喷雾腐蚀机在Ti/Al腐蚀工艺中的应用
1
作者 徐俊 孙运玺 申强 《电子工业专用设备》 2022年第1期4-7,24,共5页
介绍了喷雾腐蚀机的主要结构和设计优点,简述了SiC功率器件Ti/Al湿法腐蚀工艺;并就生产过程中出现的腐蚀液温度控制、液位传感器、图像识别对中等方面存在的不足做了相应改进。提高了工艺稳定性和生产效率。
关键词 喷雾腐蚀 碳化硅 钛/铝 腐蚀液温度 位传感器 对中
下载PDF
Effect of liquid nitriding at 400–670 ℃ on microstructure and properties of C110 Steel
2
作者 闫静 王均 +4 位作者 谷坛 潘东 王单奇 林元华 范洪远 《Journal of Central South University》 SCIE EI CAS CSCD 2017年第2期325-334,共10页
Liquid nitriding of Cll0 steel was conducted in a wide range of temperatures (400-670 ℃) using a kind of chemical heat-treatments, and the hardness, mechanical and corrosion properties of the nitrided surface were ... Liquid nitriding of Cll0 steel was conducted in a wide range of temperatures (400-670 ℃) using a kind of chemical heat-treatments, and the hardness, mechanical and corrosion properties of the nitrided surface were evaluated. Experimental results revealed that the microstructure and phase constituents of the nitrided surface alloy are highly depended on the processing condition. When C 110 steel was subjected to liquid nitriding at 430 ℃, the nitrided layer was almost composed of a thin e-Fe2-3N layer. When C 110 steel was subjected to liquid nitriding at 640 ℃, the phase composition of the nitrided layer was greatly changed. The nitrided layer depth increased significantly with increasing the treating temperature. The liquid nitriding effectively improved the surface hardness. After liquid nitriding, the absorption energy of the treated sample decreased and the tensile strength increased by Charpy V-notch (CVN) test. But the elongation of treated sample decreased. The reason is that the nitrided layer of sample is hardened and there is brittlement by diffusion of nitrogen atom. Despite of treatment temperature, the liquid nitriding can improve the corrosion. After being nitrided at 430 ℃, the nitrided layer of the C110 steel was mainly composed by e-Fe2 3N, which has excellent corrosion resistance and high microhardness, the nitrided sample has the best corrosion resistance. After nitriding temperature over 580 ℃, especially at 680 ℃, the sample's surface was covered by the thick oxide layer, which has very low hardness and corrosion resistance. So, the corrosion resistance of samples is severely compromised. 展开更多
关键词 liquid nitriding treated temperature C110 steel corrosion HARDNESS properties