Microstructure control of AZ31 alloy by self-inoculation method for semisolid rheocasting 被引量:6
2
作者 邢博 郝远 +2 位作者 李元东 马颖 陈体军 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第3期567-575,共9页
A novel rheocasting process, self-inoculation method (SIM), was developed for the microstructure control of semisolid wrought Mg alloy. This process involves mixing between liquid alloy and particles of solid alloy ... A novel rheocasting process, self-inoculation method (SIM), was developed for the microstructure control of semisolid wrought Mg alloy. This process involves mixing between liquid alloy and particles of solid alloy (self-inoculants), subsequently pouring the mixed melt into a special designed multi-stream fluid director. The primary phase with dendritic morphology in the conventionally cast AZ31 alloy has readily transformed into near spherical one in the slurry produced by SIM from melt treatment temperature between 690 ℃ and 710 ℃ and self-inoculants addition of 3%-7%. Achievement of the non-dendritic microstructure at the higher melt treatment temperature requires more self-inoculants addition or decreases in the slope angle of fluid director. Primary phase in the slurry thus produced has attained an ideally globular morphology after isothermal holding at 620 ℃ for 30 s. The increasing holding time leads to decrease of shape factor but the coarsening of particle size. The spheroidization and coarsening evolution process of solid particles during the isothermal holding were analyzed by Lifshitz-Slyozov-Wagner (LSW) theory. 展开更多
关键词 AZ31 alloy MICROSTRUCTURE semisolid rheocasting self-inoculation method