期刊文献+
共找到3篇文章
< 1 >
每页显示 20 50 100
一个与准晶相关的新Al-Cu相
1
作者 董闯 傅尧春 +3 位作者 王德和 徐为平 宋美丽 王英敏 《材料研究学报》 EI CAS CSCD 1995年第2期107-110,共4页
本文报道一个新Al-Cu相具有正交结构,空间群Fddd.点阵常数为:a=0.8166nm,b=0.9995nm,c=1.4149nm,表达式为Al43.2Cu56.8.该相与Al-Cu-Fe准晶的价电子浓度相同,是一... 本文报道一个新Al-Cu相具有正交结构,空间群Fddd.点阵常数为:a=0.8166nm,b=0.9995nm,c=1.4149nm,表达式为Al43.2Cu56.8.该相与Al-Cu-Fe准晶的价电子浓度相同,是一个由CsCl结构衍生的类似相. 展开更多
关键词 准晶 晶体结构 铝铜合金相
下载PDF
Stress-level dependency of creep ageing behavior for friction stir welded Al-Cu alloy 被引量:1
2
作者 WANG Dong-yao ZHAN Li-hua +3 位作者 ZHONG Jue TANG Zhi-mao ZENG Quan-qing GAN Ke-fu 《Journal of Central South University》 SCIE EI CAS CSCD 2022年第9期3030-3053,共24页
Creep ageing forming(CAF)has been widely used in the aerospace engineering,but how to optimize the processing conditions,especially under complex stress state of the CAF process for large-size components produced by f... Creep ageing forming(CAF)has been widely used in the aerospace engineering,but how to optimize the processing conditions,especially under complex stress state of the CAF process for large-size components produced by friction-stir welding is still a great challenge to now.In this work,the creep ageing behaviors and underlying microstructure evolution of a thick friction-stir welded Al-Cu alloy plate after CAF process under different stress levels are systematically investigated.The creep strain and the strength of the joint are both significantly increased when the stress is close to the average yield strength of the initial weld joint.The grain size reduces while the local strain and dislocation density increase from top to bottom of the NZ;hence,the bottom layer of the weld joint exhibits higher creep strain and steady-stage creep strain rate during the CAF process.The results reveal that the gradient microstructures sensitive to the stress level effectively govern the creep-ageing performance from the upper to the bottom layer in a thick friction stir welded Al-Cu alloy plate.Rationally increasing the initial dislocation density of the weld joint can both enhance the tensile properties and promote the creep deformation of the weld joint for CAF process. 展开更多
关键词 creep age forming friction stir welding inhomogeneous gradient microstructure thick Al-Cu alloy plate precipitation microstructure evolution mechanical property
下载PDF
Enhanced thermal stability and mechanical properties of high-temperature resistant Al-Cu alloy with Zr and Mn micro-alloying 被引量:7
3
作者 Teng-teng SUN Ji-wei GENG +5 位作者 Ze-yu BIAN Yi WU Ming-liang WANG Dong CHEN Nai-heng MA Hao-wei WANG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2022年第1期64-78,共15页
The high temperature(HT)thermal stability and mechanical properties of Al-5%Cu(AC)and Al-5%Cu-0.2%Mn-0.2 Zr%(ACMZ)alloys from 573 to 673 K were systematically studied.The results displayed that micro-alloying addition... The high temperature(HT)thermal stability and mechanical properties of Al-5%Cu(AC)and Al-5%Cu-0.2%Mn-0.2 Zr%(ACMZ)alloys from 573 to 673 K were systematically studied.The results displayed that micro-alloying additions of Zr and Mn elements have presented a significant role in stabilizing the main strengthening metastableθ′precipitates at a temperature as high as 573 K.Simultaneously,the HT tensile test demonstrated that ACMZ alloy retained their strength of(88.6±8.8)MPa,which was much higher than that of AC alloy((32.5±0.8)MPa)after the thermal exposure at 573 K for 200 h.Finally,the underlying mechanisms of strength and ductility enhancement mechanism of the ACMZ alloy at HT were discussed in detail. 展开更多
关键词 Al-Cu alloy micro-alloying thermal stability precipitate evolution high-temperature mechanical properties