Cu_(2)O基复合材料光降解罗丹明-B性能研究
1
作者 陆海冰 陶玺 +2 位作者 石香香 马紫薇 孙开莲 《广州化工》 CAS 2022年第8期71-72,76,共3页
室温下通过液相反应合成了Cu_(2)O/C_(3)N_(4)和Cu_(2)O/r-GO(还原石墨烯)两种复合材料。采用XRD、SEM对它们进行物相表征,并分别研究它们在可见光下的光催化降解罗丹明-B性能。与纯Cu_(2) O粉末相比,两种复合光催化剂性能都显著提高,... 室温下通过液相反应合成了Cu_(2)O/C_(3)N_(4)和Cu_(2)O/r-GO(还原石墨烯)两种复合材料。采用XRD、SEM对它们进行物相表征,并分别研究它们在可见光下的光催化降解罗丹明-B性能。与纯Cu_(2) O粉末相比,两种复合光催化剂性能都显著提高,这归功于复合材料中C_(3)N_(4)和/r-GO降低了光生电子和空穴的复合湮灭。Cu_(2)O/r-GO光催化剂中面积较小薄层石墨烯片根植于Cu_(2) O立方体中,起到了转移光生电子的作用。高比表面积C_(3)N_(4)不仅起到了分散作用,可能也作为可见光光催化剂与Cu_(2)O形成异质结。 展开更多
关键词 Cu_(2)O Cu_(2)O/C_(3)N_(4) Cu_(2)O/石墨烯 均相还原法光催化降解 罗丹明-B
下载PDF
废旧羊绒制品的L-半胱氨酸回收法 被引量:2
2
作者 白云 麻文效 胡丙南 《印染》 CAS 北大核心 2022年第1期43-46,共4页
采用L-半胱氨酸对废旧羊绒纤维进行降解,并提取其中的角蛋白。通过分析L-半胱氨酸浓度、尿素浓度、pH、温度、时间对羊绒降解率和角蛋白提取率的影响,得到羊绒纤维降解的最优工艺为:pH=10,L-半胱氨酸0.7 mol/L,尿素4 mol/L,温度85℃,时... 采用L-半胱氨酸对废旧羊绒纤维进行降解,并提取其中的角蛋白。通过分析L-半胱氨酸浓度、尿素浓度、pH、温度、时间对羊绒降解率和角蛋白提取率的影响,得到羊绒纤维降解的最优工艺为:pH=10,L-半胱氨酸0.7 mol/L,尿素4 mol/L,温度85℃,时间6 h。羊绒纤维的降解率最高为89%,角蛋白提取率为79%。提取到的角蛋白粉末分子质量为10000~40000 g/mol,可以纺丝加工或用作功能助剂。 展开更多
关键词 废旧羊绒制品 角蛋白 L-半胱氨酸 还原法降解
下载PDF
Preparation and magnetic properties of nickel nanorods by thermal decomposition reducing methods
3
作者 罗愉 张建成 +3 位作者 沈悦 江树涛 刘国勇 王林军 《中国有色金属学会会刊:英文版》 CSCD 2006年第B01期96-100,共5页
The single-crystalline nickel nanorods with narrow size distribution and better magnetic properties were synthesized by thermal decomposition of nickel hydroxide nanorods precursor powders, which were produced by soft... The single-crystalline nickel nanorods with narrow size distribution and better magnetic properties were synthesized by thermal decomposition of nickel hydroxide nanorods precursor powders, which were produced by soft template method using nickel oxalic acid as raw material. The influences of hydrothermal reaction temperature and time on morphology of the products were investigated. The structure, morphology and magnetic properties of the products were characterized by X-ray powder diffraction (XRD), transmission electron microscopy (TEM), thermogravimetric differential scanning calorimetry (TGA-DSC) and vibrating sample magnetometer (VSM). The as-prepared nickel nanorods are uniform with a diameter of 10?15 nm and length 70?120 nm. The results of magnetic measurements show that the specific saturation magnetization(σs) and coercivity values(Hc) of the nickel nanorods are 50.649 A·m2/kg and 190.0×(103/4π)A/m,respectively. Finally, a possible mechanism for the formation of nickel nanorods was discussed briefly. 展开更多
关键词 镍纳米棒 氢氧化镍 降解还原法 制备 磁性质