单吹颗粒镁铁水脱硫工艺及应用 被引量:1
1
作者 黄伟烈 徐吕平 《冶金动力》 2014年第4期75-77,共3页
介绍了铁水脱硫的几种方法。详细描述了单吹颗粒镁铁水脱硫技术应用于铁水预处理工艺,从而使生产中脱硫时间被缩短,降低了成本,提高了生产效率,钢铁制品质量得到保证,同时对环境的保护起到非常重要的作用。
关键词 铁水 单吹颗粒镁 达标率 脱硫时间
下载PDF
Acid leaching decarbonization and following pressure oxidation of carbonic refractory gold ore 被引量:2
2
作者 张杜超 肖庆凯 +3 位作者 刘伟锋 陈霖 杨天足 刘又年 《Journal of Central South University》 SCIE EI CAS CSCD 2016年第7期1584-1590,共7页
Carbonate decomposition of carbonic refractory gold ore and the following pressure oxidation were studied.In the carbonate decomposition procedure,the effects of liquid-to-solid ratio and reaction time on decompositio... Carbonate decomposition of carbonic refractory gold ore and the following pressure oxidation were studied.In the carbonate decomposition procedure,the effects of liquid-to-solid ratio and reaction time on decomposition ratio of carbonate were investigated.The experimental result shows that the decomposition ratio of carbonate is 98.24%under the conditions of liquid-to-solid ratio of 5:1,Fe^(3+)concentration of 20 g/L,sulfuric acid concentration of 20 g/L,reaction temperature of 80 ℃ and reaction time of 2 h.Then,the slurry obtained from carbonate decomposition was put into the titanium autoclave for pressure oxidation leaching.Effects of liquid-to-solid ratio,temperature,time and oxygen partial pressure on sulfur oxidation ratio were studied during pressure oxidation.With the prolonged time,pyrite and arsenopyrite are oxidized to ferric subsulfate,hydrated ferric sulfate and jarosite,resulting in the increasing residue ratio.The residue ratio and the sulfur content in the residue can be decreased by ferric subsulfate dissolution.The oxidation ratio of the sulfur is 99.35% under the conditions of oxidation time of 4 h,temperature of 210 ℃,oxygen partial pressure of 0.8 MPa and stirring speed of 600 r/min. 展开更多
关键词 carbonic refractory gold ore carbonate decomposition pressure oxidation ferric subsulfate dissolution
下载PDF