低品质粉煤灰制备蒸养加气混凝土试验研究
1
作者 孙鑫蕊 王学志 +1 位作者 董锦坤 贺晶晶 《广东水利电力职业技术学院学报》 2022年第3期12-15,共4页
以低品质粉煤灰为原材料,采用高温高湿蒸养养护工艺制备加气混凝土,探究其各项物理及力学性能。结果表明,在适宜的配合比下,低品质粉煤灰也能制备出性能合格的蒸养加气混凝土。在低品质粉煤灰掺量为61%、水胶比为0.51时抗压强度最高,达... 以低品质粉煤灰为原材料,采用高温高湿蒸养养护工艺制备加气混凝土,探究其各项物理及力学性能。结果表明,在适宜的配合比下,低品质粉煤灰也能制备出性能合格的蒸养加气混凝土。在低品质粉煤灰掺量为61%、水胶比为0.51时抗压强度最高,达到5.98 MPa。 展开更多
关键词 低品质粉煤灰 蒸养养护 加气混凝土 力学性能
下载PDF
蒸养和蒸压条件下粉煤灰水泥浆体中铝配位分布规律 被引量:1
2
作者 赵子远 胡晨光 +3 位作者 白瑞英 刘刚 安宇坤 封孝信 《功能材料》 EI CAS CSCD 北大核心 2018年第5期5096-5102,共7页
采用XRD、^(27 )Al核磁共振测试方法,研究了蒸养和蒸压条件下粉煤灰水泥浆体中铝配位分布的规律。结果表明:蒸养温度升高可提高粉煤灰火山灰效应,增大四配位铝(Al[4])进入C-S-H的数量,促进水钙沸石矿物生成;加快AFt中六配位铝(Al[6])向... 采用XRD、^(27 )Al核磁共振测试方法,研究了蒸养和蒸压条件下粉煤灰水泥浆体中铝配位分布的规律。结果表明:蒸养温度升高可提高粉煤灰火山灰效应,增大四配位铝(Al[4])进入C-S-H的数量,促进水钙沸石矿物生成;加快AFt中六配位铝(Al[6])向AFm转化,增大第三类水化铝酸盐(Third aluminate hydrate,TAH)、含硅水化石榴石、水化石榴石中Al[6]生成量,但不影响莫来石中五配位铝(Al[5])的配位状态。蒸压养护提高粉煤灰火山灰效应显著高于蒸养,升高蒸压温度和延长蒸压时间,可明显提高含铝托勃莫来石和水钙沸石的生成量;同时,不仅可提高AFt、AFm分解向TAH转化程度,而且促进粉煤灰反应形成水化氢氧铝钙石、水化铝酸二钙和TAH,增大莫来石中Al[5]向Al[6]转化程度,使TAH在Al[6]分布中成为主体含铝相。 展开更多
关键词 养护 粉煤灰 水泥浆体 Al3+配位分布
下载PDF
常压下RPC200配制技术的研究 被引量:2
3
作者 张胜 周锡玲 谢友均 《山东建材》 2007年第2期33-37,共5页
研究了常压90℃蒸汽养护下不同配合比对活性粉末混凝土(Reactive Powder Concrete,简称RPC)强度的影响。试验结果表明:常压90℃蒸汽养护下通过优选组分,能配制出抗压强度为200MPa的RPC,抗折强度接近40MPa。
关键词 PRC 抗压强度 蒸养养护
下载PDF
地下管廊预制方涵构件生产技术研究 被引量:3
4
作者 熊远顺 《建筑技术》 2020年第2期189-191,共3页
采用工厂化预制地下管廊,产品质量好,但构件重量大、拼装精度要求高、需研究预制管廊构件的生产技术。以山钢集团日照钢铁精品基地项目供配电电缆隧道工程项目为工程背景,研究预制方涵构件的生产准备工作、模板拼装、浇筑混凝土、蒸汽... 采用工厂化预制地下管廊,产品质量好,但构件重量大、拼装精度要求高、需研究预制管廊构件的生产技术。以山钢集团日照钢铁精品基地项目供配电电缆隧道工程项目为工程背景,研究预制方涵构件的生产准备工作、模板拼装、浇筑混凝土、蒸汽养护以及拆模等施工步骤。 展开更多
关键词 地下管廊 预制方涵构件 型钢模板 养护
下载PDF
Effects of secondary water curing on the long-term strength and durability of concrete after steam-autoclave curing
5
作者 Li Guo Gao Xiang 《Journal of Southeast University(English Edition)》 EI CAS 2018年第4期488-494,共7页
To study the effects of secondary water( SW) curing of 20 ℃ for 7 d on concrete long-term strength and durability after steam-autoclave curing, concrete specimens were fabricated and subjected to standard,steam-autoc... To study the effects of secondary water( SW) curing of 20 ℃ for 7 d on concrete long-term strength and durability after steam-autoclave curing, concrete specimens were fabricated and subjected to standard,steam-autoclave or steamautoclave + SW curing. The compressive strength,accelerated carbonation depth, and Coulomb electric charges of the specimens were tested at the ages of 28,90,180,and 360 d.Furthermore,mercury intrusion porosimetry experiments on the specimens were conducted at the age of 180 d. Results indicate that compared with standard curing,steam-autoclave curing can enhance the early-age strength of concrete; however, it is detrimental to the development of later-age strength, and reduces chloride and carbonation resistance. Due to the replenishment of water into concrete,SW curing can refine the micro-pore size and decrease the ratio of harmful and more harmful pores in concrete. As a result,SW curing is effective in improving the long-term strength and durability of steamautoclaved concrete,and makes it approach that under standard curing. The improvement amplitudes of SW curing on the concrete compressive strength, chloride and carbonation resistance at 360 d can reach 20. 3%,48. 6%,and 80. 9%,respectively. 展开更多
关键词 CONCRETE steam-autoclave curing secondary water curing compressive strength DURABILITY
下载PDF