009年6月14日因哮喘发作就医。主诉反复咳嗽、气促30余年,近半月加重。无其他特殊现病史。查体:呼吸稍促、双肺呼吸音粗伴哮鸣音。肺功能报告:FEVl/FVC(第一秒用力呼气容积/用力肺活量)〈70%、FEVl〈30%预计值,极重度阻塞性通气功能障碍,支气管扩张试验阴性。诊断:支气管哮喘。给予常规抗哮喘口服药和气雾剂,回家按医嘱用药,约3h后,咳嗽、气促急剧加重并出现胸闷、喘息及呼吸困难,急请120,诊断哮喘持续状态,现场抢救无效死亡。 展开更多
关键词 法医病理学 组织气泡 气栓 阻塞性通气障碍
原文传递
Effects of processing parameters on microstructure of semi-solid slurry of AZ91D magnesium alloy prepared by gas bubbling 被引量:3
2
作者 张扬 吴国华 +3 位作者 刘文才 张亮 庞松 丁文江 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2015年第7期2181-2187,共7页
The semi-solid slurry of AZ91 D magnesium alloy was prepared by gas bubbling process.The effect of processing parameters,including gas flow rate,cooling rate and stirring end temperature,on microstructure of AZ91 D se... The semi-solid slurry of AZ91 D magnesium alloy was prepared by gas bubbling process.The effect of processing parameters,including gas flow rate,cooling rate and stirring end temperature,on microstructure of AZ91 D semi-solid slurry was investigated.With increasing the gas flow rate from 0 to 5 L/min,the average size of primary α-Mg particles decreases from 119.1 to77.2μm and the average shape factor increases continuously from 0.1 to 0.596.The formation of non-dendritic primary α-Mg particles during gas bubbling is the result of combined effects of dendrite fragmentation and copious nucleation.With increasing the cooling rate from 3.6 to 14.6℃/min,the average particle size of primary α-Mg phase decreases from 105.0 to 68.1μm while the average shape factor peaks at 9.1℃/min.Both high and low cooling rates can induce dendritic growth of primary α-Mg particles.Changing the stirring end temperature from 590 to 595℃ has little effect on the average size and shape factor of primary α-Mg particles in AZ91 D semi-solid slurry.The insensitivity of semi-solid microstructures to the stirring end temperature is attributed to the sufficient quantity of primary particles formed in the melt. 展开更多
关键词 AZ91D magnesium alloy semi-solid slurry gas bubbling MICROSTRUCTURE