The CsCdBr 3∶U 3+ crystal was grown by the Bridgman technique from the starting materials CsBr, CdBr 2, and UBr 4. X-ray check showed that the sample crystallized in the CsNiBr 3 structure. Under selective excitation...The CsCdBr 3∶U 3+ crystal was grown by the Bridgman technique from the starting materials CsBr, CdBr 2, and UBr 4. X-ray check showed that the sample crystallized in the CsNiBr 3 structure. Under selective excitation at low temperature, the emission spectra and the fluorescence decay curve were measured and discussed.展开更多
文摘The CsCdBr 3∶U 3+ crystal was grown by the Bridgman technique from the starting materials CsBr, CdBr 2, and UBr 4. X-ray check showed that the sample crystallized in the CsNiBr 3 structure. Under selective excitation at low temperature, the emission spectra and the fluorescence decay curve were measured and discussed.