奥氏体不锈钢铅液池裂纹修复 被引量:2
1
作者 曲金光 马春霞 《压力容器》 北大核心 2008年第5期26-29,共4页
纯奥氏体不锈钢焊接难度较大。奥氏体不锈钢铅液池进行国产化制作,要求焊接后进行固溶处理,固溶处理后经探伤发现焊缝上有大量的裂纹。通过对材料、固溶处理工艺、焊接工艺研究分析,找出了产生焊接裂纹缺陷的原因,采用适于奥氏体不锈钢... 纯奥氏体不锈钢焊接难度较大。奥氏体不锈钢铅液池进行国产化制作,要求焊接后进行固溶处理,固溶处理后经探伤发现焊缝上有大量的裂纹。通过对材料、固溶处理工艺、焊接工艺研究分析,找出了产生焊接裂纹缺陷的原因,采用适于奥氏体不锈钢焊接修复的焊接材料,并采用适当的焊接工艺,成功地进行了焊接修复。 展开更多
关键词 铅液池 奥氏体不锈钢 裂纹 焊接修复
下载PDF
Evaluation of substrates for zinc negative electrode in acid PbO_2–Zn single flow batteries 被引量:2
2
作者 Junli Pan YuehuaWen +3 位作者 Jie Cheng Junqing Pan Shouli Bai Yusheng Yang 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2016年第4期529-534,共6页
An investigation was performed on the suitability of carbon materials, metallic lead and its alloys as substrates for zinc negative electrode in acid PbO2-Zn single flow batteries. The zinc deposition process was carr... An investigation was performed on the suitability of carbon materials, metallic lead and its alloys as substrates for zinc negative electrode in acid PbO2-Zn single flow batteries. The zinc deposition process was carried out in the mediumofl mol.L 1H2SO4 at room temperature. No maximum current appears on the potentiostatic current transients for the zinc deposition on lead and its alloys. With increasing overpotential, the progressive nucleation turns to be a 3D-instantaneous nucleation process for the resin-graphite composite. Hydrogen evolution on the graphite composite is effectively suppressed with the doping of a polymer resin. The hydrogen evolution reaction on the lead is relatively weak, while on the lead alloys, it becomes serious to a certain degree. Although the ex- change current density of zinc deposition and dissolution process on the graphite composite is relatively low, the zinc corrosion is weakened to a great extent. With the increase of deposition time, zinc deposits are more compact. The cyclings of zinc galvanostatic charge-discharge on the graphite composite provide more than 90% of coulombic and 80% of energy efficiencies, and exhibit superior cycling stability during the first 10 cycles. 展开更多
关键词 Acid single flow batteryZinc negative electrodeElectro-depositionSubstrate
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部