胶管密封结构失效分析
1
作者 封慧 庄士俊 +3 位作者 祁同晖 李正现 王晶 王泉明 《中国科技纵横》 2024年第9期61-63,共3页
胶管密封结构应用广泛,解决胶管密封结构的泄漏和难装配问题至关重要。基于此,本文介绍了胶管密封结构的组成以及密封机理,从设计、质量和装配三个方面总结了胶管密封结构的故障原因,详细分析了胶管破裂故障和难装配故障,以期为后续密... 胶管密封结构应用广泛,解决胶管密封结构的泄漏和难装配问题至关重要。基于此,本文介绍了胶管密封结构的组成以及密封机理,从设计、质量和装配三个方面总结了胶管密封结构的故障原因,详细分析了胶管破裂故障和难装配故障,以期为后续密封结构设计提供参考,防止此类问题的再次发生。 展开更多
关键词 胶管密封结构 密封 泄漏
下载PDF
对钢丝增强型液压胶管接头拔脱故障的研究 被引量:1
2
作者 戚伟 陈振广 《特种橡胶制品》 2016年第5期64-66,共3页
从胶管尺寸、粘合和接头的结构、装配方面分析了造成胶管拔脱的各种原因,以及如何通过控制生产工艺和过程、如何选择接头、如何进行装配等来预防和控制接头拔脱。
关键词 接头拔脱 粘合 胶管结构 接头设计 扣压
下载PDF
Thermal Structure of Glass Fiber Reinforce Plastic Support Structure 被引量:2
3
作者 刘康 汪荣顺 +1 位作者 石玉美 顾安忠 《Journal of Shanghai Jiaotong university(Science)》 EI 2008年第3期370-374,共5页
The assembled form of thick-wall glass fiber reinforced plastics (GFRP) tube and 0Cr18Ni9 austenitic stainless steel pipes was designed as the radius thermal-insulating and load-supporting structure in cryogenic vesse... The assembled form of thick-wall glass fiber reinforced plastics (GFRP) tube and 0Cr18Ni9 austenitic stainless steel pipes was designed as the radius thermal-insulating and load-supporting structure in cryogenic vessels. In order to study the thermal leakage and gap changes on the support structure, as well as radius temperature and stress distribution on GFRP tube, an experimental investigation has been taken. The results indicate that the support structure is proved to fit well as thermal-insulating and load-supporting part in cryo-genic vessels, furthermore has high security during cryogenic applications. 展开更多
关键词 glass fiber reinforced plastics (GFRP) tube support structure CRYOGENIC temperature stress
下载PDF
Surface treatment of 3D outside serrated integral-fin tube manufactured by rolling and extrusion
4
作者 白鹏飞 刘小康 +1 位作者 燕辉 唐彪 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2010年第5期844-848,共5页
The outside serrated integral-fin tubes fabricated by rolling-plowing-extrusion processing were surface-treated through different processes of annealing in hydrogen atmosphere,electrochemical corrosion or sandblasting... The outside serrated integral-fin tubes fabricated by rolling-plowing-extrusion processing were surface-treated through different processes of annealing in hydrogen atmosphere,electrochemical corrosion or sandblasting.The purpose was to eliminate residual stress,clear secondary micro-fins and enhance heat transfer performance.By comparing the surface characteristics,it is found that the finned tubes treated by electrochemical corrosion have the most glabrous surfaces where the fins are almost perfectly reserved.Clear layer cracks can be observed on the top of the fins.These structures are effective in enhancing heat transfer performance when being applied to flow heat exchange.Therefore,the finned tubes treated by electrochemical corrosion are proper for the tubular exchanger with water coolant.The finned tubes treated by sandblasting have rougher surfaces with layer cracks and micro gaps removed.As these structures are useful to clearing adhesive feculence,the tubes are more suitable for the tubular heat exchanger with oil coolant. 展开更多
关键词 finned tube surface treating heat transfer multi-dimensional surface
下载PDF
Analysis of the Microstructure and Permeability of the Laminates with Different Fiber Volume Fraction
5
作者 马悦 李炜 梁子青 《Journal of Donghua University(English Edition)》 EI CAS 2008年第3期282-285,共4页
Microstructures of laminates produced by epoxy/carbon fibers with different fiber volume fraction were studied by analyzing the composite cross-sections.The main result of the compaction of reinforcement is the flatti... Microstructures of laminates produced by epoxy/carbon fibers with different fiber volume fraction were studied by analyzing the composite cross-sections.The main result of the compaction of reinforcement is the flatting of bundle shape,the reducing of gap and the embedment of bundles among each layer.The void content outside the bundle decreased sharply during the compaction until it is less than that inside the bundle when the fiber volume fraction is over 60%.The resin flow velocity in the fiber tow is 102-104 times greater than the flow velocity out the fiber tow no matter the capillary pressure is taken into account or not. 展开更多
关键词 MICROSTRUCTURE fiber zolume fraction PERMEABILITY capillary pressure wid