Effects of multivalent metallic cations, such as Ca2+ and Fe3+, on the flotation of spodumene and beryl were studied. The results show that Fe3+ and Ca2+ exhibit efficient activation on the flotation of spodumene and ...Effects of multivalent metallic cations, such as Ca2+ and Fe3+, on the flotation of spodumene and beryl were studied. The results show that Fe3+ and Ca2+ exhibit efficient activation on the flotation of spodumene and beryl. The ac- tivation of Fe3+ happens quite well within a pH range of 6-9 while the concentration of Fe3+ is 35 mg/L. Efficient acti- vation of Ca2+ takes place over at a pH over 11.6 at a concentration of 140 mg/L. The zeta potential of beryl and spo- dumene shifts slightly to positive values when activated by Ca2+, but markedly by Fe3+. New stretching frequencies of 1594.24 cm-1 and 1587.13 cm-1 have been found in the FTIR spectra of the two minerals after their interaction with Fe3+ and the collector. These new stretching frequencies are the asymmetric stretching frequencies of COO-(carboxyl anion), so thecollector may be chemically absorbed on the surface of Fe3+-activated beryl and spodumene.展开更多
In this work, different flotation–preoxidation–cyanidation methods are considered for treating a lowgrade refractory gold ore. On the one hand, the results of selective flotation show that 22% and 31.1%of total Sb a...In this work, different flotation–preoxidation–cyanidation methods are considered for treating a lowgrade refractory gold ore. On the one hand, the results of selective flotation show that 22% and 31.1%of total Sb and As, respectively, remained in the final tailings and only about 28% of the total Au remained for further cyanidation processes. On the other hand, in bulk method of flotation the maximum Au recovery of 90.6% achieved after 60 min of flotation at the grind size with K80 of 146 micron. In addition, the bulk flotation method resulted in the concentrate with low concentrations of Sb and As elements. To improve the recovery of low-grade refractory gold ores, flotation should be followed by roasting, biological, or pressure oxidation processes so that the gold could be liberated prior to cyanidation processes. It is also found that the pressure oxidation pre-treatment of the concentrates prior to cyanidation may yield high gold recoveries of over than 83%. In these processes, recoveries are controlled by the temperature and the oxygen partial pressure in the solvent. However, by utilizing the bio-oxidation technique, the oxidation of sulfur to sulfate cannot be completed and, consequently, the gold recovery may be limited to only 72.2%.展开更多
基金Project 2005CB623701 supported by the National Key Basic Research & Development Program (973) of China
文摘Effects of multivalent metallic cations, such as Ca2+ and Fe3+, on the flotation of spodumene and beryl were studied. The results show that Fe3+ and Ca2+ exhibit efficient activation on the flotation of spodumene and beryl. The ac- tivation of Fe3+ happens quite well within a pH range of 6-9 while the concentration of Fe3+ is 35 mg/L. Efficient acti- vation of Ca2+ takes place over at a pH over 11.6 at a concentration of 140 mg/L. The zeta potential of beryl and spo- dumene shifts slightly to positive values when activated by Ca2+, but markedly by Fe3+. New stretching frequencies of 1594.24 cm-1 and 1587.13 cm-1 have been found in the FTIR spectra of the two minerals after their interaction with Fe3+ and the collector. These new stretching frequencies are the asymmetric stretching frequencies of COO-(carboxyl anion), so thecollector may be chemically absorbed on the surface of Fe3+-activated beryl and spodumene.
文摘In this work, different flotation–preoxidation–cyanidation methods are considered for treating a lowgrade refractory gold ore. On the one hand, the results of selective flotation show that 22% and 31.1%of total Sb and As, respectively, remained in the final tailings and only about 28% of the total Au remained for further cyanidation processes. On the other hand, in bulk method of flotation the maximum Au recovery of 90.6% achieved after 60 min of flotation at the grind size with K80 of 146 micron. In addition, the bulk flotation method resulted in the concentrate with low concentrations of Sb and As elements. To improve the recovery of low-grade refractory gold ores, flotation should be followed by roasting, biological, or pressure oxidation processes so that the gold could be liberated prior to cyanidation processes. It is also found that the pressure oxidation pre-treatment of the concentrates prior to cyanidation may yield high gold recoveries of over than 83%. In these processes, recoveries are controlled by the temperature and the oxygen partial pressure in the solvent. However, by utilizing the bio-oxidation technique, the oxidation of sulfur to sulfate cannot be completed and, consequently, the gold recovery may be limited to only 72.2%.