评刘宗昌等关于贝氏体铁素体形核的工作
1
作者 徐祖耀 《热处理》 CAS 2013年第6期1-4,共4页
评述了刘宗昌等关于贝氏体铁素体形核的工作,包括:(1)过少有关贝氏体铁素体形核机制文献综述;(2)实验工作远不够形核所要求的精确;(3)母相(奥氏体)中的成分和结构等起伏(涨落)不能成为贝氏体铁素体形核的基础;(4)提出的所谓"贝氏... 评述了刘宗昌等关于贝氏体铁素体形核的工作,包括:(1)过少有关贝氏体铁素体形核机制文献综述;(2)实验工作远不够形核所要求的精确;(3)母相(奥氏体)中的成分和结构等起伏(涨落)不能成为贝氏体铁素体形核的基础;(4)提出的所谓"贝氏体形成属非切变非扩散机制"未得到先进相变理论和精细实验的支持。 展开更多
关键词 贝氏体形成 形核一长大 相变机制
下载PDF
Effect of coating material and lubricant on forming force and surface defects in wire drawing process 被引量:5
2
作者 S.M.BYON S.J.LEE +2 位作者 D.W.LEE Y.H.LEE Y.LEE 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2011年第A01期104-110,共7页
A pilot wire drawing machine as well as wire end-pointing roller was developed. Using these machines, a wire drawing test for four different coating materials and two different lubricants was performed as the reductio... A pilot wire drawing machine as well as wire end-pointing roller was developed. Using these machines, a wire drawing test for four different coating materials and two different lubricants was performed as the reduction ratio increased from 10% to 30%. Materials used for a substrate in this study are plain carbon steel (AIS11045) and ultra low carbon bainite steel. To compute the friction coefficient between the coating layer of wire and the surface of die lbr a specific lubricant, a series of finite element analyses were carried out. SEM observations were also conducted to investigate the surface defects of wire deformed. Results show that the behavior of drawing force varies with the lubricant-type at the initial stage of drawing. The powder-typed lubricant with a large particle causes the retardation of lull lubrication on the entire contact surface and the local delamination of coating layer on the wire surface. As the flow stress of a substrate increases, the delamination becomes severe. 展开更多
关键词 COATING LUBRICANT wire drawing DELAMINATION
下载PDF
铁基合金的贝氏体基元及其生长演化
3
作者 徐启昆 周正 《材料科学进展》 CSCD 1991年第4期301-307,共7页
用透射电镜研究了 Fe-C-Mo 和 Fe-C-Si-Mn 合金中温转变早期产物的组织形态,发现在整个中温转变范围非平衡先析型转变都是按贝氏体铁素体相变基元形成及其扩散生长演化方式进行,说明经生长演化一些时间后的基元难于作为判断贝氏体形核... 用透射电镜研究了 Fe-C-Mo 和 Fe-C-Si-Mn 合金中温转变早期产物的组织形态,发现在整个中温转变范围非平衡先析型转变都是按贝氏体铁素体相变基元形成及其扩散生长演化方式进行,说明经生长演化一些时间后的基元难于作为判断贝氏体形核机制的形态学依据。从基元生长演化进程区分了低碳贝氏体和板条马氏体。 展开更多
关键词 铁基合金 贝氏体基元 贝氏体形成